Microstructure and Vickers hardness of mechanically alloyed and spark plasma sintered Ti-2Zn-22Si-11B and Ti-6Zn-22Si-11B alloys
Source abstract
Abstract
Abstract This work reports on effect of zinc and milling time on microstructure and Vickers hardness of mechanically alloyed and spark plasma sintered (66,7-x)Ti-xZn-22,2Si-11,1B alloys (at.-%, with x = 2 and 6 at.-%). Ball milling at different times (20, 60, 180 and 300 min) was performed under argon atmosphere in a planetary ball mill from these elemental powder mixtures. Cylinder bodies with 10 mm diameter were consolidated by spark plasma sintering (1100 °C, 12 min, 20 MPa) under argon atmosphere. As-milled powders and sintered Ti-Zn-Si-B samples were evaluated by X-ray diffraction, scanning electron microscopy, energy dispersive spectrometry, laser diffraction particle size analysis, and Vickers hardness tests. It was noted a similar behavior during ball milling of Ti-Zn-Si-B powder mixtures. Only the α-Ti and Si peaks were indexed in XRD patterns of Ti-Zn-Si-B powders milled for 300 min. Rietveld refining indicated that the amount of amorphous structures has increased during milling up to 300 min, which was more pronounced for the Ti-6Zn-22Si-11B powders. The particle sizes of the Ti-2Zn-22Si-11B and Ti-6Zn-22Si-11B powder mixtures increased during milling from 94 (20 min) to 156 (300 min) μm and from 101 (20 min) to 136 (300 min) μm, respectively. Coherently, the average specific surface area of powder particles was continuously reduced during milling. Despite the adopted parameters, the SPS process produced dense Ti-xZn-22Si-11B (x = 2 and 6 at.-%) alloys with 98% from their theoretical specific mass. Regardless of milling time, the Ti6Si2B formation was inhibited in microstructure of the spark plasma sintered Ti-6Zn-22Si-11B alloy previously milled for longer times. EDS analysis indicated that the Ti6Si2B phase dissolved close to 1.8 at.-% Zn. Beside the TiB and Ti5Si3, the Ti2Zn and Ti3Zn (not explored) phases were also found in microstructure of sintered Ti-Zn-Si-B alloys. The Ti-2Zn-22Si-11B alloy presented average Vickers hardness values higher than 1050 HV whereas the Ti-6Zn-22Si-11B alloy varied between 970 and 1036 HV, which could be associated with the Ti6Si2B formation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Kopova · Mat. Sci. Eng. C – Mater. · 2016 · 60 · 23010.1016/j.msec.2015.11.043 ↗
2. Mohammed · J. Alloys Compd. · 2015 · 634 · 27210.1016/j.jallcom.2015.02.095 ↗
3. Ozan · J. Mech. Behav. Biomed. · 2018 · 78 · 22410.1016/j.jmbbm.2017.11.025 ↗
4. Mohammed · Karbala Int. J. Modern Sci. · 2017 · 3 · 22410.1016/j.kijoms.2017.08.005 ↗
5. Chen · Nonferrous Metal. Soc. · 2006 · 16 · s82410.1016/S1003-6326(06)60308-7 ↗
6. Kunčická · Prog. Mater. Sci. · 2017 · 88 · 23210.1016/j.pmatsci.2017.04.002 ↗
7. Ramos · Intermetallics · 2004 · 12 · 48710.1016/j.intermet.2004.01.001 ↗
8. Silva · Intermetallics · 2006 · 14 · 58510.1016/j.intermet.2005.08.005 ↗
9. Kato · Mat. Sci. Eng. C – Mater. · 2009 · 29 · 98010.1016/j.msec.2008.08.022 ↗
10. Fernandes · Surf. Coating. Technol. · 2013 · 228 · 19510.1016/j.surfcoat.2013.04.029 ↗
11. Ramos · J. Alloys Compd. · 2014 · 601 · 9410.1016/j.jallcom.2014.02.179 ↗
12. Zanardo · Mater. Sci. Forum · 2014 · 802 · 910.4028/www.scientific.net/MSF.802.9 ↗
13. Ferreira · Mater. Sci. Forum · 2014 · 802 · 2010.4028/www.scientific.net/MSF.802.20 ↗
14. Khajuria · Mat. Sci. Eng. C – Mater. · 2016 · 63 · 7810.1016/j.msec.2016.02.062 ↗
15. Vassilev · Alloys Compd. · 2004 · 375 · 16210.1016/j.jallcom.2003.11.026 ↗
16. Okamoto · Binary Alloy Phase Diagr. · 1990 · 1 · 559
17. Olesinski · Bull. Alloy Diagr. · 1985 · 6 · 54510.1007/BF02887156 ↗
18. A profile refinement method for nuclear and magnetic structures10.1107/S0021889869006558 ↗
19. Quantitative phase Analysis from neutron powder diffraction data using the rietveid method theory10.1107/S0021889887086199 ↗
20. The Scherrer equation versus the ‘Debye-Scherrer equation’10.1038/nnano.2011.145 ↗
21. R factors in Rietveld analysis: how good is good enough?10.1154/1.2179804 ↗
22. Rietveld refinement guidelines
23. A profile refinement method for nuclear and magnetic structures10.1107/S0021889869006558 ↗
24. ASTM: C-1327-15 · 2015 · 1
25. Phase stability and cohesive properties of Ti–Zn intermetallics: first-principles calculations and experimental results10.1016/j.actamat.2006.04.038 ↗
26. On the eutectoid transformation behavior of the Ti-Zn system and its metastable phases10.1016/j.jallcom.2017.05.103 ↗
27. Chepulskii · 2009