journal article·2024-04

High temperature and short-term oxidation behavior of a TiBw/TA15 network composite in an air environment at 950 °C

Xunhu Xu, Qingxin Kang, Yongkang Liu, Zhenlun Li, Guofeng Wang

Publisher page

Abstract

The oxidation behavior of materials used in aerospace is crucial for their service life, and short-term oxidation behavior is an essential means to reveal the oxidation mechanism. The high temperature and short-term oxidation behavior of the TiBw/TA15 network composite in an air environment at 950 °C for 5 min, 15 min, 30 min, and 60 min was investigated. The experimental result indicates that the composite shows a slight mass change over the whole test times. The all-oxide scale mainly contains two-layer. From the top to the bottom of the oxide scale, an Al 2O 3 layer and a TiO 2 layer existed, which increased with the oxidation time. The oxidation mechanism of the initial oxidation behavior of the network composite has been established, which is crucial for promoting its application in high-temperature service environments.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. The oxidation of two ternary Ni–Cu–5 at% Al alloys in 1 atm of pure O2 at 800–900° C10.1023/A:1026071219529 ↗
2. The oxidation of two ternary Ni–Cu–10 at% Al alloys in 1 atm of pure O2 at 800–900° C10.1016/j.corsci.2003.10.020 ↗
3. High temperature oxidation behavior of a novel Ni-Cr-W-Al-Ti superalloy10.1016/j.corsci.2022.110141 ↗
4. Titanium alloys for aerospace applications10.1002/adem.200310095 ↗
5. Application of titanium and titanium alloys to fixed dental prostheses10.1016/j.jpor.2019.04.011 ↗
6. Opportunities and issues in the application of titanium alloys for aerospace components10.3390/met10060705 ↗
7. Production of titanium matrix composites reinforced with SiC particles10.1016/j.compscitech.2008.03.018 ↗
8. Simultaneous enhancements of strength, ductility, and toughness in a TiB reinforced titanium matrix composite10.1016/j.actamat.2023.118995 ↗
9. Microstructure and mechanical properties of Ti6Al4V/B4C titanium matrix composite fabricated by selective laser melting (SLM)10.1016/j.jmrt.2023.01.126 ↗
10. A variational approach to the theory of the elastic behaviour of multiphase materials10.1016/0022-5096(63)90060-7 ↗
11. K. Morsi, V.V. Patel, Processing and properties of titanium–titanium boride (TiB w) matrix composites—a review, J. Mater. Sci. 42 (200) 2037–2047.10.1007/s10853-006-0776-2 ↗
12. Effects of heat treatments on the microstructure and mechanical properties of as-extruded TiBw/Ti6Al4V composites10.1016/j.msea.2012.08.071 ↗
13. Room temperature tensile fracture characteristics of in situ TiBw/Ti6Al4V composites with a quasi-continuous network architecture10.1016/j.scriptamat.2011.01.011 ↗
14. Overcoming the strength-ductility trade-off dilemma in TiBw/TC18 composites via network architecture with trace reinforcement10.1016/j.msea.2022.143092 ↗
15. Skillfully enhanced the oxidation resistance of the traditional TA15 titanium alloy through TiB ceramic phase with network distribution10.1016/j.ceramint.2023.05.065 ↗
16. Oxidation behaviors of TA15 titanium alloy and TiBw reinforced TA15 matrix composites prepared by spark plasma sintering10.1016/j.jmst.2019.07.037 ↗
17. A novel characterization method for oxidation products of TiBw reinforced TA15 matrix composite10.1016/j.matlet.2023.134548 ↗
18. High temperature and short-term oxidation behavior of CoCrCu1.2FeNi high entropy alloy in solid and semi-solid state10.1016/j.corsci.2021.109897 ↗
19. Short-term oxidation behavior of 304 stainless steel in N2-21 vol% O2 environment between 900 and 1200°C10.1016/j.corsci.2022.110612 ↗
20. Evaluation of electrically-assisted vacuum diffusion bonding of a TiBw/TA15 composite by microstructural analysis and mechanical testing10.1016/j.jmrt.2023.06.009 ↗
21. Transient oxidation of Mo–Si–B alloys: effect of the microstructure size scale10.1016/j.actamat.2009.06.036 ↗
22. Thermal oxidation of Ti6Al4V alloy: microstructural and electrochemical characterization10.1016/j.matchemphys.2009.09.007 ↗
23. Effect of in situ TiB short fibre on oxidation behavior of Ti-6Al-1.2 B alloy10.1016/S1359-6462(02)00081-7 ↗
24. Air oxidation behaviour of Ti-6Al-4V alloy between 650 and 85010.1016/0010-938X(94)90069-8 ↗
25. Microstructure and high- temperature oxidation resistance of Ti-Al-Nb coatings on a Ti-6Al-4V alloy fabricated by laser surface alloying10.1016/j.surfcoat.2018.03.060 ↗
26. In-situ reaction synthesis of composite coating on titanium alloy for improving high temperature oxidation resistance10.1016/j.jallcom.2017.09.200 ↗
27. High temperature oxidation resistance of W-containing high entropy alloys
28. High-temperature oxidation of FeCrAl alloys: the effect of Mg incorporation into the alumina scale
29. High temperature oxidation behavior of Co-20Re-25Cr-2Si alloy at different oxygen pressures10.1016/j.corsci.2020.108562 ↗
30. Oxidation mechanism of three Fe-Al alloys with and without addition of 0.1 at% yttrium at 800° C10.1016/j.jre.2019.10.007 ↗
31. Gale · 2004
32. Characterization of oxide structures formed on nickel-chromium alloy during low pressure oxidation at 500–600 °C10.1007/BF00666809 ↗
33. The effect of pre-oxidation treatment on the high-temperature oxidation of Co-Re-Cr model alloys at laboratory air10.1007/s11085-010-9213-7 ↗
34. Oxidation of titanium matrix composites reinforced with (TiB+ TiC) particulates10.1007/s12540-018-00212-z ↗
35. Oxidation behavior of in situ TiB short fibre reinforced Ti-6Al-1.2 B alloy in air10.1023/A:1020019431992 ↗
36. Oxidation behavior of TiB-whisker-reinforced Ti60 alloy composites with three-dimensional network architecture10.1016/j.corsci.2014.03.033 ↗
37. Microstructure and mechanical properties of in situ TiB reinforced titanium matrix composites based on Ti–FeMo–B prepared by spark plasma sintering10.1016/j.compscitech.2004.05.013 ↗
38. Stacking faults formation mechanism of in situ synthesized TiB whiskers10.1016/j.scriptamat.2006.07.006 ↗
39. High temperature oxidation behavior and research status of modifications on improving high temperature oxidation resistance of titanium alloys and titanium aluminides: a review10.1016/j.jallcom.2016.06.212 ↗
40. Oxide properties of a γ-TiAl: a surface science study
41. Oxidation behavior of Fe-Cr alloys with high Cr content at 800 °C
42. Stability of protective oxide films on Ti-base alloys10.1007/BF01151593 ↗
43. Gale · 2004 · 236