Enhanced superplasticity of ultra-fine grained Ti-17 powder compact prepared through HIP/IF
Source abstract
Abstract
Abstract The superplasticity of ultra-fine grained Ti-17 powder compact prepared through hot isostatic pressing and isothermal forging was investigated in the range of temperature from 780 °C to 920 °C and strain rate from 5 × 10 −4 to 1 × 10 −2 s −1 . A uniform microstructure with the size of many equiaxed α phases less than 1 μm was produced. Superplastic tensile experiments indicate that this ultra-fine grained Ti-17 powder compact exhibits superplasticity in all tested conditions and a maximum elongation-to-failure of 1353% is obtained at temperature of 830 °C and initial strain rate of 5 × 10 −4 s −1 . During superplastic deformation of prepared Ti-17 powder compact, the coarsening of the microstructure is seriously influenced by the coalescence of dynamically recrystallized grains and the superplastic failure is caused by a combination of necking, cavity growth and cavity interlinkage. Almost all prepared Ti-17 powder compact specimens present better superplasticity than conventional cast and forged Ti-17 alloy even at high strain rate of 10 −3 s −1 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and mechanical properties · Titanium Alloys Microstructure and Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Sergueeva · Scripta Mater. · 2000 · 43 · 81910.1016/S1359-6462(00)00496-6 ↗
2. Park · Mater. Sci. Eng. A · 2010 · 527 · 520310.1016/j.msea.2010.04.082 ↗
3. Zhu · Scripta Mater. · 2005 · 52 · 65110.1016/j.scriptamat.2004.11.017 ↗
4. Mallikarjun · J. Mater. Process Technol. · 2003 · 134 · 3510.1016/S0924-0136(02)00916-0 ↗
5. Wang · J. Alloys Comp. · 2010 · 491 · 21310.1016/j.jallcom.2009.11.046 ↗
6. Nakahigashi · J. Alloys Comp. · 2002 · 330–332 · 38410.1016/S0925-8388(01)01528-6 ↗
7. Mitchell · Mater. Sci. Eng. A · 1998 · 243 · 25710.1016/S0921-5093(97)00810-1 ↗
8. Shamblen · Metall. Mater. Trans. B · 1997 · 28B · 89910.1007/s11663-997-0017-3 ↗
9. Zhao · Mater. Sci. Eng. A · 2012 · 549 · 19310.1016/j.msea.2012.04.032 ↗
10. Zhao · J. Mater. Process Technol. · 2012 · 212 · 149510.1016/j.jmatprotec.2012.02.011 ↗
11. Semiation · JOM · 1997 · 49 · 3310.1007/BF02914711 ↗
12. Mishra · Mater. Sci. Eng. A · 2001 · 298 · 4410.1016/S0921-5093(00)01338-1 ↗
13. Hirofumi · Int. J. Hydrogen Energy · 2002 · 27 · 76910.1016/S0360-3199(01)00157-4 ↗
14. Arieli · Metall. Trans. A · 1977 · 8A · 159110.1007/BF02644864 ↗
15. Ma · Acta Mater. · 2003 · 51 · 355110.1016/S1359-6454(03)00173-3 ↗
16. Langdon · Metal Sci. · 1982 · 16 · 17510.1179/030634582790427208 ↗