journal article·2010-03

Microstructure and electron properties of Sm modified lead calcium titanate ceramics

Sarabjit Singh, Chandra Prakash, K.K. Raina

Journal of Alloys and Compounds· Volume 492· Issue 1-2
Publisher page

Abstract

Abstract Lead calcium titanate ceramics modified by partial substitution of rare earths for lead, particularly, (Pb, Sm, Ca)(Ti, Mn)O 3 ceramics, were explored for their structural, dielectric and piezoelectric properties. These modified ceramics with a composition of Pb 0.76−3 x /2 Sm x Ca 0.24 Ti 0.98 Mn 0.02 O 3 ( x = 0 − 0.08) were prepared by solid state reaction route. The XRD study showed single-phase formation with tetragonal structure. Lattice anisotropy ( c / a ) was found to decrease from 1.057 to 1.023 with increase in Sm substitution from 0 to 8 mol%, respectively. Microstructural study revealed the average grain size between 1.2 and 2.2 μm. The relative density was found to increase from 95% to 98.4% with increase in samarium substitution from 0 to 8 mol%, respectively. Detailed dilatometric study was performed in order to study the shrinkage behaviour during the sintering schedule. The maximum shrinkage was found to occur between 900 °C and 1100 °C. The dielectric constant ( ɛ ′) and loss (tan δ ) for all the compositions were investigated over a wide frequency (100 Hz to 1 MHz) and temperature (25–450 °C) range. The room temperature (25 °C) dielectric constant was found to increase from 130 (at 10 kHz) for pure lead calcium titanate sample to 380 (at 10 kHz) for 8 mol% samarium substituted sample and also showed a decreasing trend with increase in the frequency for all the substitutions (0–8 mol% Sm). Curie temperature, T C (determined from the plot of ɛ ′ vs. temperature) and tan δ were found to decrease with increasing samarium content. The Curie temperature was found to decrease from 348 °C to 192 °C for 0–8 mol% Sm substitutions, respectively. Piezoelectric coefficients were also measured at room temperature. Electromechanical anisotropy ( k t / k p ) was observed to increase from 11.7 (0 mol% Sm) to 27 (8 mol% Sm). Piezoelectric anisotropy ( d 33 / d 31 ) was also observed to increase from 22.5 for un-substituted sample to 28 for the sample substituted with 8 mol% samarium. The experimental results successfully showed that samarium substitution not only reduces the lattice anisotropy but also helps in improving piezoelectric properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Acoustic Wave Resonator Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Ikegami · J. Acoust. Soc. Am. · 1971 · 50 · 106010.1121/1.1912729 ↗
2. Takahashi · Ceram. Bull. · 1990 · 69 · 691
3. Ueda · Jpn. J. Appl. Phys. · 1972 · 11 · 45010.1143/JJAP.11.450 ↗
4. Mendiola · Ferroelectrics · 1988 · 29 · 1249
5. Takeuchi · 1986 · 402
6. Iijima · Am. Ceram. Soc. Bull. · 1987 · 66 · 699
7. Ahmed · 1992 · 520
8. Rittenmeyer · Ferroelectrics · 1990 · 110 · 17110.1080/00150199008008914 ↗
9. Banno · 1990 · 67
10. Takeuchi · J. Acoust. Soc. Am. · 1982 · 72 · 111410.1121/1.388319 ↗
11. Yamashita · Jpn. J. Appl. Phys. · 1981 · 20 · 18310.7567/JJAPS.20S4.183 ↗
12. Xue · 1994 · 101
13. Shenglin · Piezoelect. Acoust. · 1995 · 17 · 26
14. Ueda · Jpn. J. Appl. Phys. · 1968 · 7 · 23610.1143/JJAP.7.236 ↗
15. Duran · J. Mater. Sci. · 1988 · 23 · 446310.1007/BF00551945 ↗
16. Duran · J. Mater. Sci. · 1989 · 24 · 44710.1007/BF01107425 ↗
17. Singh · Int. J. Mod. Phys. B · 2006 · 20 · 31510.1142/S0217979206033280 ↗
18. Singh · Phase Trans. · 2005 · 78 · 65510.1080/01411590500271235 ↗
19. Singh · J. Phys. D: Appl. Phys. · 2005 · 38 · 162110.1088/0022-3727/38/10/018 ↗
20. Fukumoto · Ferroelectrics · 1982 · 40 · 21710.1080/00150198208218171 ↗
21. Rittenmyer · J. Acoust. Soc. Am. · 1986 · 79 · 207310.1121/1.393165 ↗
22. Mendiola · Ferroelectrics · 1989 · 94 · 18310.1080/00150198908014251 ↗
23. Rhodes · 1995
24. Masao · J. Am. Ceram. Soc. · 2001 · 84 · 246910.1111/j.1151-2916.2001.tb01037.x ↗
25. Snow · J. Am. Ceram. Soc. · 1973 · 56 · 9110.1111/j.1151-2916.1973.tb12365.x ↗
26. Kingon · J. Am. Ceram. Soc. · 1983 · 66 · 25310.1111/j.1151-2916.1983.tb15708.x ↗
27. Swartz · Mater. Res. Bull. · 1982 · 17 · 124510.1016/0025-5408(82)90159-3 ↗
28. Randall · J. Mater. Res. · 1990 · 8 · 88010.1557/JMR.1993.0880 ↗
29. Prakash · Ferroelectrics · 2001 · 262 · 32110.1080/00150190108225169 ↗
30. Prakash · Mater. Lett. · 2003 · 57 · 231010.1016/S0167-577X(02)01217-X ↗
31. Voltzke · Solid State Sci. · 2000 · 2 · 14910.1016/S1293-2558(00)00128-X ↗
32. Singh · Physica B · 2005 · 355 · 28010.1016/j.physb.2004.11.010 ↗
33. Singh · Physica B · 2005 · 369 · 6410.1016/j.physb.2005.07.039 ↗
34. Thakur · Phase Trans. · 2003 · 76 · 56710.1080/01411590290030708 ↗
35. Okazaki · Ceram. Bull. · 1984 · 63 · 1150
36. Lines · 1977
37. Gurevich · 1971
38. Frutos · Ferroelectrics · 1992 · 126 · 34110.1080/00150199208227083 ↗
39. Jaffe · Proc. IRE · 1961 · 49 · 116110.1109/JRPROC.1961.287917 ↗
40. Jimenez · Ferroelectrics · 1988 · 87 · 9710.1080/00150198808201373 ↗