Microstructural evolution of lamellar freeze-cast Fe-Cu-Ni foams during oxidation/reduction cycling
Source abstract
Abstract
A novel iron-based alloy, Fe-15Cu-10Ni (wt%), has been introduced as a candidate for storage energy of iron air batteries. Cyclical experiments involving steam oxidation and hydrogen reduction were conducted on the Fe-15Cu-10Ni (wt%), lamellar foams fabricated by freeze-casting method, and were compared with the Fe-25Cu and Fe-25Ni alloys with the same foam structure. The experiments were carried out at a high temperature of 800 °C, which is relevant to the energy storage in iron-air batteries. Scanning electron microscopy, energy-dispersive X-ray spectroscopy, and X-ray diffraction techniques are employed to analyze the microstructure and chemical evolution of the cycled foams. Upon oxidation, Fe-15Cu-10Ni lamellae form a core rich in Ni and Cu (since Cu and Ni do not oxidize under steam), surrounded by an Fe 3O 4 shell. This reduces fractures and slows down the growth of Kirkendall pores, thereby delaying the sintering and densification of the foam structure. Upon reducing Fe 3O 4 , the Fe-rich shells and the Cu-rich and Ni-rich cores homogenize, creating a reversible microstructure after a complete redox cycle. The Fe-15Cu-10Ni composition presents notable advantages compared to Fe-25Ni, exhibiting a higher oxidation rate, increased energy density, and lower cost. As a result, Fe-15Cu-10Ni emerges as the optimal composition within the scope of this study, showcasing superior properties.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen Storage and Materials · Catalysis and Hydrodesulfurization Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Iron–air battery operating at high temperature10.1002/ente.201600438 ↗
2. High performance solid-state iron-air rechargeable ceramic battery operating at intermediate temperatures (500–650 °C)
3. Electrochemical characterization of Fe-air rechargeable oxide battery in planar solid oxide cell stacks10.1016/j.jpowsour.2016.10.059 ↗
4. Electrochemical properties of Fe2O3 microparticles and their application in Fe/air battery anodes10.1016/j.jallcom.2015.09.170 ↗
5. An intermediate-temperature solid oxide iron-air redox battery operated on O2- chemistry and loaded with pd-catalyzed iron-based energy storage material10.1021/acsenergylett.6b00529 ↗
6. Characteristics of Fe-air battery using Y2O3-stabilized-ZrO2 electrolyte with Ni-Fe electrode and Ba0.6La0.4CoO3-δ electrode operated at intermediate temperature10.1016/j.est.2016.06.003 ↗
7. A review of the iron-air secondary battery for energy storage10.1002/cplu.201402238 ↗
8. Fe-air rechargeable battery using oxide ion conducting electrolyte of Y2O3 stabilized ZrO210.1016/j.jpowsour.2012.11.121 ↗
9. Redox cycling stability of Fe2 NiO4/YSZ composite storage materials for rechargeable oxide batteries10.1016/j.ensm.2020.02.032 ↗
10. Development of storage materials for high-temperature rechargeable oxide batteries10.1016/j.est.2014.12.001 ↗
11. Proton-mediated energy storage in intermediate-temperature solid-oxide metal–air batteries
12. Simulation of solid oxide iron-air battery: effects of heat and mass transfer on charge/discharge characteristics10.1016/j.jpowsour.2015.03.149 ↗
13. Application of iron-based materials in heterogeneous advanced oxidation processes for wastewater treatment: A review10.1016/j.cej.2020.127191 ↗
14. Renewable hydrogen production from biogas using iron-based chemical looping technology
15. Iron-iminopyridine complexes as charge carriers for non-aqueous redox flow battery applications10.1016/j.ensm.2021.01.035 ↗
16. A high-performance all-iron non-aqueous redox flow battery10.1016/j.jpowsour.2019.227331 ↗
17. Recent progress of metal-air batteries-a mini review
18. Iron-based flow batteries to store renewable energies10.1007/s10311-018-0709-8 ↗
19. Enhanced reversibility and durability of a solid oxide fe–air redox battery by carbothermic reaction derived energy storage materials10.1039/C3CC47673A ↗
