RETRACTED: Mechanical, microstructural and electrical evaluation of reinforced AA5083 with nano-ceramic powders of silicon dioxide Si2O3 for naval structures
This record is marked as retracted by the source. Review the publisher’s notice before using its findings.
Source abstract
Abstract
This article has been retracted: please see Elsevier Policy on Article Withdrawal ( https://www.elsevier.com/about/our-business/policies/article-withdrawal ). This article has been retracted at the request of the Editor-in-Chief. Although the text has been rephrased, the whole content is largely identical with the article accepted in the CIRP Journal of Manufacturing Science and Technology, "Improvement of mechanical properties of AA5083 in shipbuilding applications by adding nano ceramic powders of silicon dioxide Si2O3 via friction stir processing technique", Majed H. Moosa, Yasmin A. Abdelraouf , W.M. Farouk, Eyd M. ELSayed, W.M. Shewakh, Ahmed Abu-Oqail , Hanan A. Abd El-Fattah, Mohamed Abu-Okail, Available online 7 June 2020, https://nam03.safelinks.protection.outlook.com/?url=https%3A%2F%2Fdoi.org%2F10.1016%2Fj.cirpj.2020.05.007&data=02%7C01%7Cl.birla%40elsevier.com%7C0bc09cc711684473f04708d82e258c21%7C9274ee3f94254109a27f9fb15c10675d%7C0%7C0%7C637310086091620581&sdata=WloQprSCnVn8OkpWP67l57DzKZomgjmZAEYhosxp3AU%3D&reserved=0. The manuscript was submitted to the CIRP Journal on April 20, 2020 and to the Journal of Alloys and Compounds on April 28, 2020, falling into the category of double submission. A detailed comparative analysis of the figures in these two articles revealed the following conclusion : - Fig. 1, lower right: identical to CIRPJ-Fig.1, right. Strangely enough, it is claimed that this is a magnification of Fig. 1, lower left, which is obviously not the case. Fig. 1 upper right is claimed again to be a magnification of Fig. 1 lower right, which is also not the case. Figure captions are identical. - Fig. 2, right: more or less identical with JIRPJ-Fig.2, right. Identical text below the figure, identical figure caption. - Fig. 4 (b): identical with JIRPJ-Fig. 4, lower part. Almost identical figure caption. - Fig. 7 (a), upper part: identical with CIRPJ-Fig. 17 (a). - Fig. 7 (b), upper part: identical with CIRPJ-Fig. 17 (b). Captions almost identical. - Figs. 8, 9, 13, 20, 21, 22 and 23 with similar meaning as CIRPJ-Figures 15, 18, 19 (lower part), 20 (lower part), 21, 22, 23. - Fig. 10: identical with figures in CIRPJ-Table 6, lower two pictures in the middle row. - Fig. 12 (lower part): very similar to CIRPJ-Fig.25 lower part, with some conditions varying a bit. - Fig. 14: identical with figures in CIRPJ-Table 3, lower two pictures in the middle row, plus CIRPJ-Table 2, third picture in the middle row. - Fig. 16 (a): identical with JIRPJ-Fig.7, upper right, including partial figure caption. - Fig. 17: identical to JIRPJ-Fig. 10, including figure caption. - Fig. 19: identical to JIRPJ-Fig. 14, including figure caption. The corresponding author and the co-authors were informed about this decision. One of the conditions of submission of a paper for publication is that authors declare explicitly that their work is original and has not appeared in a publication elsewhere. As such this article represents a severe abuse of the scientific publishing system. The scientific community takes a very strong view on this matter and apologies are offered to readers of the journal that this was not detected during the submission process.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · MXene and MAX Phase Materials · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Aluminium based in-situ composite fabrication through friction stir processing: a review, alloy10.1016/j.jallcom.2017.04.309 ↗
2. Microstructural evolution and mechanical properties of Mg Zn Y Zr alloy during friction stir processing10.1016/j.jallcom.2016.12.068 ↗
3. Mechanical and tribological characterization of industrial wastes reinforced aluminum alloy composites fabricated via friction stir processing10.1016/j.jallcom.2020.154832 ↗
4. Recent development in aluminium alloys for the automotive industry10.1016/S0921-5093(99)00653-X ↗
5. Formability of friction stir processed low carbon steels used in shipbuilding10.1016/j.jmst.2017.10.020 ↗
6. Aluminium matrix composites: challenges and opportunities10.1007/BF02717141 ↗
7. Science and metal matrix composites-from science to technological significance10.1016/j.compscitech.2005.05.027 ↗
8. Twenty-year uninterrupted endeavor of friction stir processing by focusing on copper and its alloys10.1016/j.jallcom.2018.12.083 ↗
9. Titanium particulate reinforced AZ31 magnesium matrix composites with improved ductility prepared using friction stir processing10.1016/j.msea.2019.138793 ↗
10. Corrosion-wear behavior of AA1050/mischmetal oxides surface nano-composite fabricated by friction stir processing10.1016/j.jallcom.2020.153964 ↗
11. Effects of precipitate shape and orientation on dispersion strengthening in magnesium alloys10.1016/S1359-6462(02)00497-9 ↗
12. Effect of GNPs content at various compaction pressures and sintering temperatures on the mechanical and electrical properties of hybrid Cu/Al2O3/xGNPs nano-composites synthesized by high energy ball milling10.1016/j.ceramint.2020.04.120 ↗
