journal article·2018-04

Structure and luminescence of core-shell phosphor aluminate-boron oxide

Chen-Yu Wu, Chien-Ming Lei, Toshiaki Takei, Rudder Wu, Shing-Hoa Wang, Chau-Chang Chou, Horng-Yi Chang

Publisher page

Abstract

Abstract Long-afterglow phosphor SrAl2O4: 0.01Eu2+, 0.01Dy3+ (SAO) requires a high sintering temperature of 1400 °C even when boric acid is added as flux via a solid-state reaction. The aluminum source NaAlO2 behaved as a good mineralizer in the designed hydrothermal process to achieve a large surface-to-thickness ratio of SAO. The flower-like shape of hydrothermally prepared hSAO without B2O3 after annealing at 1100 °C/4 h transformed into a rod-like plate phosphor with nano-thickness. Such a small rod-like plate exhibited higher photoluminescence (PL) intensity than large-grained B2O3-added bSAO prepared via a solid-state reaction. The annealed hSAOs inherited the morphology of the as-hydrothermally prepared aluminates. A nano-thick sheet of annealed aSAO containing B2O3 further enhanced the PL significantly and indicated a blue shift independent of the grain size. Furthermore, the nano-thick sheet of phosphors exhibited the same afterglow as the conventional tens-of-micrometers-sized phosphors. Fourier-transform infrared spectroscopy and X-ray diffraction results showed that the B O4 bond may substitute Al O4 in the structure and the B O3 bond is in a flux outside the annealed aSAO and bSAO grains. The molten flux formed a thin layer on the surface of the SAO particles to be a core-shell of the SAO-B2O3 structure, behaving as a diffusion-assistant medium and environmental protection layer against acid and humidity.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Luminescence Properties of Advanced Materials · Ammonia Synthesis and Nitrogen Reduction · Advanced Photocatalysis Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Long persistent phosphors - from fundamentals to applications10.1039/C5CS00582E ↗
2. Persistent phosphor SrAl2O4:Eu, Dy in outdoor conditions: saved by the trap distribution10.1364/OE.23.00A868 ↗
3. Studies on the persistent luminescence of Eu2+ and Dy3+ - doped SrAl2O4 phosphors: a review10.1007/s11164-012-0966-2 ↗
4. A new long phosphorescent phosphor with high brightness, SrAl2O4:Eu2+, Dy3+10.1149/1.1837067 ↗
5. Effects of composition on the long phosphorescent SrAl2O4 : Eu2 + , Dy3 + phosphor crystals10.1149/1.1837931 ↗
6. Role of B2O3 on the phase stability and long phosphorescence of SrAl2O4: Eu, Dy10.1016/S0925-8388(03)00009-4 ↗
7. Crystal chemistry of some AB2O4 compounds10.1111/j.1151-2916.1963.tb11755.x ↗
8. Megaw · 1973
9. Crystal structure of hexagonal SrAl2O4 at 1073K10.1016/j.jssc.2005.06.012 ↗
10. Phase transition in SrAl2O4
11. Tuning of emission colours in strontium aluminate long persisting phosphor10.1088/0022-3727/36/18/012 ↗
12. Synthesis of long afterglow phosphors doped B SrA12O4:Eu2+, Dy3+ and its luminescent properties10.1016/S1002-0721(07)60530-4 ↗
13. Phase evolution and thermal behaviors of the solid-state reaction between SrCO3 and Al2O3 to form SrAl2O4 under air and CO2-air atmospheres10.1016/j.ceramint.2011.10.077 ↗
14. Effect of B2O3 on long-last phosphorescence of SrAl2O4:Eu2+, Dy3+
15. Comparative study of optical and structural properties of micro-and nano crystalline SrAl2O4:Eu2+, Dy3+ phosphors10.1016/j.jlumin.2014.06.028 ↗
16. Mechanism of persistent luminescence in Eu2+ and Dy3+ codoped aluminate and silicate compounds10.1149/1.1926652 ↗
17. Mechanism of phosphorescence appropriate for the long afterglow phosphors Eu2+ doped with codopants Dy3+ and B3+10.1021/cm050763r ↗
18. Traps in SrAl2O4:Eu2+ phosphor with rare-earth ion doping10.1016/S0022-2313(97)00043-4 ↗
19. Persistent luminescence of Eu2+ doped alkaline earth aluminates, MAl2O3: Eu2+10.1016/S0925-8388(01)01084-2 ↗
20. Effect of temperature on the luminescence processes of SrAl2O4: Eu2+10.1016/j.radmeas.2004.01.031 ↗
21. Optical properties of rare earth doped strontium aluminate (SAO) phosphors: a review10.1134/S0030400X14110101 ↗
22. Effect of boron substitution on the preparation and luminescence of Eu2+ doped strontium aluminates10.1016/j.jallcom.2003.11.078 ↗
23. Nakamoto · 1963
24. A top-down method to fabricate SrAl2O4:Eu2+, Dy3+ nanosheets from commercial blocky phosphors10.1016/j.optmat.2014.02.010 ↗
25. Characterizations of Eu, Dy co-doped SrAl2O4 phosphors prepared by the solid-state reaction with B2O3 addition10.1016/j.jallcom.2007.07.078 ↗
26. Controlled synthesis of single-crystal SrAl2O4: Eu2+, Dy3+ nanosheets with long-lasting phosphorescence10.1016/j.jallcom.2010.04.186 ↗
27. Influence of precalcination and boron-doping on the initial photoluminescent properties of SrAl2O4: Eu, Dy phosphors10.1021/cg700719h ↗
28. Combustion synthesis and photoluminescence of SrAl2O4: Eu, Dy phosphor nanoparticles10.1016/S0167-577X(03)00499-3 ↗
29. Crystal field splitting of 5d states and luminescence mechanism in SrAl2O4:Eu2+ phosphor10.1016/j.jlumin.2016.10.015 ↗
30. Luminescent properties of (Sr, Zn)Al2O4: Eu2+, B3+ particles as a potential green phosphor for UV LEDs10.1021/cm060003w ↗
31. Fabrication of Eu:SrAl2O4-based glass ceramics using frozen sorbet method10.2109/jcersj2.119.609 ↗