Solid solution range of boron and properties of the perovskite-type NdRh3B
Source abstract
Abstract
Abstract Polycrystalline samples of NdRh 3 B x have been synthesized by arc melting technique. The crystal structure of NdRh 3 B x is the perovskite-type cubic system (space group Pm 3 m ) for nominal boron concentration in the range of 0.706≤ x ≤1.000 (15–20 mol.% B). The lattice parameter a varies linearly from 0.41749(7) nm ( x =0.706) to a =0.42136(6) nm ( x =1.000). Thermogravimetric analysis indicates that the oxidation onset temperature for NdRh 3 B 1.000 is 663 K. The weight gain of the sample by heating in air up to 1473 K is 10.00% for NdRh 3 B 1.000 , and oxidized products are Rh and NdBO 3 . The micro-Vickers hardness is 4.9±0.05 GPa for NdRh 3 B 1.000 . NdRh 3 B 1.000 shows a metallic temperature dependence of the resistivity down to 0.5 K. Magnetic susceptibilities for NdRh 3 B 1.000 show Curie-like paramagnetic temperature dependence due to Nd 3+ moments. No trace of magnetic phase transitions and superconductivity is found.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Rare-earth and actinide compounds · Magnetic Properties of Alloys · Inorganic Chemistry and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Woolf · J. Low Temp. Phys. · 1979 · 35 · 65110.1007/BF00117903 ↗
2. Superconductivity in ternary compounds II
3. Boron, borides and related compounds
4. Shishido · J. Alloys Comp. · 1998 · 280 · 6510.1016/S0925-8388(98)00714-2 ↗
5. Holleck · J. Less-Common Metals · 1977 · 52 · 16710.1016/0022-5088(77)90248-X ↗
6. Rogl · J. Less-Common Metals · 1983 · 91 · 9710.1016/0022-5088(83)90099-1 ↗
7. Shishido · J. Alloys Comp. · 1999 · 291 · 5210.1016/S0925-8388(99)00239-X ↗
8. Shishido · J. Ceram. Soc. Jpn. · 2000 · 108 · 68310.2109/jcersj.108.1259_683 ↗
9. Honig · RCA Rev. · 1962 · 23 · 571
10. Samsonov · 1980 · 303