Strengthening of an Fe-C-Cr-Ni hypoeutectic alloy by rapid solidification under additive manufacturing conditions and further strengthening by post heat treatment
Source abstract
Abstract
This paper investigates the effects of γ-Fe dendrite arm spacing and inter-dendritic eutectic Cr 7 C 3 particle spacing on the hardness of an as-solidified hypoeutectic alloy (Fe-2.14mass%C-32.38mass%Cr-6.48mass%Ni-0.90mass%Si), as well as the effects of subsequent heat treatment on the hardness. When the cooling rate was varied between 10 4 and 10 7 o C/s, the hardness of the as-solidified alloy increased exponentially with decreasing dendrite arm spacing and eutectic particle spacing. When this alloy was subjected to laser powder bed fusion (LPBF) process, the hardness exceeded 700 HV, more than twice that of Inconel 718 Ni-based superalloy fabricated using the same process. During subsequent heat treatment at 800 °C, extremely fine Cr 23 C 6 particles precipitated in both the γ-Fe dendrite arms and the γ-Fe matrix phase of the eutectic structure, increasing the hardness of the alloy samples. Although the initial hardness of the dendrite arms was lower than that of the eutectic region, the increase in hardness was greater in the dendrite arms, indicating greater precipitation hardening in the dendrite arms than in the eutectic region. The average hardness of a large arear of the hypoeutectic structure, consisting of dendrites and eutectic regions, was always higher in the heat-treated samples with higher cooling rates during solidification. This is due to the higher supersaturation of Cr and C during cooling, which resulted in a higher number density and volume fraction of Cr 23 C 6 particles precipitated in the γ-Fe.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Additive Manufacturing Materials and Processes · Surface Treatment and Residual Stress
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. Creep behaviour of Ni-base single-crystal superalloys with various γ′ volume fraction10.1016/j.actamat.2004.04.028 ↗
2. Overview of mechanical, microstructural, oxidation properties and high-temperature applications of superalloys10.1016/j.matpr.2020.12.523 ↗
3. Nickel-based superalloys for advanced turbine engines: chemistry, microstructure and properties10.2514/1.18239 ↗
4. A review on superalloys and IN718 Nickel-Based INCONEL superalloy
5. Hall-Petch strengthening of an Fe-C-Cr-Ni eutectic alloy under additive manufacturing conditions10.1016/j.jallcom.2025.184213 ↗
6. Correlation of secondary dendrite arm spacing with the mechanical behaviour of cast 718 alloy 8th International Symposium on Superalloy 718 and Derivatives
7. The effects of grain size, dendritic structure and crystallographic orientation on fatigue crack propagation in IN713C nickel-based superalloy10.1016/j.ijplas.2019.09.010 ↗
8. Theoretical model of yield strength for eutectic colony microstructure materials10.1016/j.scriptamat.2023.115443 ↗
9. Secondary dendritic arm spacing and cooling rate relationship for an ASTM F75 alloy10.1016/j.jmrt.2022.06.146 ↗
10. Melt pool temperature and cooling rates in laser powder bed fusion
11. Investigation into the Microstructure and Hardness of Additively Manufactured (3D-Printed) Inconel 718 Alloy10.3390/ma16062383 ↗