journal article·2026-06

Microstructural origin of yield drop and work-hardening behavior in annealed Al-Zr-Er alloy wire

Yingjie Wu, Chenxi Deng, Jiehua Liu, Yichang Tian, Junliang Lin, Qiang Wang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Microstructure and mechanical properties · Metallurgy and Material Forming · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Effects of natural aging and pre-aging on the strength and electrical conductivity in Al-Mg-Si AA6201 conductor alloys10.1016/j.msea.2021.141538 ↗
2. The difference of La and Ce as additives of electrical conductivity aluminum alloys10.1016/j.matchar.2019.109963 ↗
3. Three principles for preparing Al wire with high strength and high electrical conductivity10.1016/j.jmst.2018.11.013 ↗
4. A modified processing route for high strength Al-Mg-Si aluminum conductors based on twin-roll cast strip10.1016/j.jmatprotec.2019.116463 ↗
5. Microstructures and properties of Al-Mg-Si alloy overhead conductor by horizontal continuous casting and continuous extrusion forming process10.1016/j.msea.2015.09.114 ↗
6. Quantitative model for grain boundary effects on strength-electrical conductivity relation10.1016/j.actamat.2024.120390 ↗
7. Optimizing strength and electrical conductivity of 6201 aluminum alloy wire through rotary swaging and aging processes10.1016/j.jmatprotec.2024.118497 ↗
8. Simultaneously improved strength, ductility and conductivity in a Be-added Al-Mg-Si alloy conductor under various heat treatments10.1016/j.matlet.2025.138575 ↗
9. Effects of annealing treatment on the microstructure evolution and the strength degradation behavior of the commercially pure Al conductor10.1016/j.msea.2017.09.075 ↗
10. Kiessling · 2003
11. An investigation of microstructural stability in an Al-Mg alloy with submicrometer grain size10.1016/1359-6454(95)00395-9 ↗
12. Mechanical and electrical properties of an ultrafine grained Al-8.5wt% RE (RE=5.4wt% Ce, 3.1wt% La) alloy processed by severe plastic deformation10.1016/j.matdes.2015.10.163 ↗
13. A nanostructural design to produce high-strength Al alloys with enhanced electrical conductivity10.1016/j.scriptamat.2013.12.002 ↗
14. Enhanced mechanical properties and electrical conductivity in ultrafine-grained Al alloy processed via ECAP-PC10.1007/s10853-013-7279-8 ↗
15. Enhanced strength and electrical conductivity of Al-Mg-Si alloy by thermo-mechanical treatment10.1016/j.msea.2015.10.050 ↗
16. Modification of AA-6201 alloy for manufacturing of high conductivity and extra high conductivity wires with property of high tensile stress after artificial aging heat treatment for all-aluminium alloy conductors10.1016/j.matdes.2005.06.005 ↗
17. A high strength Al-Zr alloy with good electrical conductivity by combining gas-assisted continuous casting and extrusion with subsequent thermomechanical treatment
18. Thermal stability of Al-Zr-Sc conductor alloys during long-term elevated-temperature exposures10.1016/j.jmrt.2025.01.043 ↗
19. Achieving superior strength and conductivity for Al-Zr-Sc wires by coupling design of deformation and ageing10.1080/21663831.2024.2360161 ↗
20. Ambient- and high-temperature mechanical properties of isochronally aged Al-0.06Sc, Al-0.06Zr and Al-0.06Sc-0.06Zr (at%) alloys10.1016/j.actamat.2010.10.017 ↗
21. Effect of Er additions on ambient and high-temperature strength of precipitation-strengthened Al-Zr-Sc-Si alloys10.1016/j.actamat.2012.02.030 ↗
22. The precipitation evolution and coarsening resistance of dilute Al-Zr-Er-Yb (-Sc) alloys10.1016/j.jmst.2024.11.014 ↗
23. Coarsening resistance at 400°C of precipitation-strengthened Al-Zr-Sc-Er alloys10.1016/j.actamat.2011.07.057 ↗
24. Precipitation evolution in Al-Er-Zr alloys during aging at elevated temperature10.1016/j.jallcom.2013.03.237 ↗
25. Quasi in-situ analysis of compressive creep behaviors and microstructure evolutions in Al-Zr alloys with Sc and Er additions10.1016/j.msea.2022.143650 ↗
26. Effects of deformation on electric conductivity in Al-Zr alloys10.4028/www.scientific.net/MSF.475-479.1743 ↗
27. Effect of Zr on the microstructure, recrystallization behavior, mechanical properties and electrical conductivity of the novel Al-Er-Y alloy10.1016/j.jallcom.2018.06.163 ↗
