Sm12Co59Cu6Fe20Zr3 sintered magnets made from as-cast alloy and melt-spun ribbons

Ji-bing Sun, Zhe-xu Zhang, Chun-xiang Cui, Wei Yang, Liang Li, Dan Han, Li-guo Yang, Li-jie Li

Journal of Alloys and Compounds· Volume 486· Issue 1-2
Publisher page

Abstract

Abstract A comparative study between Sm12Co59Cu6Fe20Zr3 master alloy magnet and melt-spun ribbon magnet is made by applying the same traditional sintering-solid solution-aging-slow cooling method. The X-ray diffractometer, electron microscope and magnetometer are employed to investigate the structure and magnetic properties of the magnets. It is found that two types of sintered magnets are formed both of which have Th2Zn17-type main phase. Master alloy sintered magnet has a typical cellular structure, with average cell size of 88.3 nm and cell wall width less than 20 nm, and the comprehensive magnetic properties are: Hci = 21.1 kOe, Mr = 75.9 emu/g and Ms9T = 107.8 emu/g. The coercivity of the ribbons melt-spun at a speed of 20 m/s is merely 2.1 kOe, while in ribbon sintered magnet, this value can approach as high as 27.4 kOe, together with remanence 61.8 emu/g and maximum magnetization Ms9T = 103.6 emu/g. A typical cellular–lamellar microstructure is obtained in ribbon sintered magnet, with average cell size of 102.3 nm, cell wall width less than 10 nm and lamellar size of 1–3 nm. The high-coercivity of ribbon sintered magnet can be attributed to the following factors: the existence of lamellar phases, larger cell size, thinner cell walls, more cell boundary phases and desirable composition distribution.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials · Magnetic Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Walmer · IEEE Trans. Magn. · 2000 · 36 · 337610.1109/20.908807 ↗
2. Kim · J. Appl. Phys. · 1998 · 83 · 671510.1063/1.367936 ↗
3. Kim · J. Appl. Phys. · 1997 · 81 · 560910.1063/1.364615 ↗
4. Kronmüller · J. Magn. Magn. Mater. · 2004 · 272–276 · e31910.1016/j.jmmm.2003.11.384 ↗
5. Goll · J. Appl. Phys. · 2004 · 96 · 653410.1063/1.1809250 ↗
6. Kronmüller · Scripta Mater. · 2003 · 48 · 83310.1016/S1359-6462(02)00619-X ↗
7. Kronmüller · Scripta Mater. · 2002 · 47 · 54510.1016/S1359-6462(02)00177-X ↗
8. Tang · J. Magn. Magn. Mater. · 2001 · 226 · 136510.1016/S0304-8853(00)00912-4 ↗
9. Hadjipanayis · IEEE Trans. Magn. · 2000 · 36 · 338210.1109/20.908808 ↗
10. Crabbe · IEEE Trans. Magn. · 1994 · 30 · 69610.1109/20.312380 ↗
11. Gopalan · J. Appl. Phys. · 2004 · 95 · 496210.1063/1.1688446 ↗
12. Gopalan · J. Magn. Magn. Mater. · 2005 · 295 · 710.1016/j.jmmm.2004.12.033 ↗
13. Yan · Mater. Sci. Eng. A · 2004 · 375–377 · 116910.1016/j.msea.2003.10.223 ↗
14. Yan · J. Magn. Magn. Mater. · 2005 · 290–291 · 120610.1016/j.jmmm.2004.11.386 ↗
15. Gjoka · Mater. Sci. Eng. B · 2008 · 152 · 8110.1016/j.mseb.2008.06.003 ↗
16. Panagiotopoulos · J. Magn. Magn. Mater. · 2002 · 242–245 · 130410.1016/S0304-8853(01)01272-0 ↗
17. Sun · J. Alloys Compd. · 2009 · 476 · 57510.1016/j.jallcom.2008.09.052 ↗
18. Sun · Mater. Sci. Eng. B · 2009 · 157 · 7210.1016/j.mseb.2008.12.019 ↗
19. Goll · Appl. Phys. Lett. · 2000 · 76 · 105410.1063/1.125936 ↗
20. Makridis · IEEE Trans. Magn. · 2002 · 38 · 292210.1109/TMAG.2002.803068 ↗
21. Babita · J. Alloys Compd. · 2007 · 432 · 2310.1016/j.jallcom.2006.06.003 ↗
22. Zhang · J. Appl. Phys. · 2005 · 97 · 10H10710.1063/1.1853851 ↗
23. Gutfleisch · Acta Mater. · 2006 · 54 · 99710.1016/j.actamat.2005.10.026 ↗
24. Tang · J. Magn. Magn. Mater. · 2000 · 221 · 26810.1016/S0304-8853(00)00508-4 ↗
25. Gopalan · Scripta Mater. · 2009 · 60 · 76410.1016/j.scriptamat.2009.01.006 ↗
26. Makridis · J. Magn. Magn. Mater. · 2008 · 320 · 232210.1016/j.jmmm.2008.04.122 ↗