Abstract
In situ age hardening phenomenon observed in as-sprayed Al-Sc binary alloys is reported. This, along with substantial grain refinement in the as-sprayed alloys exhibited hardness in the range of 605 MPa (Al-0.3 wt% Sc) to 923 MPa (Al-0.8 wt% Sc) that are comparable to the optimum hardness values typically obtained by age hardening in similar as-cast alloys. Transmission electron microscopy of the spray deposits revealed densely spaced Al3Sc precipitates of about 10 nm suggesting in-situ age hardening of these alloys during spray forming. This behavior is attributed to the inherent heating cycle associated with the spray forming process and the rapid kinetics of Al3Sc precipitation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al (Sc) alloys10.1016/S1359-6454(02)00201-X ↗
2. The aging of Al-0.3 at.% Sc alloy
3. On the solubility of group IV elements (Ti, Zr, Hf) in liquid aluminum below 800 °C10.1007/s11669-013-0278-2 ↗
4. Some comments on the misfit and coherency loss of Al3Sc particles in Al–Sc alloys10.1016/j.scriptamat.2005.02.023 ↗
5. Effect of scandium on recrystallization of aluminum and its alloys10.4028/www.scientific.net/MSF.331-337.793 ↗
6. A study of coarsening, recrystallization, and morphology of microstructure in Al-Sc-(Zr)-(Mg) alloys10.1007/s11661-004-0135-3 ↗
7. Scandium in aluminium alloys10.1179/174328005X14311 ↗
8. Metastable state diagram of the Al-Sc system in the range rich in aluminium
9. Extension of the N-model to predict competing homogeneous and heterogeneous precipitation in Al-Sc alloys10.1016/S1359-6454(02)00540-2 ↗
10. The effect of cooling rate on the morphology of primary Al3Sc intermetallic particles in Al–Sc alloys10.1016/S1359-6454(01)00050-7 ↗
11. Spray forming10.1016/0079-6425(95)00004-6 ↗
12. https://imagej.nih.gov/ij/ (Accessed on 3rd May 2016).
13. Rapid solidification processing with specific application to aluminium alloys10.1179/imr.1992.37.1.1 ↗
14. Structural state and decomposition kinetics in rapidly quenched Al - Sc, Al-Mg-Sc alloys10.4028/www.scientific.net/MSF.396-402.763 ↗
15. Grain refining in A356 alloys
16. Kinetics of precipitation in Al-Sc alloys and low temperature solid solubility of scandium in aluminium studied by electrical resistivity measurements10.1016/0921-5093(93)90401-Y ↗
17. On the addition of precipitation- and work-hardening in an Al–Sc alloy10.1016/j.msea.2006.09.164 ↗
18. The effect of Sc additions on the microstructure and age hardening behavior of as cast Al–Sc alloys10.1016/j.matdes.2012.06.019 ↗
19. Spray casting of steel strip: process analysis10.1007/BF02647318 ↗
20. Three dimensional atom probe investigation on the formation of Al3(Sc, Zr)-dispersoids in aluminium alloys10.1016/j.scriptamat.2004.03.033 ↗
21. Effect of yttrium and chromium on the recrystallization of Al–Sc alloys10.1134/S0036029507040131 ↗
22. Precipitation in cold-rolled Al–Sc–Zr and Al–Mn–Sc–Zr alloys prepared by powder metallurgy10.1016/j.matchar.2013.09.010 ↗
23. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
24. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
25. Determination of elasto-plastic properties by instrumented sharp indentation: guidelines for property extraction10.1016/S1359-6462(00)00311-0 ↗
26. Determination of elastoplastic properties by instrumented sharp indentation10.1016/S1359-6462(99)00011-1 ↗
27. Computational modeling of the forward and reverse problems in instrumented sharp indentation10.1016/S1359-6454(01)00295-6 ↗