13. Mechanical alloying, sintering and characterization of Al2O3–20wt%–Cu nano-composite10.1016/j.ceramint.2013.05.099 ↗
14. Effect of friction stir welding process parameters with interlayer strip on microstructural characterization and mechanical properties10.1007/s11668-020-00813-0 ↗
15. Enhancement ductility of friction stir welded aluminum blanks AA2024 via adding interlayer strip width of AA7075
16. Improving microstructural and mechanical properties of AA2024 base metal by adding reinforced strip width of AA7075 via vertical compensation friction stir welding technique10.1007/s11668-020-00814-z ↗
17. Production of tailor-welded blanks by vertical compensation friction stir welding technique10.1080/02670836.2018.1510070 ↗
18. Effect of changing heat treatment conditions on microstructural and mechanical properties of friction stir welded sheets of AA2024 with interlayer strip width AA7075
19. Development and characterization of AA5083 reinforced with SiC and Al2O3 particles by friction stir processing
20. Friction-stir processing of an AA8026-TiB2- Al2O3 hybrid nano-composite: microstructural developments and mechanical properties10.1016/j.msea.2016.02.081 ↗
21. Development of ultrafine grained high strength age hardenable Al 7075 alloy by cryorolling10.1016/j.matdes.2011.02.051 ↗
22. Particle reinforced aluminium and magnesium matrix composites10.1179/imr.1994.39.1.1 ↗
23. Enhanced strength and ductility of friction-stir-processed Mg–6Zn alloys via Y and Zr co-alloying10.1016/j.msea.2019.138877 ↗
24. Essam B, Melaibari A, Busha M. Wear and microhardness behaviors of AA7075/SiC-BN hybrid nano-composite surfaces fabricated by friction stir processing. Ceram. Int. https://doi.org/10.1016/j.ceramint.2020.03.274.10.1016/j.ceramint.2020.03.274 ↗
25. Production and characterization of an advanced AA6061-Graphene-TiB2 hybrid surface nano-composite by multi-pass friction stir processing10.1016/j.surfcoat.2019.124914 ↗
26. Fabrication of Al5083 surface composites reinforced by CNTs and cerium oxide nano particles via friction stir processing. Alloy10.1016/j.jallcom.2014.10.158 ↗
27. The effects of friction stir processing and friction stir vibration processing on mechanical, wear and corrosion characteristics of Al6061/SiO2 surface composite10.1016/j.jmapro.2019.07.034 ↗
28. Evaluation of the microstructure and mechanical properties of WC particle reinforced aluminum matrix composites fabricated by friction stir processing10.1016/j.matchar.2018.01.053 ↗
29. Strengthening and toughening mechanisms of CNTs/Mg-6Zn composites via friction stir processing10.1016/j.msea.2018.07.011 ↗
30. An innovative fabrication of nano-HA coatings on Ti-CaP nano-composite layer using a combination of friction stir processing and electrophoretic deposition10.1016/j.ceramint.2012.07.092 ↗
31. Surface composites by friction stir processing: a review10.1016/j.jmatprotec.2015.04.019 ↗
32. Effect of friction stir processing on microstructure and mechanical properties of Cu-TiC composite10.1016/j.ceramint.2014.04.158 ↗
33. Effect of Sc addition, friction stir processing, and T6 treatment on the damping and mechanical properties of 7055 Al alloy10.1016/j.jallcom.2018.09.109 ↗
34. Modeling the microstructural evolution and effect of cooling rate on the nanograins formed during the friction stir processing of Al508310.1016/j.msea.2009.08.040 ↗
35. Ultrahigh strength Mg-Al-Ca-Mn extrusion alloys with various aluminum contents10.1016/j.jallcom.2019.03.319 ↗
36. Optimization of the process parameters on the mechanical and wear properties of Al-SiC nano-composites fabricated by friction stir processing using desirability approach10.1007/s12633-019-00178-6 ↗
37. Influence of friction stir processing on the microstructure and mechanical properties of a compocast AA2024-Al2O3 nano-composite10.1016/j.matdes.2016.05.114 ↗
38. Formation of Al/(Al13 Fe4+ Al2O3) nano-composites via mechanical alloying and friction stir processing10.1007/s11665-018-3170-8 ↗
39. Reactive friction stir processing of AA 5052–TiO2 nano-composite: process–microstructure–mechanical characteristics10.1179/1743284714Y.0000000573 ↗
40. Surface reinforcement of AA5083-H111 by friction stir processing assisted by electrical current10.1016/j.jmatprotec.2014.10.005 ↗
41. A new approach in surface modification and surface hardening of aluminum alloys using friction stir process: Cu-reinforced AA508310.3390/ma13061278 ↗
42. Influence of SiC content on microstructure and tribological properties of friction stir-processed SiC/AA5083 surface composites10.1007/s11661-019-05219-8 ↗
43. Manufacturing process of AA5083/nano-γAl2O3 localized composite metal foam fabricated by friction stir processing route (FSP) and microstructural characterization10.1007/s10853-017-1802-2 ↗
44. Noncontact evaluation of the dependency of electrical conductivity on stress for various Al alloys as a function of plastic deformation and annealing10.1063/1.3456996 ↗
45. Modification of electrical conductivity by friction stir processing of aluminum alloys10.1007/s00170-011-3308-4 ↗