Obtaining of reinforced Cu-Ti, Cu-Ti-TiB2 foils through green compact laser sintering
Source abstract
Abstract
Abstract Homogenized Cu-4Ti (wt%) and Cu-4Ti-1.4B (wt%) powders were cold pressed and then sintered by pulsed, millisecond Nd:YAG laser system. Phases present in laser sintered samples were characterized by X-ray diffraction (XRD), while quantitative chemical analysis of the sintered samples was conducted using inductively coupled plasma-atomic emission spectrometry (ICP-AES). The microstructure of powders and laser sintered foils was examined with scanning electron microscope with an energy dispersive X-ray spectroscope (EDS). Optical microscopy was used also for microstructural characterization of the foils. The tensile test was carried out using a universal testing machine with a crosshead speed of 0.5 mm/min at room temperature. Foils with dimensions 20 × 6 × 0.4 mm were used for tensile testing. In the obtained Cu-Ti foils, after aging at 550 °C for 4 h, rapidly solidified structure and metastable Cu4Ti precipitates affected high degree of copper matrix strengthening (peak aged). In Cu-Ti-TiB2 foils, after aging at 550 °C for 3 h, rapidly solidified structure, as well as the presence of TiB2 particles and metastable Cu4Ti precipitates, also affected high degree of copper matrix strengthening which, thanks to the ceramic particles, is retained at longer times (6 h). Fractured surfaces were observed with an optical microscope. It was determined that the best structural and mechanical properties of laser-sintered foils were reached using the following parameters: laser frequency 4 Hz, laser pulse duration 9 ms, pulse energy ∼20 J, number of scans 2.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Advanced materials and composites · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Mechanical alloying of high-strength copper alloys containing TiB2 and Al2O3 dispersoid particles10.1016/0956-716X(94)90267-4 ↗
2. Preparation and properties of TiB2 particle reinforced copper matrix composites by in situ processing10.1016/S0167-577X(01)00442-6 ↗
3. Spray forming of metal matrix composites10.1179/pom.1994.37.2.123 ↗
4. Formation of a TiB2-reinforced copper-based composite by mechanical alloying and hot pressing10.1007/s11661-002-0228-9 ↗
5. Strengthening of Cu-Ti alloys by addition of boron10.1179/mst.1992.8.12.1108 ↗
6. Synthesis and properties of a Cu-Ti-TiB2 composite hardened by multiple mechanisms10.1016/j.msea.2011.07.061 ↗
7. Metallurgical mechanisms in direct laser sintering of Cu-CuSn-CuP mixed powder10.1016/j.jallcom.2006.08.040 ↗
8. Balling phenomena during direct laser sintering of multi-component Cu-based metal powder10.1016/j.jallcom.2006.06.011 ↗
9. Laser sintering of Cu-Zr-ZrB2 composite10.1016/j.apsusc.2014.10.021 ↗
10. www.allfoils.com.
11. High-quality PVD graphene growth by fullerene decomposition on Cu foils10.1016/j.carbon.2017.04.067 ↗
12. Growth of millimeter-size single crystal graphene on Cu foils by circumfluence chemical vapor deposition
13. www.nmm.jx-group.co.jp.
14. In-situ processing of TiB2 nanoparticle-reinforced copper matrix composites10.2298/SOS0902143B ↗
15. Carslaw · 1959
16. Hardening by spinodal decomposition10.1016/0001-6160(63)90022-1 ↗
17. Hardening by spinodal modulated structure10.1016/0001-6160(80)90163-7 ↗
18. Precipitation hardening10.1007/BF02670416 ↗
19. Size effects in tensile testing of thin cold rolled and annealed Cu foil10.1016/j.msea.2005.10.060 ↗