Hydrogen absorption in amorphous and quasicrystalline Ti45Ni17Zr38 powders synthesized by mechanical alloying
Source abstract
Abstract
Abstract Hydrogen absorption in amorphous and quasicrystalline Ti 45 Ni 17 Zr 38 powders, obtained both directly by mechanical alloying (MA) and after subsequent annealing, was studied. MA was performed in a planetary ball mill under protective argon atmosphere. The powders were hydrogenated at 503 and 573 K under initial pressure of 2.9 kPa. Hydrogen absorption of the as-milled amorphous samples led to formation of TiH 2 , ZrH 2 and (ZrTi)H 2 hydrides. Hydrogenation of quasicrystalline phase resulted in formation of hydrogen solution in quasicrystalline phase and ZrH 2 . The maximum registered concentration of H 2 in the samples was 1.38 H/M. Quasicrystalline phase disappeared after partial degassing up to 1.25 H/M. Activation energies of hydrogen absorption and hydrogen evolution were measured, these values were found as 40.4 ± 0.2 and 25.2 ± 0.1 kJ/mol correspondingly.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Quasicrystal Structures and Properties · Metallic Glasses and Amorphous Alloys · Mineralogy and Gemology Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (7)
Show source-provided references
1. Viano · Phys. Rev. B · 1995 · 51 · 1202610.1103/PhysRevB.51.12026 ↗
2. Kelton · 1997 · 272
3. Kelton · 1997 · 261
4. Kelton · MRS Bull. · 1997 · 22 · 6910.1557/S0883769400034473 ↗
5. Gibbons · 1999 · 403
6. Takasaki · Philos. Mag. Lett. · 2002 · 82 · 35310.1080/09500830210136390 ↗
7. Majzoub · Mater. Sci. Eng. A · 2000 · 10810.1016/S0921-5093(00)01092-3 ↗