Enhanced thermoelectric figure of merit by composite effects and low thermal conductivity in distrontium silicide (Sr2Si)
Source abstract
Abstract
Abstract The thermoelectric properties of Sr2Si, Sr5Si3, and their composites are reported. Sr2Si-Sr5Si3 composites were synthesized by partial decomposition of Sr2Si to Sr5Si3 during spark plasma sintering. Semiconducting Sr2Si grains were surrounded by boundary regions composed of smaller grains of Sr2Si, metallic Sr5Si3, and semiconducting Sr3SiO. Addition of the Sr5Si3 phase reduced the electrical resistivity from 1.69 × 10−3 Ωm to 6.45 × 10−5 Ωm at room temperature, which corresponded to the samples having no and the maximum amount of the Sr5Si3 phase, respectively. The electrical resistivity decreased; however, the Seebeck coefficient slightly increased to 157 μV/K at 773 K, and the thermal conductivity was approximately constant. Therefore, the power factor and ZT monotonically increased with an increase in the amount of the Sr5Si3 phase in the composite samples, which confirmed almost no effect resulted from the Sr3SiO phase. A low thermal conductivity was demonstrated by Sr2Si (ca. 1 W/mK at 776 K), which resulted from weaker atomic bonds, heavier atomic mass, greater atomic volume, and a greater number of atoms in the unit cell. A further enhancement of ZT can be achieved for higher amounts of Sr5Si3 and at higher temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Superconductivity in MgB2 and Alloys · Thermal Expansion and Ionic Conductivity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Lattice stability of intermediate phases of the Sr–Si system10.1016/j.jallcom.2007.03.023 ↗
2. Thermoelectric silicides: past, present and future
3. Highly effective Mg2Si1−xSnx thermoelectrics10.1103/PhysRevB.74.045207 ↗
4. The p-type Mg2LixSi0.4Sn0.6 thermoelectric materials synthesized by a B2O3 encapsulation method using Li2CO3 as the doping agent10.1039/C5TC03692E ↗
5. Thermoelectric properties of BaSi2, SrSi2, and LaSi10.1063/1.2778747 ↗
6. Electrical properties of Ca2Si sintered compact synthesized by spark plasma sintering10.1016/j.phpro.2011.01.038 ↗
7. Effect of Na addition on electric properties of Ca2Si sintered compacts10.1088/1757-899X/18/14/142014 ↗
8. The effect of crystallite size on thermoelectric properties of bulk nanostructured magnesium silicide (Mg2Si) compounds10.1063/1.3684615 ↗
9. Fabrication and thermoelectric properties of Mg2Si-based composites using reduction reaction with additives10.1016/j.intermet.2012.08.026 ↗
10. High performance thermoelectrics from earth-abundant materials: enhanced figure of merit in PbS by second phase nanostructures10.1021/ja208658w ↗
11. Enhanced thermoelectric properties of Mg2Si by addition of TiO2 nanoparticles10.1063/1.3675512 ↗
12. Effect of trivalent Bi doping on the Seebeck coefficient and electrical resistivity of Ca3Co4O910.1007/s11664-015-3924-0 ↗
13. Comparison of thermoelectric properties of nanostructured Mg2Si, FeSi2, SiGe, and nanocomposites of SiGe–Mg2Si, SiGe–FeSi210.1063/1.4966138 ↗
14. Synthesis and characterization of Bi-doped Mg2Si thermoelectric materials10.1016/j.jssc.2012.05.004 ↗
15. Vanadium concentration dependence of thermoelectric properties of β-rhombohedral boron Prepared by spark plasma sintering10.2320/matertrans.M2010272 ↗
16. Hybrid effect to possibly overcome the trade-off between Seebeck coefficient and electrical conductivity10.1016/j.scriptamat.2015.09.010 ↗
17. In situ synthesis and thermoelectric properties of PbTe–graphene nanocomposites by utilizing a facile and novel wet chemical method10.1039/c3ta12494k ↗
18. The phase diagram of the Sr–Si system10.1016/j.jallcom.2003.11.003 ↗
19. Electronic structures of semiconducting alkaline-earth metal silicides10.1016/S0925-8388(03)00037-9 ↗
20. MgSrSi-type compounds as a possible new family of thermoelectric materials10.1007/s11664-012-2226-z ↗
21. Lattice stability of Ca, Sr and Yb disilicides10.1016/j.intermet.2006.01.061 ↗
22. Vapor pressures and thermodynamic properties of strontium silicides10.1016/j.intermet.2005.10.008 ↗
23. Theory of enhancement of thermoelectric properties of materials with nanoinclusions10.1103/PhysRevB.77.214304 ↗
24. Microstructural effects on thermoelectric efficiency: a case study on magnesium silicide10.1016/j.actamat.2014.05.041 ↗
25. Synthesis and characterization of Al-doped Mg2Si thermoelectric materials10.1007/s11664-013-2482-6 ↗
26. Spark plasma sintering and thermoelectric evaluation of nanocrystalline magnesium silicide (Mg2Si)10.1007/s10853-012-6959-0 ↗
27. Thinking like a chemist: intuition in thermoelectric materials10.1002/anie.201508381 ↗
28. Unique nanostructures and enhanced thermoelectric performance of melt-spun BiSbTe alloys10.1063/1.3097026 ↗
29. Enhancement of thermoelectric performance driven by Ge substitution in SrSi2 alloy10.1088/0022-3727/46/31/315303 ↗
30. Si/Ge–WSi2 composites: processing and thermoelectric properties10.1016/j.actamat.2015.07.025 ↗
31. Bismuth doped Mg2Si with improved homogeneity: synthesis, characterization and optimization of thermoelectric properties10.1016/j.jpcs.2016.11.027 ↗
32. Lower limit to the thermal conductivity of disordered crystals10.1103/PhysRevB.46.6131 ↗