Effect of annealing on microstructure and mechanical properties of Ti17 titanium alloy repaired by wire laser direct energy deposition

Zhe Wang, Meng Jiang, Xi Chen, Zhijian Lu, Yuan Chen, Xuan Su, Peng He, Yanbin Chen

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes · Surface Treatment and Residual Stress

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. TC17 titanium alloy laser melting deposition repair process and properties[J]10.1016/j.optlastec.2016.02.013 ↗
2. Laser shock peening induced fatigue crack retardation in Ti-17 titanium alloy[J]10.1016/j.msea.2018.09.016 ↗
3. Laser welding-brazing under temporal and spatial power modulation for dissimilar materials AA6061 to Ti6Al4V joints[J]
4. Microstructure and tensile properties of Ti/Al dissimilar joint by laser welding-brazing at subatmospheric pressure[J]10.1016/j.jmapro.2020.04.062 ↗
5. Laser metal deposition of Ti6Al4V-A brief review[J]
6. Additive manufacturing of Ti6Al4V alloy: A review[J]10.1016/j.matdes.2018.107552 ↗
7. Microstructural evolution and performance of high-tin-content Cu40Sn60 (wt%) core/shell powder TLPS bonding joints[J]10.1016/j.jmapro.2022.01.045 ↗
8. Microstructure and mechanical properties of wire arc additive repairing Ti–6.5Al–2Sn–2Zr–4Mo–4Cr titanium alloy[J]10.1080/02670836.2020.1822061 ↗
9. Wire feeding based laser additive manufacturing TC17 titanium alloy[J]10.1179/1753555715Y.0000000075 ↗
10. A state-of-the-art review on energy consumption and quality characteristics in metal additive manufacturing processes[J]10.1007/s40430-020-02323-4 ↗
11. Basic principles of additive manufacturing: different additive manufacturing technologies[G]
12. Additive manufacturing of titanium alloys: microstructure and texture evolution, defect formation and mechanical response[G]
13. Cyclic softening behavior of TC17 titanium alloy fabricated by laser directly energy deposition[J]
14. Combining manufacturing of titanium alloy through direct energy deposition and laser shock peening processes[J]10.1016/j.matdes.2021.109626 ↗
15. Enhancing the mechanical properties of electron beam welded TC17 titanium alloy joint by post-weld heat treatment[J]10.1016/j.jallcom.2019.151937 ↗
16. Wire arc additive manufacturing: approaches and future prospects[G]10.1016/B978-0-12-822056-6.00004-7 ↗
17. Enhanced surface finish and reduced porosity of TiC nanoparticles reinforced 2219 aluminum alloy deposit fabricated via oscillating laser-arc hybrid additive manufacturing[J]10.1016/j.jmapro.2024.04.071 ↗
18. Macro/micro-structure and mechanical properties of Al-6Mg-0.3Sc alloy fabricated by oscillating laser-arc hybrid additive manufacturing[J]
19. Anisotropic characterization of wire-arc additive manufacturing Ti-5Al-2Sn-2Zr-4Mo-4Cr alloy: Influence of texture and microstructure[J]10.1016/j.msea.2025.148020 ↗
20. Morphology, microstructure, and hardness of titanium (Ti-6Al-4V) blocks deposited by wire-feed additive layer manufacturing (ALM)[J]10.1016/j.msea.2011.10.095 ↗
21. Microstructural characterization and comparison of Ti-6Al-4V manufactured with different additive manufacturing processes[J]10.1016/j.matchar.2018.02.003 ↗
22. Effects of thermal undercooling and thermal cycles on the grain and microstructure evolution of TC17 titanium alloy repaired by wire arc additive manufacturing[J]
23. Grain morphology control and texture characterization of laser solid formed Ti6Al2Sn2Zr3Mo1.5Cr2Nb titanium alloy[J]10.1016/j.jmatprotec.2016.07.011 ↗
