A successful process to prevent corrosion of rich Gd-based room temperature magnetocaloric material during ageing
Source abstract
Abstract
Abstract When the heat transport processes occur in a magnetic refrigeration device, there is possibility of corrosion thereforth, insight on the magnetocaloric regenerator corrosion could be shed in light. Our work mimicks this phenomenon by subjecting the magnetocaloric material Gd6Co1.67Si3 to controlled water flow. The corrosion is first explained based on the elemental electrochemical oxidation thereby allowing a new test by the exposing material in passive fluid (KOH) up to 1 year. The neglected degradation of the material was justified by X-Ray photoelectron spectroscopy (XPS) and depth profile Auger spectroscopy, and thus the control of its corrosion is reported. The effective control of the corrosion when material is exposed to KOH could be a universal procedure in magnetic refrigeration prototype.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic and transport properties of perovskites and related materials · Shape Memory Alloy Transformations · Thermal Expansion and Ionic Conductivity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Review on research of room temperature magnetic refrigeration10.1016/S0140-7007(03)00048-3 ↗
2. Smith · Eur. Phys. J. H · 2013 · 38 · 50710.1140/epjh/e2013-40001-9 ↗
3. Caballero-Flores · Phys. Condens. Matter · 2014 · 26 · 28600110.1088/0953-8984/26/28/286001 ↗
4. A. Conde Magnetocaloric effect: from materials research to refrigeration devices10.1016/j.pmatsci.2017.10.005 ↗
5. A review and new perspectives for the magnetocaloric effect: new materials and local heating and cooling inside the human body10.1016/j.ijrefrig.2016.04.020 ↗
6. A review of magnetic refrigerator and heat pump prototypes built before the year 201010.1016/j.ijrefrig.2010.04.002 ↗
7. Overview of existing magnetocaloric prototype devices
8. Thermal energy harvesting system based on magnetocaloric materials10.1051/epjap/2019180284 ↗
9. Ageing effect on the magnetocaloric properties of Gd, Gd5Si1.9Ge2.1 and on the eutectic composition Gd75Cd2510.1088/0022-3727/41/15/155004 ↗
10. Corrosion behavior of magnetic refrigeration material La–Fe–Co–Si in distilled water10.1016/j.jallcom.2010.12.122 ↗
11. Advanced materials for magnetic cooling: fundamentals and practical aspects Appl
12. Magnetic hysteresis loss and corrosion behavior of LaFe11.5Si1.5 particles coated with Cu10.1063/1.4795265 ↗
13. Structural and magnetocaloric properties of the new ternary silicides Gd6M5/3Si3 with M = Co and Ni10.1021/cm8000859 ↗
14. A core–shell phenomenon maintain the magnetocaloric properties of the ternary silicide Gd6Co1.67Si3 during water flux ageing10.1016/j.jallcom.2013.08.211 ↗
15. Study of XPS photoemission of some gadolinium compounds10.1016/0368-2048(91)85016-M ↗
16. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Cr, Mn, Fe, Co and Ni10.1016/j.apsusc.2010.10.051 ↗