Mapping defects during phase transformation in high Cr content NiCr solid-solution through positron trapping
Source abstract
Abstract
Understanding the role of point defects towards hardening –and influence on secondary phase evolution demands a systematic investigation of defects during aging. In the present work, we investigate defects present/evolved during thermal aging in high Cr content NiCr solid-solution using positron annihilation lifetime and coincidence Doppler broadening spectroscopy. Thermal aging at the studied temperature results in phase transformation of the matrix primarily by discontinuous precipitation leading to Cr precipitation as revealed from field-effect scanning electron microscopy. Positron annihilation results reveal that non-equilibrium thermal (excess) vacancies are predominant defects in the studied alloy. These vacancies are retained in the alloy due to the formation of vacancy-solute complex. During solutionization treatment, the excess vacancies are largely recovered attaining an equilibrium vacancy concentration. On the other hand, excess vacancies are not recovered during thermal aging and stable up to 24 h aging period. In addition to vacancy-solute complex, dislocations are evolved at higher aging times and suggested to be present at the interface of Cr precipitate and matrix. Under the consideration of positron trapping model, the estimated atomic concentration of vacancies (vacancy-solute complex) in the phase transformed NiCr is ~ 10 −5 and the dislocation density is ~ 4 × 10 9 cm −2.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Muon and positron interactions and applications · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. Influence of composition on microstructural parameters of single crystal nickel-based superalloys10.1016/j.matchar.2012.05.001 ↗
2. Understanding the microstructure evolution of Ni-based superalloy within two different fretting wear regimes in high temperature high pressure water10.1016/j.scriptamat.2019.05.037 ↗
3. Room temperature tensile behavior of service exposed and thermally aged service exposed alloy 62510.1016/S1359-6462(01)00965-4 ↗
4. R.A. MacKay, T.P. Gabb, J.L. Smialek, M.V. Nathal, Low Density, High Creep Resistant Single Crystal Superalloys for Turbine Airfoils, US Patent 7,26 1,783 B1; August 28, 2007.
5. R. A. MacKay, T. P. Gabb, J.L. Smialek, M. V. Nathal, Alloy Design Challenge: Development of Low Density Superalloys for Turbine Blade Applications, NASA TM-2009-215819, National Aeronautics and Space Administration, Glenn Research Center, Cleveland, OH, October 2009. 〈http://ntrs.larc.nasa.gov〉.
6. The effect of phase chemistry on the extent of strengthening mechanisms in model Ni-Cr-Al-Ti-Mo based superalloys10.1016/j.actamat.2018.04.064 ↗
7. Unveiling the Re effect in Ni-based single crystal superalloys
8. Experimental investigation of the ordering pathway in a Ni-33at%Cr alloy10.1016/j.actamat.2016.06.014 ↗
9. Atomic ordering in the phases of a nickel-chromium-based superalloy10.1134/S0036029508060086 ↗
10. Kinetics and grain boundary selectivity of discontinuous precipitation in Ni-Cr alloy10.1007/s11661-017-4066-1 ↗
11. Phase stability of γ’-Ni2Cr and α-Cr in the Ni-Cr binary10.1016/j.actamat.2018.07.015 ↗
12. New Determination of solubility limit of Chromium in Ni-Cr solid solution10.1007/BF01602807 ↗
13. Structure of chromium-rich Cr-Ni, Cr-Fe, Cr-Co, and Cr-Ni-Fe alloy particles made by evaporation in argon10.1007/BF02647663 ↗
14. Effects of Al and Ta on the high temperature oxidation of Ni-based Superalloys10.1016/j.corsci.2014.10.025 ↗
15. Precipitation hardening in metals10.1179/026708399773002782 ↗
16. Precipitation hardening in Al–Mg–Si alloys with and without excess Si10.1016/S0921-5093(01)01247-3 ↗
17. Strengthening in rapidly solidified age hardened Cu-Cr and Cu-Cr-Zr alloys10.1016/S1359-6454(96)00142-5 ↗
18. Phase transformation strengthening of high-temperature superalloys10.1038/ncomms13434 ↗
