An improved method to dissolve alloyed plutonium residues

L. Pescayre, C. Passot, D. Cardonna, H. Chollet

Publisher page

Abstract

Abstract An improved method to dissolve alloyed plutonium has been investigated. The purpose is to recycle plutonium residues which contain gallium greater than 15 wt%. The process consists of two main steps: oxidation by a moist Ar/O2 mixture and then HNO3/HF dissolution. The burning process is shown to be efficient to oxidize only the plutonium. The only oxide species obtained is PuO2, which is suitable for a HNO3/HF dissolution at 70 °C. The global recovery yield is higher than 97%.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear materials and radiation effects · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (3)

Show source-provided references
1. Tsarenko · At. Energ. · 2000 · 89/6 · 95410.1023/A:1011366803541 ↗
2. Haschke · J. Alloys Compd. · 2001 · 320 · 5810.1016/S0925-8388(01)00932-X ↗
3. Scott Barney · J. Inorg. Nucl. Chem. · 1977 · 39 · 166510.1016/0022-1902(77)80123-1 ↗