journal article·2020-09

Femtosecond laser dot-matrix marking on nickel-based alloy using a simple diaphragm-based spatial shaped modulation: Size and position control of marking units with high recognition rate

Xiaoyun Sun, Wenjun Wang, Xuesong Mei, Aifei Pan, Ju Zhang, Guoji Li

Publisher page

Abstract

Abstract In this study, a method for dot-matrix marking with femtosecond laser on nickel-based alloy using diaphragm modulation was proposed. The simulation results showed that the edge quality and recognition uniformity of the crater were improved because of the diffraction effect of the diaphragm. Moreover, the confinement of the diaphragm could ensure the position accuracy. First, the reasonable size of diaphragm turned out to be from 8 to 10 mm. With the addition of the diaphragms, the regular variation of the diameters of the craters under different parameters was beneficial to control the size of the marking units. Thanks to the edge diffraction effect, the melt phenomenon on the edge of the craters almost disappeared, so the boundary of the crater was clear. In addition, the roundness of the crater increased by a maximum of 6%. Because the difference of gray value of different areas within the crater decreased by 60%, the recognition uniformity and the recognition rate of the marking were improved. Moreover, it was found that the contaminated area did not affect the identification of the marking. Therefore, with spatial shaping of laser beam with diaphragm, the femtosecond laser marking technology can have the advantage of high position precision, dimensional accuracy, processing quality and recognition rate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Laser Material Processing Techniques · Surface Roughness and Optical Measurements · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. High performance cutting of advanced aerospace alloys and composite materials10.1016/j.cirp.2015.05.002 ↗
2. Effect of plasma immersion ion implantation and deposition on high temperature oxidation of titanium alloy IMI 834-aluminizing10.1016/j.jallcom.2006.02.034 ↗
3. Materials selection in design of structures and engines of supersonic aircrafts: a review10.1016/j.matdes.2012.10.001 ↗
4. Durability evaluation of biopolymer coating on titanium alloy substrate10.1016/j.jmbbm.2014.03.003 ↗
5. Micro-scale abrasive wear behavior of medical implant material Ti-25Nb-3Mo-3Zr-2Sn alloy on various friction pairs
6. Preparation of micro-nanostructure on titanium implants and its bioactivity10.1016/S1003-6326(16)64217-6 ↗
7. Corrosion behavior of a ZrCN coated Ti alloy with potential application as a bipolar plate for proton exchange membrane fuel cell10.1016/j.jallcom.2015.12.197 ↗
8. Self-healing, chromate-free conversion coating for magnesium alloys10.1016/S0026-0576(13)70127-2 ↗
9. Reliability of dot peen marking in product traceability
10. Direct part marking by vibration assisted face milling10.1016/j.protcy.2016.08.025 ↗
11. Printing data matrix code on food-grade tracers for grain traceability10.1016/j.biosystemseng.2012.09.012 ↗
12. High contrast laser marking of alumina10.1016/j.apsusc.2014.10.004 ↗
13. Experimental investigations on fiber laser color marking of steels10.1016/j.apsusc.2015.05.095 ↗
14. Rapid and flexible laser marking and engraving of tilted and curved surfaces10.1016/j.optlaseng.2010.09.003 ↗
15. Controlling 2D laser nano structuring over large area with double femtosecond pulses10.1016/j.apsusc.2018.11.106 ↗
16. Artificial compound eyes prepared by a combination of air-assisted deformation, modified laser swelling, and controlled crystal growth10.1021/acsnano.8b04047 ↗
17. Picosecond and femtosecond lasers for industrial material processing
18. Sequential combination of femtosecond laser ablation and induced micro/nano structures for marking units with high-recognition-rate10.1002/adem.201900350 ↗
19. Laser marking of titanium coating for aerospace applications10.1016/j.procir.2016.01.006 ↗
20. Experimental investigation and mathematical modeling of laser marking two-dimensional barcodes on surfaces of aluminum alloy10.1016/j.jmapro.2015.12.007 ↗
21. Study of the laser marking process of cold sprayed titanium coatings on aluminium substrates10.1016/j.optlastec.2016.04.007 ↗
22. Controllable dot-matrix marking on titanium alloy with anti-reflective micro-structures using defocused femtosecond laser10.1016/j.optlastec.2019.02.022 ↗
23. Laser direct marking applied to rasterizing miniature Data Matrix Code on aluminum alloy10.1016/j.optlastec.2015.08.020 ↗
24. Laser microsculpting for the generation of robust diffractive security markings on the surface of metals10.1016/j.jmatprotec.2015.03.001 ↗
25. Polarization and fluence effects in femtosecond laser induced micro/nano structures on stainless steel with antireflection property10.1016/j.apsusc.2017.07.157 ↗
26. Direct femtosecond laser fabrication of antireflective layer on GaAs surface10.1007/s00340-013-5350-4 ↗
27. Near-unity below-band gap absorption by microstructured silicon10.1063/1.1358846 ↗
28. The relationship of processing parameters and surface topography of selective laser melted GH4169 alloy10.4028/www.scientific.net/MSF.893.207 ↗
29. A finite element analysis of thermal relaxation of residual stress in laser shock processing Ni-based alloy GH416910.1016/j.matdes.2013.08.054 ↗
30. Characterization of rapid PDMS casting technique utilizing molding forms fabricated by 3D rapid prototyping technology (RPT)10.1007/s12289-012-1119-2 ↗
31. Effect of mold treatment by solvent on PDMS molding into nanoholes10.1186/1556-276X-8-394 ↗
32. Does flat epithelial atypia have rounder nuclei than columnar cell change/hyperplasia? A morphometric approach to columnar cell lesions of the breast10.1007/s00428-016-1923-z ↗
33. AISI 304 stainless steel marking by a Q-switched diode pumped Nd:YAG laser10.1016/j.jmatprotec.2010.03.018 ↗
34. A study on the laser marking process of stainless steel10.1016/S0924-0136(03)00234-6 ↗
35. High-contrast laser marking of microelectronic packaging modules10.2961/jlmn.2015.02.0013 ↗