journal article·2000-04

Effect of annealing period on the resistive transitions and AC losses in a Bi1.6Pb0.4Sr2Ca3Cu4O12 superconductor fabricated by a wet technique

S. Nezir, S. Çelebi, M. Altunbaş

Journal of Alloys and Compounds· Volume 302· Issue 1-2
Publisher page

Abstract

Abstract We estimated the irreversibility lines from the resistive-superconducting transition in DC magnetic fields up to 1 T for the Bi 1.6 Pb 0.4 Sr 2 Ca 3 Cu 4 O 12 superconducting samples prepared by liquid ammonium nitrate with the same heat treatment but 25 h and 200 h of annealing time. Increasing the annealing time from 25 h to 200 h at 840°C shifted the irreversibility temperature to a higher temperature. A non-linear Arrhenius plot of the resistive tail has been found. The activation energy obtainable from Arrhenius plots seems to be non-linear temperature dependent. The peak temperature T p , in the imaginary part of the AC susceptibility seems to be shifted to a higher temperature by nearly the same amount as the shift in irreversibility temperature with increasing annealing time. Temperature variation of the critical current density extracted from the theoretical calculation of matrix susceptibility and irreversibility line obey the same power law dependence of (1− T / T c ) n , where n =2.7 and 2.5 for the 25-h and 200-h samples, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Physics of Superconductivity and Magnetism · Magnetic and transport properties of perovskites and related materials · Advanced Condensed Matter Physics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Palstra · Phys. Rev. B · 1990 · 41 · 662110.1103/PhysRevB.41.6621 ↗
2. Yeshurun · Phys. Rev. Lett. · 1988 · 60 · 220210.1103/PhysRevLett.60.2202 ↗
3. Tinkham · Phys. Rev. Lett. · 1988 · 61 · 165810.1103/PhysRevLett.61.1658 ↗
4. Palstra · Phys. Rev. Lett. · 1988 · 61 · 166210.1103/PhysRevLett.61.1662 ↗
5. Inui · Phys. Rev. Lett. · 1989 · 63 · 242110.1103/PhysRevLett.63.2421 ↗
6. Han · Physica C · 1999 · 311 · 2910.1016/S0921-4534(98)00631-5 ↗
7. Schilling · Physica C · 1993 · 216 · 610.1016/0921-4534(93)90626-2 ↗
8. Ateş · J. Alloys Comp. · 1998 · 268 · 21510.1016/S0925-8388(97)00463-5 ↗
9. Çelebi · J. Alloys Comp. · 1998 · 268 · 25610.1016/S0925-8388(97)00613-0 ↗
10. Müller · Phys. Rev. Lett. · 1987 · 58 · 114310.1103/PhysRevLett.58.1143 ↗
11. Brandt · Physica C · 1991 · 185 · 27010.1016/0921-4534(91)91984-C ↗
12. Iye · Jpn. J. Appl. Phys. Pt. 2 · 1987 · 26 · L105710.1143/JJAP.26.L1057 ↗
13. Oh · Phys. Rev. B · 1988 · 37 · 786110.1103/PhysRevB.37.7861 ↗
14. Fang · Phys. Rev. B · 1988 · 37 · 233410.1103/PhysRevB.37.2334 ↗
15. Sagdahl · Phys. Rev. B · 1990 · 42 · 679710.1103/PhysRevB.42.6797 ↗
16. Nezir · 1996
17. Gencer · Supercond. Sci. Technol. · 1996 · 9 · 46710.1088/0953-2048/9/6/005 ↗
18. Batista-Levya · Physica C · 1999 · 314 · 7310.1016/S0921-4534(99)00144-6 ↗
19. Xu · Phys. Rev. B · 1990 · 42 · 875610.1103/PhysRevB.42.8756 ↗
20. Gapud · Phys. Rev. B · 1999 · 59 · 20310.1103/PhysRevB.59.203 ↗
21. Chen · Cryogenics · 1989 · 29 · 80010.1016/0011-2275(89)90153-7 ↗
22. Çelebi · Physica C · 1999 · 316 · 25110.1016/S0921-4534(99)00284-1 ↗
23. Bean · Rev. Mod. Phys. · 1964 · 36 · 3110.1103/RevModPhys.36.31 ↗
24. Clem · Physica C · 1988 · 153 · 5010.1016/0921-4534(88)90491-1 ↗