Enhancement of mechanical properties and thermoelectric performance of spark plasma sintered P-type Bismuth Telluride by powder surface oxide reduction
Source abstract
Abstract
Abstract In the present investigation, key mechanical design parameters and the thermoelectric performance of powder ball milled spark plasma sintered P-typ e Bi0·4Sb1·6Te3 material was determined. In particular, the effect of the powder preparation technique on the powder surface oxide layer as well as both the mechanical and thermoelectric properties were determined. All measurements were performed on identically prepared sintered samples in both parallel and perpendicular to the applied sintering pressure. The mechanical properties determined included relative density, uniaxial tensile strength, coefficient of thermal expansion, Young’s modulus, Poisson’s ratio, and shear modulus. The thermoelectric properties measured included the Seebeck coefficient, electrical resistivity, and thermal conductivity. A mechanically agitated reduction facility built in-house was used to reduce the powder surface oxide at 380 °C for 24 h using dry 5% H2 95% Ar. To separate between the annealing and the reduction effects, the P-type ( Bi , Sb ) 2 Te 3 powder was annealed using highly purified Ar at the same temperature and time as the reduction process. The oxygen content in the sintered P-type samples was then measured using the inert gas fusion technique. The oxygen content was found to be decreased by 35 wt% after 24 h of reduction but did not change significantly after annealing with Ar only relative to the dried powders. The reduction of the surface oxides increased the relative density of the sintered parts from 97.1% to 99.2%. Consequently, the characteristic uniaxial tensile strength increased from 13.9 MPa to 26.3 MPa and from 16.3 MPa to 30.6 MPa in the parallel and the perpendicular directions to the sintering pressure, respectively, for the sintered bodies from the reduced powder. Both the Young’s modulus and the shear modulus increased from 44.3 GPa to 48.7 GPa and 17.8 GPa–19.5 GPa in the parallel direction, respectively, after the reduction treatment and sintering. The figure of merit, ZT, increased from 0.35 to 0.80 and from 0.42 to 1.13 at room temperature (25 °C) in the parallel and the perpendicular directions, respectively, after the surface oxide reduction treatment.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Heusler alloys: electronic and magnetic properties · Thermal Expansion and Ionic Conductivity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Rowe · 2006
2. Influence of composition and texture on the thermoelectric and mechanical properties of extruded (Bi1-xSbx)2(Te1-ySey)3 alloys10.1109/ICT.2003.1287438 ↗
3. The variation of the equilibrium of chemical reactions in the process of (Bi 2 Te 3)( Sb 2 Te 3)(Sb 2 Se 3) crystal growth10.1016/S0022-0248(01)01808-5 ↗
4. Effect of annealing on thermoelectric properties of bismuth telluride compounds10.1143/JJAP.42.492 ↗
5. Improving hardness and thermoelectric performance in pseudo-ternary thermoelectric alloys (Bi2Te3)(Bi2Se3)(Nd2Te3)10.1143/JJAP.45.7032 ↗
6. Thermal properties of high quality single crystals of bismuth telluride—Part I: experimental characterization10.1016/0022-3697(88)90182-5 ↗
7. Effect of hydrogen annealing of ball-milled Bi0.5Sb1.5Te3 powders on thermoelectric properties10.1016/j.jallcom.2017.02.181 ↗
8. Effect of powder mixing on thermoelectric properties in Bi2Te3-based sintered compounds10.1016/j.intermet.2005.10.018 ↗
9. Thermoelectric performance of p-type Bi-Sb-Te materials prepared by spark plasma sintering10.1016/j.jallcom.2004.07.056 ↗
10. Preparation and Properties of p-Type (Bi2Te3)x(Sb2Te3)1-x
11. Mechanically enhanced p- and n-type Bi2Te3-based thermoelectric materials reprocessed from commercial ingots by ball milling and spark plasma sintering10.1016/j.mseb.2015.03.011 ↗
12. Effect of ball milling time on the thermoelectric properties of p-type (Bi,Sb)2Te310.1016/j.jallcom.2013.03.062 ↗
