Post annealing effect on transport properties of La0.67Ca0.33MnO3 films grown on vicinal cut substrates
Source abstract
Abstract
Abstract La0.67Ca0.33MnO3 thin films have been grown on 10°, 15°, and 20° vicinal cut SrTiO3 (1 0 0) substrates by pulse laser deposition. The single phase and the least textured growth have been studied by X-ray diffraction analysis. The post annealing effect with high temperature and high oxygen pressure on the transport properties of films has been investigated by resistance versus temperature measurements. Films with post annealing show large enhancement of metal–insulator transition temperature Tp about 20–30 K towards higher temperature and obvious decrease of resistance, which is attributed to the refilling of oxygen, the change of Mn–O–Mn angle and the improvement of crystallinity by the post annealing effect. Specially, film on 20° vicinal cut substrate exhibits the biggest range gap of peak resistance drop, which may originate from more defects caused by steps at this tilt angle and many of these defects are removed after post annealing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic and transport properties of perovskites and related materials · Advanced Condensed Matter Physics · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. 2000
2. H. Fukuzawa, H. Yuasa, H. Fuke, H. Iwasaki, M. Sahashi, United States Patent 7,593,195 (2009).
3. Prellier · J. Phys.: Condens. Matter · 2001 · 13 · R91510.1088/0953-8984/13/48/201 ↗
4. Egilmez · Appl. Phys. Lett. · 2008 · 92 · 16251510.1063/1.2908931 ↗
5. Paranjape · Phys. Rev. B · 2003 · 67 · 21441510.1103/PhysRevB.67.214415 ↗
6. Xiong · J. Appl. Phys. · 2005 · 97 · 0839099
7. Prellier · Appl. Phys. Lett. · 1999 · 75 · 144610.1063/1.124720 ↗
8. Zhang · J. Alloys Compd. · 2009 · 457 · 8810.1016/j.jallcom.2007.12.045 ↗
9. Salvato · J. Appl. Phys. · 2005 · 97 · 10371210.1063/1.1898451 ↗
10. Choi · Appl. Phys. Lett. · 2001 · 78 · 35310.1063/1.1338972 ↗
11. Yu · J. Cryst. Growth · 2011 · 322 · 4110.1016/j.jcrysgro.2011.03.010 ↗
12. Habermeier · Solid State Commun. · 1999 · 110 · 47310.1016/S0038-1098(99)00111-8 ↗
13. Li · J. Magn. Magn. Mater. · 2000 · 211 · 23210.1016/S0304-8853(99)00739-8 ↗
14. Zhao · Physica B · 2005 · 373 · 7210.1016/j.physb.2005.10.135 ↗
15. Zhang · Opt. Laser Technol. · 2004 · 36 · 34110.1016/j.optlastec.2003.09.018 ↗
16. Zhang · J. Nanomater. · 2008 · 2008 · 32960110.1155/2008/329601 ↗
17. Hong · Phys. Rev. Lett. · 2005 · 95 · 09550110.1103/PhysRevLett.95.095501 ↗
18. Soltan · Phys. Rev. B · 2004 · 70 · 14451710.1103/PhysRevB.70.144517 ↗
19. Dijkkamp · Appl. Phys. Lett. · 1987 · 51 · 61910.1063/1.98366 ↗
20. Gross · J. Magn. Magn. Mater. · 2000 · 211 · 2210.1016/S0304-8853(99)00708-8 ↗
21. Ju · Phys. Rev. B · 1995 · 51 · 614310.1103/PhysRevB.51.6143 ↗
22. Haghiri-Gosnet · J. Phys. D · 2003 · 36 · R12710.1088/0022-3727/36/8/201 ↗