journal article·2000-11

Hydrogen absorption and electrode properties of Zr1−xTixV1.2Cr0.3Ni1.5 Laves phases

Dan Lupu, Alexandru Sorin Biriş, Alexandru Radu Biriş, Ioan Mişan, Emil Indrea

Journal of Alloys and Compounds· Volume 312· Issue 1-2
Publisher page

Abstract

Abstract Substitution of titanium for zirconium in Zr 1− x Ti x V 1.2 Cr 0.3 Ni 1.5 ( x =0.25; 0.4; 0.6) results in the C15 cubic phase as the main component, the lattice parameter decreasing with increasing Ti content. The desorption isotherms show sloping plateaux and the dehydriding enthalpy decreases with the increasing x . The discharge capacity of the hydride electrode shows remarkable constancy up to 200 cycles for Zr 0.4 Ti 0.6 V 1.2 Cr 0.3 Ni 1.5 (238 mAh g −1 ).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fuel Cells and Related Materials · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Lupu · J. Alloys Comp. · 1999 · 291 · 28910.1016/S0925-8388(99)00273-X ↗
2. Bououdina · J. Alloys Comp. · 1997 · 253–254 · 30210.1016/S0925-8388(96)02901-5 ↗
3. Griessen · 1988 · Vol. 63 · 247
4. Shaltiel · J. Less-Common Met. · 1980 · 73 · 32910.1016/0022-5088(80)90326-4 ↗
5. Züttel · J. Alloys Comp. · 1997 · 253–254 · 58710.1016/S0925-8388(96)02989-1 ↗
6. Joubert · J. Alloys Comp. · 1997 · 253–254 · 56410.1016/S0925-8388(96)03088-5 ↗
7. Knosp · J. Electrochem. Soc. · 1998 · 145 · 147810.1149/1.1838507 ↗
8. Miyamura · Z. Phys. Chem. · 1994 · 183 · S34710.1524/zpch.1994.183.Part_1_2.347 ↗