journal article·2009-06

Citrate-oxide method to prepare SrBi4Ti4O15 powders and ceramics

Zhijun Xu, Ruiqing Chu, Jigong Hao, Guorong Li, Qingrui Yin

Journal of Alloys and Compounds· Volume 479· Issue 1-2
Publisher page

Abstract

Abstract SrBi 4 Ti 4 O 15 (SBTi) powders were synthesized by citrate-oxide method. Oxides and carbonates were used as starting materials to replace other expensive soluble salts in citrate–nitrate combustion method. Attempts have been made to understand the synthesis process with the help of thermogravimetric (TG) and differential scanning calorimetry (DSC) of the samples. XRD results showed that the pure phase SBTi powders were obtained at 500 °C for 2 h, which was much lower than the calcination temperature (800–850 °C) required in solid-state reaction. The SBTi ceramics sintered at 1180 °C for 1 h exhibited a relative density of 93.7% and a piezoelectric coefficient of 19 pC/N. This sintering temperature was lower 50 °C than that required in solid-state reaction. The research results indicate that the citrate-oxide method is an efficient, quick and simple method for mass production of ceramic oxide powder.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Acoustic Wave Resonator Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Scott · Science · 1989 · 246 · 140010.1126/science.246.4936.1400 ↗
2. Asai · J. Alloys Compd. · 2000 · 309 · 11310.1016/S0925-8388(00)01081-1 ↗
3. Zhang · J. Appl. Phys. · 2002 · 91 · 316010.1063/1.1435414 ↗
4. Zhang · Mater. Lett. · 2001 · 47 · 33410.1016/S0167-577X(00)00260-3 ↗
5. Hirose · Jpn. J. Appl. Phys. · 1999 · 38 · 556110.1143/JJAP.38.5561 ↗
6. Zhu · Solid State Commun. · 2004 · 130 · 36310.1016/j.ssc.2004.01.047 ↗
7. Gelfuso · J. Am. Ceram. Soc. · 1999 · 82 · 236810.1111/j.1151-2916.1999.tb02092.x ↗
8. Noguchi · Appl. Phys. Lett. · 2000 · 77 · 363910.1063/1.1328366 ↗
9. Zhao · Mater. Sci. Eng. B · 2003 · 99 · 14310.1016/S0921-5107(02)00505-6 ↗
10. Liaoying · Mater. Sci. Eng. B · 2003 · 99 · 36310.1016/S0921-5107(02)00500-7 ↗
11. Xu · J. Am. Ceram. Soc. · 2008 · 91 · 91010.1111/j.1551-2916.2007.02201.x ↗
12. Rodriguez · J. Mater. Res. · 1996 · 11 · 228210.1557/JMR.1996.0290 ↗
13. Liu · J. Alloys Compd. · 2008 · 457 · L1210.1016/j.jallcom.2007.03.080 ↗
14. Chu · Mater. Sci. Eng. B · 2005 · 122 · 10610.1016/j.mseb.2005.05.010 ↗
15. Xu · Scripta Mater. · 2004 · 50 · 16510.1016/j.scriptamat.2003.09.008 ↗
16. Xu · J. Alloys Compd. · 2008 · 463 · 27510.1016/j.jallcom.2007.08.068 ↗
17. Yu · J. Alloys Compd. · 2008 · 459 · L110.1016/j.jallcom.2007.04.216 ↗
18. Yu · Mater. Lett. · 2003 · 58 · 4810.1016/S0167-577X(03)00412-9 ↗
19. Du · J. Alloys Compd. · 2003 · 352 · 25010.1016/S0925-8388(02)01165-9 ↗
20. Qiu · J. Mater. Sci. · 2008 · 43 · 309410.1007/s10853-008-2515-3 ↗
21. Chakrabarti · Mater. Lett. · 1997 · 30 · 16910.1016/S0167-577X(96)00191-7 ↗
22. Chen · Mater. Lett. · 2003 · 57 · 339210.1016/S0167-577X(03)00081-8 ↗
23. Kong · Prog. Mater. Sci. · 2008 · 53 · 20710.1016/j.pmatsci.2007.05.001 ↗
24. Uchino · J. Am. Ceram. Soc. · 1989 · 72 · 155510.1111/j.1151-2916.1989.tb07706.x ↗
25. Wu · J. Appl. Phys. · 2001 · 90 · 529610.1063/1.1413236 ↗