Mechanical milling of Sn–Mo powder mixtures and electrochemical performance in lithium ion batteries

Y. Liang, Y. Liu, Z.J. Jia

Journal of Alloys and Compounds· Volume 474· Issue 1-2
Publisher page

Abstract

Abstract Sn–Mo powder mixtures have been processed through mechanical milling method. The microstructure, morphology, and electrochemical performance of the powders were investigated by X-ray diffraction, scanning electron microscopy, energy dispersive X-ray spectroscopy, inductively coupled plasma mass spectroscopy and electrochemical methods. The material delivered a discharge capacity of more than 484 mAh g −1 , and a reversible volumetric capacity of 2499 mAh/cm 3 , which is three times larger than that of graphite electrode. Meanwhile, the powder mixture sintered at 850 °C for 3 h exhibited better cycle life.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Morimoto · J. Electrochem. Soc. · 1999 · 146 · 397010.1149/1.1392578 ↗
2. Pereira · Solid State Ionics · 2004 · 167 · 2910.1016/j.ssi.2004.01.001 ↗
3. Zhang · J. Power Sources · 2002 · 112 · 59610.1016/S0378-7753(02)00483-4 ↗
4. Harreld · J. Power Sources · 2003 · 115 · 1910.1016/S0378-7753(02)00626-2 ↗
5. Wang · Chem. Mater. · 2005 · 17 · 389910.1021/cm050724f ↗
6. Courtney · J. Electrochem. Soc. · 1997 · 144 · 294310.1149/1.1837941 ↗
7. Wang · J. Power Sources · 2005 · 146 · 48710.1016/j.jpowsour.2005.03.055 ↗
8. Kim · J. Electrochem. Soc. · 2000 · 147 · 441110.1149/1.1394079 ↗
9. Courtney · J. Electrochem. Soc. · 1997 · 144 · 204510.1149/1.1837740 ↗
10. Belliard · J. Power Sources · 2001 · 97–98 · 21910.1016/S0378-7753(01)00544-4 ↗
11. Zhang · J. Electrochem. Soc. · 2007 · 154 · A710.1149/1.2374949 ↗
12. Dahn · J. Electrochem. Soc. · 2006 · 153 · A121110.1149/1.2194631 ↗
13. Todd · J. Electrochem. Soc. · 2006 · 153 · A199810.1149/1.2257985 ↗
14. Tamura · J. Power Sources · 2002 · 107 · 4810.1016/S0378-7753(01)00979-X ↗
15. Sakaguchi · J. Power Sources · 2003 · 119–121 · 5010.1016/S0378-7753(03)00123-X ↗
16. Kim · J. Power Sources · 2003 · 119–121 · 10610.1016/S0378-7753(03)00134-4 ↗
17. Arbizzani · J. Power Sources · 2006 · 158 · 63510.1016/j.jpowsour.2005.06.042 ↗
18. Rönnebro · Solid State Ionics · 2005 · 176 · 274910.1016/j.ssi.2005.08.007 ↗
19. Mukaibo · Electrochem. Solid State Lett. · 2003 · 6 · A21810.1149/1.1602331 ↗
20. Tamura · Electrochim. Acta · 2004 · 49 · 194910.1016/j.electacta.2003.12.024 ↗
21. Sivashanmugam · J. App. Electrochem. · 2005 · 35 · 104510.1007/s10800-005-9043-5 ↗
22. Mao · J. Electrochem. Soc. · 1999 · 146 · 40510.1149/1.1391622 ↗
23. Fernández · Electrochim. Acta · 2006 · 51 · 339110.1016/j.electacta.2005.10.002 ↗
24. Koch · Intermetallics · 1996 · 4 · 33910.1016/0966-9795(96)00001-5 ↗
25. Morimoto · Electrochem. Solid State Lett. · 2001 · 4 · A1610.1149/1.1339239 ↗