Various ways including substitution and protection used to improve the cyclability of ‘MgNi’ electrodes
Source abstract
Abstract
Three different treatments have been investigated to improve the cyclability in KOH electrolyte of ‘MgNi’ used as hydrogen storage electrode material for Ni–MH batteries. Whereas hydrophobic molecule grafting does not give significant improvement, replacement of Mg by Ti or coating the ‘MgNi’ powder with copper in a supercritical CO2–EtOH mixture increase strongly the resistance of the electrode against hydroxylation: the capacity after 12 cycles is 98% higher for ‘Mg0.5Ti0.5Ni’ and 45% higher after coating by a thin copper film in comparison with the raw ‘MgNi’ material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen Storage and Materials · Advanced Battery Materials and Technologies · Ammonia Synthesis and Nitrogen Reduction
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. Orimo · Intermetallics · 1998 · 6 · 18510.1016/S0966-9795(97)00064-2 ↗
2. Lei · Z. Phys. Chem. · 1994 · 183 · 141910.1524/zpch.1994.183.Part_1_2.379 ↗
3. Iwakura · J. Alloys Comp. · 1998 · 270 · 14210.1016/S0925-8388(98)00517-9 ↗
4. Holtz · J. Mater. Sci. · 1997 · 32 · 226710.1023/A:1018572116447 ↗
5. Song · J. Mater. Sci. · 1995 · 30 · 134310.1007/BF00356142 ↗
6. Lenain · J. Solid State Electrochem. · 1998 · 2 · 28510.1007/s100080050102 ↗
7. Diaz · Int. J. Hydrogen Energy · 1979 · 4 · 44510.1016/0360-3199(79)90104-6 ↗
8. Liu · J. Alloys Comp. · 1997 · 261 · 28910.1016/S0925-8388(97)00220-X ↗
9. Han · J. Alloys Comp. · 2000 · 306 · 21910.1016/S0925-8388(00)00753-2 ↗
10. Pessey · J. Alloys Comp. · 2001 · 323–324 · 41210.1016/S0925-8388(01)01100-8 ↗
11. Ruggeri · J. Alloys Comp. · 2002 · 339 · 19510.1016/S0925-8388(01)01972-7 ↗
12. Bobet · Intermetallics · 2002 · 10 · 59710.1016/S0966-9795(02)00033-X ↗
13. Plueddemann · 1982