28. Comparative study of Sc and Er addition on microstructure, mechanical properties, and electrical conductivity of Al-0.2Zr-based alloy cables10.1016/j.matchar.2018.08.037 ↗
29. Aluminum alloys for electrical engineering: a review10.1007/s10853-024-09890-0 ↗
30. Revealing the thermal damage mechanism of an Al-Zr-Er alloy wire by quantitative calculation: The contribution of dislocations and nano-precipitates10.1002/adem.202301091 ↗
31. Effect of intermediate annealing time on microstructure, texture and mechanical properties of Al-Mg-Si-Cu alloy10.1016/j.matchar.2018.05.048 ↗
32. Texture evolution by shear on two planes during ECAP of a high-strength aluminum alloy10.1016/j.actamat.2008.04.022 ↗
33. Influence of deformation and annealing on electrical conductivity, mechanical properties and texture of Al-Mg-Si alloy cables10.1016/j.msea.2017.10.065 ↗
34. Achieving extraordinary strength and conductivity in copper wire by constructing highly consistent hard texture and ultra-high aspect ratio10.1016/j.jmst.2024.09.017 ↗
35. Breaking the trade-off relation of strength and electrical conductivity in pure Al wire by controlling texture and grain boundary10.1016/j.jallcom.2018.07.358 ↗
36. Schmid · 1950
37. The dislocation distribution, flow stress, and stored energy in cold-worked polycrystalline silver10.1080/14786436008238300 ↗
38. Fundamental factors on formation mechanism of dislocation arrangements in cyclically deformed fcc single crystals10.1016/j.pmatsci.2010.12.001 ↗
39. The deformation and aging of mild steel10.1088/0370-1301/64/9/303 ↗
40. What is behind the inverse Hall-Petch effect in nanocrystalline materials?10.1016/j.actamat.2007.02.021 ↗
41. Analysis of the mechanical properties and deformation behavior of nanostructured commercially pure Al processed by equal channel angular pressing (ECAP)10.1016/j.msea.2007.04.075 ↗
42. A micro-alloyed ferritic steel strengthened by nanoscale precipitates10.1016/j.msea.2011.07.065 ↗
43. A high-strength, ductile Al-0.35Sc-0.2Zr alloy with good electrical conductivity strengthened by coherent nanosized-precipitates10.1016/j.jmst.2017.01.017 ↗
44. Statistical and theoretical analysis of precipitates in dual-phase steels microalloyed with titanium and their effect on mechanical properties10.1016/S1359-6454(99)00190-1 ↗
45. Exploring unusual Lüders deformation in ultrafine-grained high-Mn austenitic steel10.1080/21663831.2024.2359611 ↗
46. Discontinuous yielding with remarkable Lüders deformation in a duplex stainless steel during tensile deformation at 77 K10.1016/j.msea.2023.145095 ↗
47. Localized deformation inside the Lüders front of a medium manganese steel10.1016/j.msea.2021.141816 ↗
48. Scale invariance in plastic flow of crystalline solids
49. Mechanical response of dislocation interaction with grain boundary in ultrafine-grained interstitial-free steel10.1016/j.actamat.2021.116621 ↗
50. Dislocation velocities, dislocation densities, and plastic flow in lithium fluoride crystals10.1063/1.1735121 ↗
51. Yield points and delay times in single crystals10.1063/1.1702538 ↗
52. A unified phenomenological description of work-hardening and creep based on one-parameter models10.1016/0001-6160(84)90202-5 ↗
53. Kinetics of flow and strain-hardening10.1016/0001-6160(81)90112-7 ↗
54. Sequential modeling of local precipitation, strength and strain hardening in friction stir welds of an aluminum alloy 6005A-T610.1016/j.actamat.2007.07.012 ↗
55. Dislocation theory based constitutive modelling: foundations and applications10.1016/S0924-0136(98)00208-8 ↗
56. The deformation behaviour of AA6111 as a function of temperature and precipitation state10.1016/S0921-5093(01)01113-3 ↗
57. Microstructure-based modelling of isotropic and kinematic strain hardening in a precipitation-hardened aluminium alloy10.1016/j.actamat.2011.02.035 ↗
58. The influence of precipitation on the work-hardening behavior of the aluminum alloys AA6111 and AA703010.1007/s11661-003-0007-2 ↗
59. The influence of microstructure on work hardening in aluminum10.1016/1359-6454(95)00403-3 ↗
60. Mechanical behavior of alloy AA6111 processed by severe plastic deformation: modeling and experiment10.1115/1.2744396 ↗
61. The relation between polycrystal deformation and single-crystal deformation10.1007/BF02900224 ↗