19. Segregation assisted plasticity in Ni-based superalloys10.1007/s11661-018-4567-6 ↗
20. Segregation and η phase formation along stacking faults during creep at intermediate temperatures in a Ni-based superalloy10.1016/j.actamat.2015.08.053 ↗
21. Effect of different heat treatments on the microstructure and mechanical properties in selective laser melted INCONEL 718 alloy10.1080/10426914.2016.1257805 ↗
22. Coherent precipitation and strengthening in compositionally complex alloys: a review10.3390/e20110878 ↗
23. The precipitation sequence in Al-Mg-Si alloys10.1016/S1359-6454(98)00059-7 ↗
24. High tensile ductility in a nanostructured metal10.1038/nature01133 ↗
25. High-strength and high-ductility nanostructured and amorphous metallic materials10.1002/adma.201401595 ↗
26. Dislocation-particle interactions
27. On the origin of the extremely high strength of ultrafine-grained Al alloys produced by severe plastic deformation10.1016/j.scriptamat.2010.07.014 ↗
28. Grain boundary segregation induced strengthening of an ultrafine-grained austenitic stainless steel10.1016/j.matlet.2014.07.188 ↗
29. Grain boundary segregation engineering in metallic alloys: a pathway to the design of interfaces10.1016/j.cossms.2014.06.002 ↗
30. Strengthening CoCrNi medium-entropy alloy by tuning lattice defects10.1016/j.scriptamat.2020.07.027 ↗
31. Fine tuning of tensile properties in CrCoNi medium entropy alloy through cold rolling and annealing10.1016/j.intermet.2019.106578 ↗
32. Dislocation mechanisms and 3D twin architectures generate exceptional strength-ductility-toughness combination in CrCoNi medium-entropy alloy10.1038/ncomms14390 ↗
33. Lattice defects and their influence on the mechanical properties of bulk materials processed by severe plastic deformation10.2320/matertrans.MF201909 ↗
34. Radiation-accelerated precipitation in Fe–Cr alloys10.1016/j.actamat.2015.11.001 ↗
35. The role of excess vacancies in precipitation10.1016/0036-9748(69)90294-4 ↗
36. Transforming solid-state precipitates via excess vacancies10.1038/s41467-020-15087-1 ↗
37. Enhanced aging kinetics in Al-Mg-Si alloys by up-quenching
38. Origin of hardening in aged Al-Cu-Mg (Cu)10.1016/S1359-6454(97)00039-6 ↗
39. Response to comments on cluster hardening in an aged Al-Cu-Mg alloy10.1016/S1359-6462(98)00364-9 ↗
40. Origin of initial rapid age hardening in an Al-1.7at%Mg-1.1at%Cu alloy10.1080/095008399176689 ↗
41. Cellular precipitation in Ni51Cr lamellar eutectic and cast Ni44Cr alloy10.1007/BF02642009 ↗
42. Defect identification in semiconductors with positron annihilation: experiment and theory10.1103/RevModPhys.85.1583 ↗
43. The study of defects in crystals by positron annihilation10.1007/BF00884229 ↗
44. Current positron studies of structural modifications in age-hardenable metallic systems
45. Annealing process in quenched Al-Sn alloys: a positron annihilation study10.1103/PhysRevB.71.064106 ↗
46. Positron studies of solute aggregation in age-hardenable aluminum alloys10.1016/S0924-0136(02)01043-9 ↗
47. Microstructure evolution of heavily deformed AA5083 Al–Mg alloy studied by positron annihilation spectroscopy10.1016/j.apsusc.2014.01.064 ↗
48. Positron annihilation study on repeated deformation/precipitation aging in Fe–Cu–B–N alloys10.1007/s10853-013-7411-9 ↗
49. Segregation of Ni at early stages of radiation damage in NiCoFeCr solid solution alloys10.1016/j.actamat.2020.06.024 ↗
50. Self-healing of radiation-induced damage in Fe-Au and Fe-Cu alloys: Combining positron annihilation spectroscopy with TEM and ab initio calculations10.1016/j.jallcom.2019.152765 ↗
51. Characterization of lattice defects in metallic materials by positron annihilation spectroscopy: a review10.1016/j.jmst.2017.11.050 ↗
52. Positron studies of lattice defects in metals
53. P. Kirkegaard, J. V. Olsen, M. M. Eldrup, N.J. Pedersen. PALSfit. Roskilde: Danmarks Tekniske Universitet, Risø National laboratoriet for Bæredygtig Energi.(Denmark. Forsknings center Risoe. Risoe-R; No. 1652(EN)), 2009.
