Phase evolution and enhanced dielectric properties of BaO·Nd 2 O 3 ·TiO 2 ·B 2 O 3 glass-based dielectrics containing CaCu 3 Ti 4 O 12
Source abstract
Abstract
CaCu3Ti4O12 (CCTO) has been studied as a filler for the potential high k LTCC (low temperature co-fired ceramics) materials based on a nonconventional BaO·Nd2O3·TiO2·B2O3 glass in terms of firing temperature and CCTO content. The material system was proven to be high crystallizable as the resultant crystalline phases of BaTi(BO3)2, BaNd2Ti5O14 and NdBO3 were observed. The relative content of the crystalline phases were strongly dependant on firing temperature and CCTO content. Interestingly, the 30 wt% CCTO sample showed early densification at 610–670 °C and then unexpected expansion after 850 °C. The 40–60 wt% CCTO samples showed the unexpected secondary densification behavior over the temperature range of 850–950 °C. As a promising example, a combination consisting of the glass and 40 wt% CCTO exhibited k ∼55 and tan δ ∼0.07, which is very rare at this low sintering temperature of 850 °C. These materials system were found to be chemically very stable especially in the H2SO4 acid solution.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dielectric properties of ceramics · Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Saito · IEEE Trans. Microw. Theory Tech. · 2001 · 49 · 242110.1109/22.971630 ↗
2. Zhu · J. Alloy Compd. · 2009 · 482 · 27210.1016/j.jallcom.2009.03.179 ↗
3. Baker · Int. J. Appl. Ceram. Technol. · 2005 · 2 · 51410.1111/j.1744-7402.2005.02052.x ↗
4. Kagata · Ceram. Trans. · 1993 · 32 · 81
5. Chang · J. Am. Ceram. Soc. · 1999 · 82 · 172510.1111/j.1151-2916.1999.tb01992.x ↗
6. Subramanian · J. Solid State Chem. · 2000 · 151 · 32310.1006/jssc.2000.8703 ↗
7. Li · J. Alloy Compd. · 2011 · 509 · 102510.1016/j.jallcom.2010.09.163 ↗
8. Kim · J. Am. Ceram. Soc. · 2010 · 93 · 233410.1111/j.1551-2916.2010.03744.x ↗
9. Doo · J. Am. Ceram. Soc. · 2010 · 93 · 33410.1111/j.1551-2916.2009.03411.x ↗
10. Mohanram · J. Am. Ceram. Soc. · 2005 · 88 · 268110.1111/j.1551-2916.2005.00497.x ↗
11. Kemethmuller · J. Am. Ceram. Soc. · 2006 · 90 · 6410.1111/j.1551-2916.2006.01362.x ↗
12. Fang · J. Am. Ceram. Soc. · 2004 · 87 · 207210.1111/j.1151-2916.2004.tb06362.x ↗
13. Lim · J. Eur. Ceram. Soc. · 2009 · 29 · 71110.1016/j.jeurceramsoc.2008.07.058 ↗
14. Jo · J. Alloy Compd. · 2011 · 509 · 84910.1016/j.jallcom.2010.09.110 ↗
15. Lu · Mater. Sci. Eng. B · 2003 · 98 · 3310.1016/S0921-5107(02)00593-7 ↗
16. Aoyagi · Ferroelectrics · 2007 · 356 · 9010.1080/00150190701509306 ↗
17. Sinclair · Appl. Phys. Lett. · 2002 · 80 · 215310.1063/1.1463211 ↗
18. Jo · Mater. Res. Bull. · 2008 · 43 · 36110.1016/j.materresbull.2007.03.002 ↗