journal article·2016-06-01Open access

Progress on electrocaloric multilayer ceramic capacitor development

Sakyo Hirose, Tomoyasu Usui, Sam Crossley, Bhasi Nair, Akira Ando, Xavier Moya, Neil D. Mathur

APL Materials· Volume 4· Issue 6

Abstract

A multilayer capacitor comprising 19 layers of 38 μm-thick 0.9Pb(Mg1/3Nb2/3)O3–0.1PbTiO3 has elsewhere been shown to display electrocaloric temperature changes of 2.2 K due to field changes of 24 V μm−1, near ∼100 °C. Here we demonstrate temperature changes of 1.2 K in an equivalent device with 2.6 times the thermal mass, i.e., 49 layers that could tolerate 10.3 V μm−1. Breakdown was compromised by the increased number of layers, and occurred at 10.5 V μm−1 near the edge of a near-surface inner electrode. Further optimization is required to improve the breakdown strength of large electrocaloric multilayer capacitors for cooling applications.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Multiferroics and related materials · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Murata Manufacturing Co., Ltd. 1 , 1-10-1, Higashikotari, Nagaokakyo, Kyoto 617-8555, Japan

University of Cambridge 2 Department of Materials Science, , Cambridge CB3 0FS, United Kingdom

References (26)

Show source-provided references
1. 1953
2. Annu. Rev. Mater. Sci. · 1984 · 14 · 2710.1146/annurev.ms.14.080184.000331 ↗
3. Jpn. J. Appl. Phys., Part 1 · 2003 · 42 · 110.1143/JJAP.42.1 ↗
4. Science · 1989 · 246 · 140010.1126/science.246.4936.1400 ↗
5. Science · 2006 · 311 · 127010.1126/science.1123811 ↗
6. Science · 2008 · 321 · 82110.1126/science.1159655 ↗
7. Adv. Funct. Mater. · 2014 · 24 · 130010.1002/adfm.201302386 ↗
8. Adv. Funct. Mater. · 2013 · 23 · 298710.1002/adfm.201202525 ↗
9. Appl. Phys. Lett. · 2009 · 95 · 24290310.1063/1.3275013 ↗
10. J. Appl. Phys. · 2009 · 106 · 06450910.1063/1.3190559 ↗
11. J. Appl. Phys. · 2011 · 110 · 09410310.1063/1.3658251 ↗
12. Int. J. Heat Mass Transfer · 2014 · 72 · 55910.1016/j.ijheatmasstransfer.2014.01.043 ↗
13. Nat. Mater. · 2014 · 13 · 43910.1038/nmat3951 ↗
14. AIP Adv. · 2015 · 5 · 06715310.1063/1.4922871 ↗
15. Appl. Phys. Lett. · 2016 · 108 · 03290210.1063/1.4938758 ↗
16. Electrocaloric effects in multilayer capacitors of 0.9Pb(Mg1/2Nb2/3)O3 − 0.1PbTiO3
17. See supplementary material at http://dx.doi.org/10.1063/1.4950796 for details of sample fabrication measurement methods, and electrocaloric data for a plate ceramic of thickness 300μm.
18. J. Appl. Phys. · 2013 · 114 · 17410510.1063/1.4829012 ↗
19. Appl. Phys. Lett. · 2008 · 92 · 13290910.1063/1.2905296 ↗
20. J. Eur. Ceram. Soc. · 2016 · 36 · 7510.1016/j.jeurceramsoc.2015.09.031 ↗
21. J. Am. Ceram. Soc. · 1990 · 73 · 164510.1111/j.1151-2916.1990.tb09809.x ↗
22. J. Am. Ceram. Soc. · 1990 · 73 · 165410.1111/j.1151-2916.1990.tb09810.x ↗
23. J. Am. Ceram. Soc. · 1989 · 72 · 224610.1111/j.1151-2916.1989.tb06069.x ↗
24. J. Am. Ceram. Soc. · 2014 · 97 · 66510.1111/jace.12811 ↗
25. 2006 · 14
26. Appl. Phys. Lett. · 2014 · 104 · 08290910.1063/1.4866256 ↗