Abstract

A comprehensive description of the phenomena at the low-alloy Fe-C-O-Ni steel/corundum interface at elevated temperatures up to 1600 °C was performed using the sessile drop method, Differential Thermal Analysis (DTA), 3D Differential Scanning Calorimetry (3D DSC) as well as several supporting methods, namely Energy Dispersive X-Ray (EDX), X-Ray Diffraction (XRD) analyses and Scanning Electron Microscopy (SEM). Steel samples with different carbon (0.04–1.56 wt%) and nickel (1.08–4.48 wt%) contents were selected to assess the effect of temperature and chemical composition on the related quantities, namely density, surface and interfacial tension, wetting angles, and the work of adhesion. While increased nickel content caused a decrease in wetting angle, and surface and interfacial tension values, the increased carbon content had the opposite effect. Two distinctly different modes of high-temperature interaction at the phase interface were also described. Little interaction was observed between the steel with lower carbon content (<0.1 wt%) and the corundum substrate. On the contrary, a more substantial interaction occurred in steel with higher carbon content and thus lower liquidus temperature . There was significant disruption of the corundum substrate at the surface and in depth up to 140 µm. The original corundum structure was replaced by new structural phases, particularly hibonite, grossite and gehlenite. In addition, when a higher chromium content was present in the steel, chromium-doped corundum was formed.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Development of processing map coupling grain size for the isothermal compression of 300 M steel10.1016/j.msea.2013.11.083 ↗
2. In-situ observations and modeling of static recrystallization in 300 M steel10.1016/j.msea.2019.138300 ↗
3. The microstructure of lath martensite in quenched 9Ni steel10.1016/j.actamat.2014.01.058 ↗
4. The growth behavior of austenite grain in the heating process of 300 M steel10.1016/j.msea.2011.02.089 ↗
5. Austenite grain refinement and isothermal growth behavior in a low carbon vanadium microalloyed steel10.1016/S1006-706X(14)60138-2 ↗
6. The surface tension of steels10.1007/s10853-005-1939-2 ↗
7. Surface tension measurements of 430 stainless steel10.2355/isijinternational.54.2104 ↗
8. Determination of the surface tension of liquid stainless steel10.1007/s10853-005-1931-x ↗
9. Surface tension of nickel, copper, iron and their binary alloys10.1007/s10853-005-1935-6 ↗
10. Surface tension and wettability studies of liquid Fe-Ni-O alloys10.1007/s11663-997-0113-4 ↗
11. The surface tension of undercooled binary iron and nickel alloys and the effect of oxygen on the surface tension of Fe and Ni10.1023/A:1022638400507 ↗
12. Effects of carbon and oxygen on Fe–C–O melt surface tension10.2355/isijinternational.53.1315 ↗
13. Studies of the wetting characteristics of liquid iron on dense alumina by the X-Ray sessile drop technique10.1007/s11663-003-0006-0 ↗
14. Investigation of the reactions between oxygen-containing iron and SiO2 substrate by X-ray sessile-drop technique10.1007/s11663-003-0035-8 ↗
15. Interfacial phenomena during wetting of graphite/alumina mixtures by liquid iron10.2355/isijinternational.43.1 ↗
16. Chemical interactions of alumina–carbon refractories with molten steel at 1823 K (1550 °C): Implications for refractory degradation and steel quality10.1007/s11663-011-9520-7 ↗
17. Carbothermic reduction of alumina at 1823 K: on the role of molten iron and reaction mechanisms10.2355/isijinternational.ISIJINT-2016-037 ↗
18. Reaction chemistry in dissolution of polycrystalline alumina in limealumina-silica slag, Brit
19. Alumina dissolution into silicate slag10.1111/j.1151-2916.2000.tb01291.x ↗
20. High – temperature interaction of molten Fe–C–O–Cr alloys with corundum10.1016/j.jallcom.2020.157128 ↗
21. AAxisymmetric Drop Shape Analysis (ADSA): An Outline10.1016/j.cis.2016.11.001 ↗
22. Melting behaviour of ferronickel slags10.1007/s11837-016-2140-6 ↗
23. Effects of basicity and FeO content on the softening and melting temperatures of the CaO-SiO2-MgO-Al2O3 slag system10.2320/matertrans.MRA2008372 ↗
24. Softening, melting, and permeation phenomena of CaO–FeO–SiO2 oxide on a coke bed10.2355/isijinternational.ISIJINT-2015-269 ↗
25. Effect of heating rate and sample geometry on the apparent specific heat capacity: DSC applications10.1016/j.tca.2011.02.033 ↗
26. Liquidus and solidus temperatures and latent heats of melting of steels10.1007/s10973-016-5942-4 ↗
27. Surface tension and density data for Fe–Cr–Mo, Fe–Cr–Ni, and Fe–Cr–Mn–Ni steels10.1007/s10853-015-9277-5 ↗
28. Surface and interfacial properties of Fe–C–O–Cr alloys in contact with Alumina10.2298/JMMB190621005N ↗
29. Effect of carbon and sulphur on the surface tension of molten iron10.1002/srin.200200001 ↗
30. Computer aided interfacial measurements10.2355/isijinternational.32.26 ↗
31. Role of interfacial phenomena in deoxidation process of molten iron10.1179/cmq.1983.22.1.19 ↗
32. Wetting of TaC by Liquid Cu and Liquid Ag10.1111/j.1151-2916.1972.tb11242.x ↗
33. Diffusion of chromium in sapphire: the effects of electron beam irradiation10.1016/j.jcrysgro.2011.01.049 ↗
34. Reaction mechanism in alumina/chromia (Al2O3–Cr2O3) solid solutions obtained by coprecipitation10.1111/j.1151-2916.2000.tb01508.x ↗
35. Crystal structure and properties of Al2O3-Cr2O3 solid solutions with different Cr2O3 contents10.1016/j.ceramint.2017.08.195 ↗
36. Chemistry of the aqueous phase of ordinary portland cement pastes at early reaction times10.1111/j.1151-2916.1998.tb02631.x ↗
37. Assessment of the CaO-Al2O3 system10.1111/j.1151-2916.1990.tb05083.x ↗
38. Mechanism of pore generation in calcium hexaluminate (CA6) ceramics formed in situ from calcined alumina and calcium carbonate aggregates10.1016/j.jeurceramsoc.2016.05.026 ↗
39. The capability of hibonite elongated grains to influence physical, microstructural, and mechanical properties of zirconia toughened alumina–CeO2–MgO ceramics10.1016/j.ijrmhm.2016.04.008 ↗