54. Direct evidence of Cd vacancies in CdSe nanoparticles: positron annihilation studies10.1140/epjb/e2011-20363-y ↗
55. On the Cr rich continuous and discontinuous precipitation kinetics in NiCr alloy by microstructural characterization and differential calorimetric analysis10.1016/j.matlet.2021.129887 ↗
56. Positron lifetime calculation for the elements of periodic table10.1088/0953-8984/19/17/176222 ↗
57. Positron annihilation study of vacancy-type defects in high-speed deformed Ni, Cu and Fe, Material10.1016/S0921-5093(02)00705-0 ↗
58. Defect energetics of concentrated solid-solution alloys from ab-initio calculations: Ni0.5Co0.5, Ni0.5Fe0.5, Ni0.8Fe0.2 and Ni0.8Cr0.210.1039/C6CP05161H ↗
59. Chromium-vacancy clusters in dilute bcc Fe-Cr alloys: an ab initio study10.1016/j.jnucmat.2017.10.038 ↗
60. The 3d-shell electrons in NiAl-based alloys containing Cr and Co studied by positron annihilation10.1016/j.jallcom.2004.06.016 ↗
61. Theory of positron in solids and on solid surfaces10.1103/RevModPhys.66.841 ↗
62. Positron affinity for elemental metals10.1088/0953-8984/1/35/008 ↗
63. Positron annihilation in Cr, Cu and Au layers embedded in Al and quantum confinement of positron in Au clusters10.1103/PhysRevB.84.014106 ↗
64. Determination of absolute defect concentrations for saturated positron trapping – deformed polycrystalline Ni as a case study10.1016/j.nimb.2005.04.130 ↗
65. Positron annihilation study on precipitation in Al-22at%Zn alloy10.4028/www.scientific.net/MSF.3.379 ↗
66. Vacancy concentrations in quenched binary alloys10.1016/0001-6160(80)90005-X ↗
67. The Cr-Ni system10.1007/BF02867812 ↗
68. dissertation on Ab-initio based modelling of radiation effects in the Ni-Fe-Cr system
69. Positron annihilation in semiconductors edited by R. Krause-Rehberg and H. S. Leipner, Hartmut, Springer Series in Solid State Sciences, 127, 1999.
70. Positron trapping rate into vacancy clusters10.1007/BF00885942 ↗
71. On the empirical determination of positron trapping coefficient at nano-scale helium bubbles in steels irradiated in spallation target10.1016/j.jnucmat.2018.03.045 ↗
72. Identification of a Ni-vacancy defect in Ni-Mn- Z (Z = Ga, Sn, In): An experimental and DFT positron-annihilation study10.1103/PhysRevB.99.064108 ↗
73. Vacancies and carbon impurities in α-iron: Electron irradiation10.1103/PhysRevB.25.762 ↗
74. Impurity-induced vacancy clustering in cold-worked, nickel10.1088/0305-4608/9/10/007 ↗
75. Positron annihilation investigation for an estimation of dislocation density and vacancy concentration of plastically deformed polycrystalline Ni of different purity10.1002/pssa.2210340239 ↗