journal article·2025-11

In-situ TiC-reinforced titanium nanocomposite synthesized via multi-pass friction stir processing with nanodiamond additions

Reza Madadi, Seyed Mohammad Hassan Pishbin, Seyed Mahmood Fatemi, Jae-Hyung Cho, Sang-Ho Han

Publisher page

Abstract

An in-situ titanium matrix composite (TMC) was fabricated via exothermic reactions between titanium and nanodiamonds (NDs) during friction stir processing (FSP). The reactions led to the formation of TiC nanoparticles, which subsequently acted as coherent nucleation sites for the a-phase upon cooling. Tungsten, introduced into the matrix from the FSP tool, played a decisive role in stabilizing the ß-phase at room temperature. The combined effects of dynamic recrystallization within the ß-phase and the pinning action of the nano-TiC phase on a-grains facilitated the development of an ultrafine-grained (UFG) equiaxed α+β microstructure. As a result, the mechanical performance of pure Ti was significantly enhanced, with yield strength and ultimate tensile strength increasing by approximately 140% and 85%, respectively, while maintaining a reasonable elongation of 10.6%.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Titanium metal matrix composites: an overview10.1016/j.compositesa.2019.04.005 ↗
2. Opportunities and issues in the application of titanium alloys for aerospace components10.3390/met10060705 ↗
3. Friction stir welding of titanium alloys: a review10.1016/j.matdes.2017.12.033 ↗
4. Orientation structural mapping and textural characterization of a CP-Ti/HA surface nanocomposite produced by friction-stir processing10.1016/j.surfcoat.2019.06.009 ↗
5. Microstructure and mechanical properties of in-situ nano TiC reinforced Ni-based alloy composites prepared by spark plasma sintering10.1016/j.jmst.2024.04.004 ↗
6. Development of in situ composites via reactive friction stir processing of Ti–B4C system10.1016/j.compositesb.2019.05.067 ↗
7. In-situ synthesized TiC/Ti-6Al-4V composites by elemental powder mixing and spark plasma sintering: microstructural evolution and mechanical properties10.1016/j.jallcom.2023.169557 ↗
8. Synthesis and mechanical properties of TiCx and Ti(C,N)reinforced Titanium matrix in situ composites by reactive spark plasma sintering10.1016/j.msea.2019.05.021 ↗
9. Microstructure and property evolutions of titanium/nano-hydroxyapatite composites in-situ prepared by selective laser melting10.1016/j.jmbbm.2017.02.021 ↗
10. Microstructure evolution and mechanical properties of in-situ Ti6Al4V–TiB composites manufactured by selective laser melting10.1016/j.compositesb.2020.108567 ↗
11. In-situ integrated fabrication of Ti-Ni coating during hot isostatic pressing of Ti6Al4V parts: microstructure and tribological behavior10.1016/j.surfcoat.2015.09.007 ↗
12. In-situ TiB/Ti-6Al-4V composites with a tailored architecture produced by hot isostatic pressing: microstructure evolution, enhanced tensile properties and strengthening mechanisms10.1016/j.compositesb.2019.01.080 ↗
13. In-situ fabrication of Ti-TiCx metal matrix composite by laser powder bed fusion with enhanced elastic modulus and superior ductility10.1016/j.matdes.2024.113499 ↗
14. Microstructural evolution and wear properties of in-situ (TiB + TiC)-reinforced Ti6Al4V matrix composite coating by laser melting deposition10.1016/j.matchar.2023.113192 ↗
15. Friction stir processing: a novel technique for fabrication of surface composite10.1016/S0921-5093(02)00199-5 ↗
16. Friction stir welding/processing of metals and alloys: a comprehensive review on microstructural evolution10.1016/j.pmatsci.2020.100752 ↗
17. Fabrication of TiCp/Ti-6Al-4V surface composite via friction stir processing (FSP): process optimization, particle dispersion-refinement behavior and hardening mechanism10.1016/j.msea.2013.03.019 ↗
18. Mechanical and tribological characterization of industrial wastes reinforced aluminum alloy composites fabricated via friction stir processing10.1016/j.jallcom.2020.154832 ↗
19. Study on the microstructure and mechanical properties of hot rolled nano-ZrB2/AA6016 aluminum matrix composites by friction stir processing
20. Enhancing mechanical, and tribological properties of aluminum metal matrix composite reinforced with high entropy alloy using friction stir processing10.1016/j.matchemphys.2025.130614 ↗
21. Preparation of graphene nanoplatelets reinforced aluminum matrix composites by friction stir processing and study of thermal conductivity and toughness properties
22. Strengthening analyses and mechanical assessment of Ti/Al2O3 nano-composites produced by friction stir processing10.1016/j.msea.2015.02.038 ↗
