Electrical conductivity of NaSi at elevated temperatures
Source abstract
Abstract
Abstract The conductivity of sodium silicide (NaSi) was measured from 100 °C to 740 °C using a four-point DC method. NaSi was synthesized by heating a mixture of silicon powder and sodium liquid in an argon atmosphere at 550–650 °C. The formation of NaSi was followed by monitoring the conductivity and confirmed by post-experiment XRD analysis. The results showed semiconductor behaviour, with a shift in the conduction activation energy occurring near 460 °C, from 0.032 eV at the lower temperatures to 1.42 eV at higher temperatures. The room temperature conductivity of 0.22 S cm−1 was obtained by extrapolation, closely matching the results from simple two-point conductivity measurements.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and interfaces · Advancements in Battery Materials · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. The na-si (sodium-silicon) system10.1007/BF02645381 ↗
2. In operando mechanism analysis on nanocrystalline silicon anode material for reversible and ultrafast sodium storage
3. A high-performance Li-ion anode from direct deposition of Si nanoparticles
4. Formation of Si grains from a NaSi melt prepared by reaction of SiO2 and Na10.1016/j.jcrysgro.2013.04.049 ↗
5. Low-temperature synthesis of Si and Si-based compounds using Na10.2109/jcersj2.122.971 ↗
6. Preparation of niobium disilicide coating by heating niobium in a sodium–silicon melt10.2320/matertrans.MAW201213 ↗
7. Electronic structures of alkali metal (Li, Na, K, Rb, and Cs) monosilicides10.1016/j.jallcom.2008.11.149 ↗
8. Refinement of the crystal structure of tetrasodium tetrasilicide, Na4Si4
9. Na–Si binary phase diagram and solution growth of silicon crystals10.1016/j.jallcom.2009.02.036 ↗
10. Silberberg · 2003 · 548
11. Nickel substituted CuMn2O4 spinel coatings for solid oxide fuel cell interconnects10.1016/j.ijhydene.2016.08.075 ↗
12. Lithium monosilicide (LiSi), a low-dimensional silicon-based material prepared by high pressure synthesis: NMR and vibrational spectroscopy and electrical properties characterization10.1016/S0022-4596(03)00045-8 ↗
13. Investigation of the energy band structure of orthorhombic BaSi2 by optical and electrical measurements and theoretical calculations10.1063/1.1498865 ↗
14. Carrier density enhancement in semiconducting NaSn and CsPb10.1103/PhysRevLett.74.1415 ↗