Effect of Pd, temperature and time on wetting and interfacial microstructure of bulk metallic glasses TiCuZrPd on Ti-6Al-4V substrate

Anna Sypien, Kamil Badura, Przemyslaw Fima, Krzysztof Miernik

Publisher page

Abstract

Melting behavior of TiCuZrPd bulk metallic glasses (BMGs) containing 10, 14, 20 at.% Pd was studied by DSC and their melting range is: 845–910, 831–900, 874–911 °C, respectively. Wetting of TiCuZrPd BMGs on Ti-6Al-4V substrate was studied at 850, 880 °C for 5, 10, 30 min. It was found that wetting angle decreases and spreading area increases with increasing temperature and time. Interfacial microstructure of TiCuZrPd/Ti-6Al-4V solidified couples was studied with scanning electron microscopy and energy dispersive spectroscopy. Three intermediate layers were identified at the interface between Ti-6Al-4V substrate and TiCuZrPd BMGs. The first layer adjacent to substrate is composed mostly of Ti, with concentrations of Al lower and V close to that in Ti-6Al-4V, whereas Cu, Pd and traces of Zr are also present. This indicates that this layer was formed by diffusion of Cu, Pd and Zr into substrate. Second layer, adjacent to the first, has higher concentration of Cu compared to the first, there is no V in this layer and concentration of Al is about 50% lower than that in the first. This and the fact that there is no Al in third layer, adjacent to BMG, indicates that Al and V do not diffuse into BMG. In the third layer concentration of Ti is similar to that in the second layer but still 50% higher than in TiCuZrPd, while concentrations of Cu and Zr are lower and concentration of Pd close to that in TiCuZrPd.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Material Properties and Applications · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Schwartz · 2003
2. Infrared brazing Ti–6Al–4V and Mo using the Ti–15Cu–15Ni braze alloy10.1016/j.ijrmhm.2005.01.002 ↗
3. Microstructures of brazing zone between titanium alloy and stainless steel using various filler metals10.1016/S1003-6326(12)61778-6 ↗
4. Brazing of Si3N4 with amorphous Ti40Zr25Ni15Cu20 filler10.1016/j.msea.2008.11.056 ↗
5. Komolafe · 2014
6. Thermal stability and mechanical properties of the TiCuZrPd glasses with 10, 14 and 20 at.% Pd10.1016/j.jallcom.2013.12.240 ↗
7. Preparation of Ti–Ni–Fe phase by levitation and its structural characterization10.1179/174328409X422257 ↗
8. Wetting of Cu and Al by Sn-Zn and Zn-Al eutectic alloys10.1007/s11665-012-0174-7 ↗
9. Microstructural evolution and shear strength of brazing C103 and Ti-6Al-4V using Ti-20Cu-20Ni-20Zr (wt%) filler metal10.1016/j.ijrmhm.2005.05.014 ↗
10. Influence of the Sn and Nb additions on the crystallization and microhardness of the TiCuZr14at.%Pd amorphous alloy10.1007/s11665-016-1898-6 ↗
11. Measurement of contact angle and work of adhesion at high temperature10.1007/s10853-005-1945-4 ↗
12. Fundamental issues of reactive wetting by liquid metals10.1007/s10853-009-4128-x ↗
13. Growth of isothermally-solidified titanium joints using a multi-component Zr–Ti–Cu–Ni–Be amorphous alloy as a brazing filler10.1016/j.matchar.2013.03.015 ↗
14. Mechanical and corrosion properties of Ti-6Al-4V alloy joints brazed with a low-melting-point 62.7-11.0Ti-13.2Cu-9.8Ni-3.3Be amorphous filler metal10.1016/j.matchar.2013.04.002 ↗
15. Increasing Ti-6Al-4V brazed joint strength equal to the base metal by Ti and Zr amorphous filler alloys10.1016/j.matchar.2012.05.016 ↗
16. Rapid formation of intermetallic compound by interdiffusion in the Cu-Sn and Ni-Sn systems
17. Cu-Ti (Copper-Titanium)10.1361/105497102770331307 ↗
18. Pd-Ti (Palladium-Titanium)10.1007/s11669-012-0137-6 ↗
19. Thermodynamic assessment of the TiZr system and calculation of the NbTiZr phase diagram10.1016/0925-8388(94)90019-1 ↗
20. Cu-Pd (Copper-Palladium)10.1007/BF02645723 ↗
21. Thermodynamic assessment of the Cu-Ti-Zr system10.1016/S0925-8388(02)01035-6 ↗
22. Evaluate of braze joint strength and microstructure characterize of titanium-CP with Ag-based filler alloy10.1016/j.matdes.2012.01.045 ↗
23. Taguchi · Diffusion of copper, silver and gold in α-titanium Philos. Mag. A · 1995 · 72 · 1649
24. Microstructural evolution of infrared brazed Ti-15-3 alloy using Ti-15Cu-15Ni and Ti-15Cu-25Ni fillers10.1016/j.scriptamat.2005.11.013 ↗
25. Massalski · 1997 · 1600
26. Experimental study of diffusion welding/bonding of titanium to copper10.1016/j.matdes.2012.01.026 ↗