journal article·2023-03

Strengthening and toughening mechanisms of P-rich phase in Cu-4Sn-P alloy wire

Xin-Rong Duan, Yan Chen, Zhi-Yuan Hong, Song-Wei Wang, Shuai-Feng Chen, Shi-Hong Zhang

Publisher page

Abstract

The Cu-4Sn and Cu-4Sn-0.15P alloys with rod diameter of 12.5 mm were prepared and then cold drawn to 2.6 mm via multi-pass drawing. The microstructure evolutions, mechanical properties, and electrical conductivity of Cu-4Sn and Cu-4Sn-0.15P alloys were comprehensively analyzed using optical microscope, scanning electron microscope, tension test and electrical conductivity tester. As compared with the P-free alloy, the addition of P can form a new kind of P-rich phase in the Cu-4Sn alloy, and thus refine the casting microstructure via pinning the grain boundary. The toughening mechanisms of P-rich phases in Cu-4Sn-P alloy wires during cold drawing were investigated. With accumulative drawing strain, the spherical P-rich phase gradually changes into fibrous phases, which thus introduce obvious fiber reinforced strengthening. In addition, the distribution of P-rich phase also enhances the< 111 > texture, and promotes the growth of fragmentation zone. It contributes to an improved ultimate tensile strength and final elongation from 664.5 MPa and ∼ 0 % in Cu-4Sn alloy to 970.5 MPa and 1.53 % in Cu-4Sn-0.15P alloy. Finally, the conductivity for Cu-4Sn-0.15P decreases slightly owing to the intensified electron scattering with high amount of primary phase after the addition of P element.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Innovative compound casting technology and mechanical properties of steel matrix syntactic foams10.1016/j.jallcom.2020.156572 ↗
2. Tension–compression asymmetry of phosphor bronze for electronic parts and its effect on bending behavior10.1016/j.ijplas.2009.01.004 ↗
3. Growth mechanisms of Cu3Sn on polycrystalline and single crystalline Cu substrates10.1016/j.actamat.2009.06.025 ↗
4. Changes in mechanical characteristics of pre-annealed wires of Cu–Sn alloy manufactured by continuous draw bending10.2320/matertrans.MD201114 ↗
5. Morphological and mechanical behaviour of Cu–Sn alloys—a review10.1007/s12540-020-00899-z ↗
6. Evaluation of effect of alloy elements in copper based CuSn10 and CuZn30 bearings on tribological and mechanical properties10.1016/j.jallcom.2009.09.068 ↗
7. Thermodynamic description of the Cu–Sn system10.1557/JMR.2007.0396 ↗
8. Formation of compounds and Kirkendall vacancy in the Cu–Sn system10.1016/j.mee.2013.09.009 ↗
9. Microstructural evolution in Cu–Sn coatings deposited on steel substrate and its effect on interfacial adhesion10.1016/j.surfcoat.2014.12.049 ↗
10. Mechanism for the development of Sn-Cu alloy coatings produced by pulsed current electrodeposition10.1016/j.matlet.2018.01.094 ↗
11. Wear behavior of high strength and high conductivity Cu alloys under dry sliding10.1016/S1003-6326(15)63844-4 ↗
12. Enhanced mechanical strength of Cu–Sn alloy by Mg addition10.1088/2053-1591/abde11 ↗
13. Solid–state diffusion–controlled growth of the intermediate phases from room temperature to an elevated temperature in the Cu–Sn and the Ni–Sn systems10.1016/j.jallcom.2017.08.178 ↗
14. Effect of electric current on grain orientation and mechanical properties of Cu-Sn intermetallic compounds joints10.1016/j.jallcom.2018.04.041 ↗
15. Columnar grains-covered small grains Cu–Sn alloy prepared by two-phase zone continuous casting10.1016/j.pnsc.2013.01.014 ↗
16. Garbacz-Klempka · Arch. Foundry Eng. · 2018
17. Enhancement of strength and ductility of Cu–Sn–Zn alloy by iron addition10.1016/j.msea.2014.06.047 ↗
18. Determination on the effect of Ti addition on the microstructural, mechanical and wear behavior of Cu–6Sn alloy in as—cast condition10.1007/s12666-019-01835-5 ↗
19. Determination on the effect of tin content on microstructure, hardness, optimum aging temperature and aging time for spinodal bronze alloys cast in metal mold
20. Effects of P addition on spinodal decomposition and discontinuous precipitation in Cu-15Ni-8Sn alloy10.1016/j.matchar.2020.110760 ↗
21. The role of binding energies for phosphorus and sulphur at grain boundaries in copper10.1016/j.jnucmat.2020.152682 ↗
22. Influence of phosphorus on the creep ductility of copper10.1016/j.jnucmat.2013.06.020 ↗
23. A note on the effect of phosphorus on the microstructure and mechanical properties of leaded-tin bronze10.1016/S0924-0136(02)00137-1 ↗
24. Design of exceptionally strong and conductive Cu alloys beyond the conventional speculation via the interfacial energy-controlled dispersion of γ-Al2O3 nanoparticles10.1038/srep17364 ↗
25. Influence of hot pressing temperature on the microstructure and mechanical properties of 75% Cu–25% Sn alloy10.1016/j.matdes.2013.06.024 ↗
26. Microstructure and phase-transformation studies of Cu-Ni-Sn alloys10.1143/JJAP.34.1619 ↗
27. Mechanisms for refining precipitation and improving strengthening of annealed Cu-2Ag alloy via La modification10.1016/j.jallcom.2021.160912 ↗
28. Co and Ti effect on hot workability of phosphor bronze10.1016/j.jallcom.2022.163778 ↗
29. Strengthening mechanisms in a high-strength bulk nanostructured Cu–Zn–Al alloy processed via cryomilling and spark plasma sintering10.1016/j.actamat.2012.09.036 ↗
30. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
31. Microstructural evolution and properties of a Cu–Cr–Ag alloy during continuous manufacturing process10.1007/s12598-019-01238-x ↗
32. Microstructure and properties of high-strength Cu–Ni–Si–(Ti) alloys10.1007/s12598-020-01699-5 ↗
33. N. Hansen, Polycrystalline strengthening, Metall. Trans. A. (n.d.) 24.
34. Strengthening in rapidly solidified age hardened Cu-Cr and Cu-Cr-Zr alloys10.1016/S1359-6454(96)00142-5 ↗
35. The effect of shear-resistant, plate-shaped precipitates on the work hardening of Al alloys: towards a prediction of the strength–elongation correlation10.1016/j.actamat.2009.08.034 ↗
36. The role of internal stresses on the plastic deformation of the Al–Mg–Si–Cu alloy AA611110.1080/14786430801894569 ↗
37. A low Sn content Cu-Ni-Sn alloy with high strength and good ductility10.1016/j.msea.2018.12.120 ↗
38. The influence of stacking fault energy on the mechanical behavior of Cu and Cu-Al alloys: deformation twinning, work hardening, and dynamic recovery10.1007/s11661-001-0109-7 ↗