24. Effects of trace Sn and Cr addition on microstructure and mechanical properties of TC17 titanium alloy repaired by wire arc additive manufacturing[J]10.1016/j.jallcom.2021.161473 ↗
25. Effects of thermomechanical treatment on the evolution pattern of the α phase and mechanical properties of Ti-17 alloy[J]
26. Phase transformation pathways in Ti-6Al-4V manufactured via electron beam powder bed fusion[J]10.1016/j.actamat.2021.117131 ↗
27. Correlation between pulse frequencies, microstructure and mechanical properties of TA15 in wire and arc additive manufacturing[J]10.1016/j.jmrt.2024.05.149 ↗
28. Influence of microstructure on mechanical properties of laser metal wire-deposited Ti-6Al-4V[J]10.1016/j.msea.2016.07.038 ↗
29. Surface morphology, microstructure and mechanical properties of Al–Mg–Sc alloy thin wall produced by laser-arc hybrid additive manufacturing[J]
30. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti-6Al-4V[M]10.1016/j.msea.2014.07.086 ↗
31. In-situ investigation on tensile deformation and fracture behaviors of inhomogeneous microstructure during laser repair of Ti-6Al-4 V titanium alloy[J]
32. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition[J]10.1016/j.actamat.2014.11.028 ↗
33. Effects of Laser Power on the Microstructure Evolution and Mechanical Properties of Ti–6Al–4V Alloy Manufactured by Direct Energy Deposition[J]
34. Role of changes in heat input on additively manufactured Ti–6Al–4V fabricated by directed energy deposition[J]10.1016/j.msea.2021.141541 ↗
35. Effect of in-process active cooling on forming quality and efficiency of tandem GMAW–based additive manufacturing[J]10.1007/s00170-018-2927-4 ↗
36. The effect of wire size on high deposition rate wire and plasma arc additive manufacture of Ti-6Al-4V[J]
37. Morphology investigation on direct current pulsed gas tungsten arc welded additive layer manufactured Ti6Al4V alloy[J]10.1007/s00170-011-3299-1 ↗
38. Effect of interlayer cooling on the microstructure and mechanical properties of titanium alloys fabricated using directed energy deposition[J]10.1016/j.jallcom.2023.170202 ↗
39. Microstructure evolution and mechanical properties of laser additive manufactured Ti–5Al–2Sn–2Zr–4Mo–4Cr alloy[J]10.1016/S1003-6326(16)64300-5 ↗
40. Formation mechanism of ultrafine α lamellae with high-density dislocations in Ti-5Al-2Sn-2Zr-4Mo-4Cr alloy fabricated by laser powder bed fusion[J]
41. Effect of heat treatment on the microstructure, microhardness and impact toughness of TC11 and TC17 linear friction welded joint[J]
42. A simulation and experiment study on phase transformations of Ti-6Al-4V in wire laser additive manufacturing[J]10.1016/j.matdes.2021.109843 ↗
43. A comparative study of wire feeding and powder feeding in direct diode laser deposition for rapid prototyping[J]10.1016/j.apsusc.2005.01.138 ↗
44. Wire arc additive manufacturing Ti6Al4V aeronautical parts using plasma arc welding: Analysis of heat-treatment processes in different atmospheres[J]10.1016/j.jmrt.2020.11.012 ↗
45. Situ Characterization of Twin Nucleation in Pure Ti Using 3D-XRD[J]10.1007/s11661-013-2082-3 ↗
46. Mechanical twinning and dislocation slip multilayered deformation microstructures in β-type Ti– Mo base alloy[J]10.1016/j.scriptamat.2015.02.018 ↗
47. Materials information and mechanical response of TRIP / TWIP Ti alloys[J]
48. Additively manufactured Inconel 718 plus superalloy with heterostructures and high mechanical properties[J]
49. Enhanced fabrication and microstructure-property optimization of IN718 superalloy via laser rolling-assisted wire-arc directed energy deposition[J]