20. Evaluation of microstructural changes and performance degradation in iron-based oxygen carriers during redox cycling for chemical looping systems with image analysis10.1021/acs.iecr.7b04966 ↗
21. Metallic architectures from 3D-printed powder-based liquid inks10.1002/adfm.201503921 ↗
22. Effects of bridging fibers on the evolution of lamellar architecture during H2/H2O redox cycling of Fe-foams10.1016/j.actamat.2022.118543 ↗
23. Microstructural evolution of paramagnetic materials by magnetic freeze casting10.1016/j.jmrt.2018.12.024 ↗
24. Intrinsic and extrinsic control of freeze casting10.1016/j.jmrt.2018.11.011 ↗
25. Pore morphology evolution and atom distribution of doped Fe2O3 foams developed by freeze-casting after redox cycling10.1016/j.jmrt.2021.06.008 ↗
26. Structural evolution of directionally freeze-cast iron foams during oxidation/reduction cycles10.1016/j.actamat.2018.09.054 ↗
27. In operando tomography reveals degradation mechanisms in lamellar iron foams during redox cycling at 800 °C10.1016/j.jpowsour.2019.227463 ↗
28. Finite element model for coupled diffusion and elastoplastic deformation during high-temperature oxidation of Fe to FeO10.1149/1945-7111/ab8ed4 ↗
29. A comprehensive review on the development of solid-state metal–air batteries operated on oxide-ion chemistry
30. Hierarchical structural changes during redox cycling of fe-based lamellar foams containing YSZ, CeO2, or ZrO210.1021/acsami.0c05107 ↗
31. Evolution of lamellar architecture and microstructure during redox cycling of Fe-Co and Fe-Cu foams10.1016/j.jallcom.2022.165606 ↗
32. Evolution of directionally freeze-cast Fe2O3 and Fe2O3+NiO green bodies during reduction and sintering to create lamellar Fe and Fe-20Ni foams
33. Fe-Ni foams self-heal during redox cycling: Via reversible formation/homogenization of a ductile Ni scaffold10.1039/D0TA06813F ↗
34. Effects of pore morphology on the cyclical oxidation/reduction of iron foams created via camphene-based freeze casting10.1016/j.jallcom.2020.156278 ↗
35. Cu-YSZ cermet solid oxide fuel cell anode prepared by high-temperature sintering10.1016/j.jpowsour.2009.12.003 ↗
36. Directional solidification with constant ice front velocity in the ice-templating process10.1002/adem.201500235 ↗
37. Computing local thickness of 3D structures with ImageJ10.1017/S1431927607074430 ↗
38. Reduction-based engineering of three-dimensional morphology of Ni-rGO nanocomposite10.1016/j.mseb.2021.115259 ↗
39. Electro-deposited nano-Ni/reduced graphene oxide composite film of corrugated surface for high voltammetric sensitivity10.1016/j.matchemphys.2022.127288 ↗
40. Chemical looping and oxygen permeable ceramic membranes for hydrogen production - a review10.1039/c2ee03470k ↗
41. Exchange correlation length and magnetoresistance in Fe-Cu and Fe-Cu-Ni melt-spun ribbons10.1209/0295-5075/26/9/011 ↗
42. Structural and microstructural properties of nanocrystalline Cu-Fe-Ni powders produced by mechanical alloying10.1016/j.powtec.2014.03.064 ↗
43. I. Gallino, Phase Diagram, Thermal Stability, and High Temperature Oxidation of the Ternary Cu-Ni-Fe System, Doctoral dissertation, Oregon State University, (2003).
44. Performance of solid oxide iron-air battery operated at 550°C10.1149/2.085308jes ↗
45. Cyclic durability of a solid oxide Fe-air redox battery operated at 650°C10.1149/2.048310jes ↗
46. Microstructural evolution of lamellar Fe-25Ni foams during steam-hydrogen redox cycling10.1016/j.actamat.2022.118148 ↗
47. Structure and high-temperature oxidation behaviour of Cu-Ni-Fe alloys prepared by high-energy ball milling for application as inert anodes in aluminium electrolysis10.1016/j.corsci.2010.06.011 ↗
48. Mechanism of solid state diffusion on the performance evolution of iron-based oxygen carrier at different operating conditions for chemical looping process10.1016/j.fuel.2022.125699 ↗
49. Improved redox performance of Fe2O3/Al2O3 oxygen carrier via element doping in chemical looping combustion10.1016/j.fuproc.2021.107030 ↗