23. Microstructural evolution and mechanical properties of a friction-stir processed Ti-hydroxyapatite (HA) nanocomposite10.1016/j.jmbbm.2018.08.025 ↗
24. Production of Ti-CNTs surface nanocomposites for biomedical applications by friction stir processing: microstructure and mechanical properties10.1016/j.matlet.2021.130138 ↗
25. Mechanical properties and corrosion behavior of titanium surface biocomposites reinforced with Al2O3 particles fabricated by friction stir processing10.1016/j.matchemphys.2023.128749 ↗
26. Titanium particulate reinforced AZ31 magnesium matrix composites with improved ductility prepared using friction stir processing10.1016/j.msea.2019.138793 ↗
27. Synergistic effects of hybrid (HA+Ag) particles and friction stir processing in the design of a high-strength magnesium matrix bio-nano composite with an appropriate texture for biomedical applications10.1016/j.jmbbm.2021.104983 ↗
28. Hybrid GA-ANN and GA-ANFIS soft computing approaches for optimizing tensile strength in magnesium-based composites fabricated via friction stir processing
29. Enhancing microstructure, mechanical strength, and electrical conductivity in Cu – W composites through multi-pass friction stir processing and pre-strain techniques10.1016/j.jmrt.2025.04.213 ↗
30. Investigating the tribological characteristics of copper surface composites reinforced with high entropy alloy (AlCoCrCuFe) through friction stir processing10.1038/s41598-023-49557-5 ↗
31. Production of in-situ hard Ti/TiN composite surface layers on CP-TI using reactive friction stir processing under nitrogen environment10.1016/j.surfcoat.2012.12.028 ↗
32. In situ intermetallics-reinforced composite prepared using multi-pass friction stir processing of copper powder on a Ti6Al4V Alloy10.3390/ma15072428 ↗
33. The properties and applications of nanodiamonds10.1038/nnano.2011.209 ↗
34. Tribological properties, thermal conductivity and corrosion resistance of titanium/nanodiamond nanocomposites10.1016/j.coco.2018.06.008 ↗
35. Pulsed direct current field-induced thermal stability and phase transformation of nanodiamonds to carbon onions10.1039/C9RA01022J ↗
36. Friction stir processing of pure titanium/nanodiamonds nanocomposites: microstructure, tribological and corrosion properties
37. Titanium/nanodiamond nanocomposites: effect of nanodiamond on microstructure and mechanical properties of titanium10.1016/j.matdes.2017.06.015 ↗
38. Constructing micro-network of Ti2Cu and in-situ formed TiC phases in titanium composites as new strategy for significantly enhancing strength10.1016/j.coco.2023.101787 ↗
39. Microstructural changes due to friction stir processing of investment-cast Ti-6Al-4V10.1007/s11661-006-9061-x ↗
40. On dynamic recrystallization during the friction stir processing of commercially pure Ti and its influence on the microstructure and mechanical properties10.3390/met14060644 ↗
41. Nanodiamonds reinforced titanium matrix nanocomposites with network architecture10.1016/j.compositesb.2018.11.110 ↗
42. Improving tribological properties of CP-Ti by in-situ fabrication of Ti-WC surface composite using a pinless WC-Co stirring tool10.1007/s11771-024-5748-7 ↗
43. Barin · 1995
44. Effect of rotational speed on friction stir welding microstructure and properties of cast and rolled (ZrB2 + Al3Zr) particle-reinforced aluminum matrix composites10.1007/s10853-024-10283-6 ↗
45. Coherent and semi-coherent interfaces induced high strength-plasticity compatibility of (Ti+Al)p/AZ31 composites prepared by laser melt injection10.1016/j.jallcom.2025.181173 ↗
46. Carbon in commercially pure titanium10.3390/ma16020711 ↗
47. Phase stability of the amorphous phase and non-equilibrium phase in a β Ti-Zr-based shape memory alloy10.1016/j.scriptamat.2021.113721 ↗
48. A novel strategy for developing α + β dual-phase titanium alloys with low Young’s modulus and high yield strength10.1016/j.jmst.2020.11.018 ↗
49. A semi-empirical approach to the prediction of deformation behaviors of β-Ti alloys10.1016/j.scriptamat.2018.08.035 ↗
50. Ultrahigh yield strength and large uniform elongation achieved in ultrafine-grained titanium containing nitrogen10.1016/j.actamat.2022.118356 ↗
51. The mechanism for an orientation dependence of grain boundary strengthening in pure titanium10.1016/j.ijplas.2022.103276 ↗
52. A study on the hardness variation of α- and β-pure titanium with different grain sizes10.1016/j.msea.2005.03.004 ↗
53. Microstructural interpretation of negligible strain-hardening behavior of submicrometer-grained low-carbon steel during tensile deformation10.1007/s11661-002-0134-1 ↗
54. An analysis of the strain hardening behavior of ultra-fine grain pure titanium10.1016/j.scriptamat.2006.01.034 ↗