13. The time-dependent process of oxidation of the surface of Bi2Te3 studied by X-ray photoelectron spectroscopy10.1088/0953-8984/12/26/307 ↗
14. Characteristics of p-type Bi0.5Sb1.5Te3compounds doped with Te10.1016/S0167-577X(97)00217-6 ↗
15. Thermoelectric properties of 25%Bi2Te3-75%Sb2Te3 solid solution prepared by hot-pressing method10.1016/S0022-3697(96)00049-2 ↗
16. Thermoelectric properties of p-type Te doped Bi0.5Sb1.5Te3 fabricated by powder extrusion10.1016/S0921-5107(01)00912-6 ↗
17. Effects of hydrogen reduction on the thermoelectric properties of spark-plasma-sintered Bi 2 Te 3 -based
18. Influence of milling atmosphere on thermoelectric properties of p-type Bi-Sb-Te based alloys by mechanical alloying10.4150/KPMI.2017.24.5.357 ↗
19. Thermal stress analysis and structure parameter selection for a Bi2Te3-based thermoelectric module10.1007/s11664-011-1611-3 ↗
20. Effect of various leg geometries on thermo-mechanical and power generation performance of thermoelectric devices10.1016/j.applthermaleng.2014.07.027 ↗
21. Estimation of thermoelectric and mechanical performances of segmented thermoelectric generators under optimal operating conditions10.1016/j.applthermaleng.2014.07.069 ↗
22. Thermodynamics and thermal stress analysis of thermoelectric power generator: influence of pin geometry on device performance10.1016/j.applthermaleng.2012.07.021 ↗
23. Thermal and stress analyses in thermoelectric generator with tapered and rectangular pin configurations10.1016/j.energy.2016.07.168 ↗
24. Numerical simulation on thermoelectric and mechanical performance of annular thermoelectric generator10.1016/j.energy.2018.02.124 ↗
25. High performance and thermal stress analysis of a segmented annular thermoelectric generator10.1016/j.enconman.2019.01.064 ↗
26. St-Laurent · 2018
27. Standard test method for transthickness tensile strength of continuous fiber- reinforced
28. Izv. Akad. Nauk SSSR
29. Kinetics of antimony trioxide reduction by hydrogen. Effect of atomic hydrogen10.1007/BF00795791 ↗
30. 2020 · 1
31. Thermoelectric and transport properties of nanostructured Bi 2Te3 by spark plasma sintering10.1557/jmr.2010.67 ↗
32. Eisenmann · 1985
33. Thermal expansion of bismuth telluride10.1134/S0018151X1103014X ↗
34. Quinn · Flexural Strength of Ceramic and Glass Rods · 2009 · 37 · 1
35. High-temperature mechanical and thermoelectric properties of p-type Bi 0.5Sb1.5Te3 commercial zone melting ingots10.1007/s11664-013-2938-8 ↗
36. Flexural strength of alumina ceramics: Weibull analysis
37. Astm · 2000 · 1
38. 2003 · 2004
39. T.A.C. Society-discussions, Effect of Porosity on Young’s, 45 (n.d.) 94–95.
40. Young’s modulus of porous brittle solids10.1007/BF01160581 ↗
41. Luo · 1999 · 25
42. Influence of porosity on Youngs modulus and Poisson’s ratio in alumina ceramics10.1016/S0955-2219(00)00314-9 ↗
43. 2015
44. Oxide formation mechanism and its effect on the microstructure and thermoelectric properties of p-type Bi 0.5 Sb 1.5 Te 3 alloys10.1016/j.intermet.2018.09.015 ↗
45. Effects of heavy deformation and annealing on the electrical properties of Bi2Te310.1063/1.1728990 ↗
46. Energy formation of antisite defects in doped Sb2Te3and Bi2Te3crystals10.1016/0022-3697(86)90010-7 ↗
47. Antisite defects in Sb2-xBixTe3 mixed crystals10.1016/0022-3697(88)90130-8 ↗
48. Influence of powder size on thermoelectric properties of p-type 25%Bi2Te3-75%Sb2Te3alloys fabricated using gas-atomization and spark-plasma sintering10.1016/j.jallcom.2016.05.340 ↗
49. Thermoelectric properties of (Bi0.25Sb0.75)2Te3 alloys fabricated by hot-pressing method10.1023/A:1004862700211 ↗
50. Thermoelectric properties of p-type Bi0.5Sb1.5Te 3 compounds fabricated by spark plasma sintering10.1007/s10832-006-6807-1 ↗
51. Electronic transport in semimetallic cerium sulfide
52. The conduction band of cerium sulfide Ce3-xS410.1016/0022-3697(63)90136-7 ↗
53. Yuanwen · 2010
54. Eaksuwanchai · 2018
55. Influence of powder morphology on thermoelectric anisotropy of spark-plasma-sintered Bi-Te-based thermoelectric materials10.1016/j.actamat.2010.09.054 ↗
56. Rowe · 1995