journal article·2026-07Open access

Processing–structure–property relationships in Ti–6Al–2Sn–4Zr–2Mo alloy processed via different direct additive manufacturing technologies

Amir Behjat, Yahya Aghayar, Ayda Shahriari, Mohsen Mohammadi, Luca Iuliano, Abdollah Saboori

Abstract

Ti–6Al–2Sn–4Zr–2Mo (Ti-6242), a near-α titanium alloy designed for high-temperature aerospace applications, was fabricated using electron beam powder bed fusion (EB-PBF), laser powder bed fusion (L-PBF), and laser powder directed energy deposition (LP-DED). A systematic comparison was conducted to elucidate the relationships between processing route, defect population, microstructure, mechanical response, and corrosion behavior. X-ray computed tomography revealed distinct porosity characteristics, with relative densities of ~99.95%, 99.97%, and 99.99% for L-PBF, EB-PBF, and LP-DED, respectively. L-PBF samples exhibited finer but more numerous lack-of-fusion and keyhole-type pores, whereas EB-PBF showed larger, predominantly gas-induced porosity. LP-DED produced the lowest defect severity with reduced pore size and volume fraction. The superior density of LP-DED is attributed to larger, more stable melt pools that facilitate gas escape, whereas the higher defect count in L-PBF stems from keyhole instabilities and lack-of-fusion associated with its smaller beam spot and higher scan speeds. Microstructural analysis revealed that while columnar prior-β grains (9–53 μm wide) were common to all processes, the final microstructure characteristics was strongly process-dependent: L-PBF resulted in refined acicular α′ martensite with lath widths below ~0.4 μm due to rapid cooling, EB-PBF produced coarser α laths (~0.5–0.8 μm) within a basketweave morphology owing to elevated build temperatures, and LP-DED exhibited the coarsest α+β microstructure with lath widths exceeding 1 μm. These variations are driven by the extreme cooling rates in L-PBF which trigger a displacive martensitic transformation, contrasted by the in-situ thermal aging of the EB-PBF heated powder bed and the high heat input of LP-DED, which promote diffusional growth of alpha laths. Correspondingly, nanoindentation hardness decreased from ~5.24 GPa (L-PBF) to ~5.12 GPa (EB-PBF) and ~4.87 GPa (LP-DED). This trend correlates with the Hall-Petch strengthening effect derived from refined lath scales and the significantly higher dislocation density observed in L-PBF samples due to severe thermal gradients. Electrochemical testing in 3.5 wt.% NaCl solution indicated superior corrosion resistance for L-PBF and LP-DED, with corrosion current densities approximately one order of magnitude lower than EB-PBF. The reduced performance of EB-PBF is attributed to the presence of larger LOF defects and the simultaneous presence of distinct alpha and β phases; this heterogeneous phase distribution likely facilitates the formation of micro-galvanic cells, accelerating localized corrosion. These findings highlight the critical role of additive manufacturing strategy in tailoring the microstructure and performance of Ti-6242 for demanding structural applications.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (97)

Show source-provided references
1. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
2. Additive manufacturing of metallic components – Process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
3. Additive Manufacturing of Titanium Alloys; Processability, Properties and Applications
4. Multi-material processing of metallic components by direct additive manufacturing methods: technologies, scientific insights, and industrial applications10.1088/2631-7990/ae5295 ↗
5. Comparison of direct energy deposition and powder bed fusion technology in the preparation of Ti–6Al–4V alloy10.1016/j.jmrt.2025.01.231 ↗
6. Selective Laser Melted Magnesium Alloys: Fabrication, Microstructure and Property10.3390/ma15207049 ↗
7. Productivity-Driven Optimization of Laser Powder Bed Fusion Parameters for IN718 Superalloy: Process Control, Microstructure, and Mechanical Properties10.1002/adem.202502853 ↗
8. Actual state-of-the-art of electron beam powder bed fusion10.1080/26889277.2022.2040342 ↗
9. Solidification in metal additive manufacturing: challenges, solutions, and opportunities10.1016/j.pmatsci.2024.101361 ↗
10. An Overview of Additive Manufacturing of Titanium Components by Directed Energy Deposition: Microstructure and Mechanical Properties10.3390/app7090883 ↗
11. Additive manufacturing of titanium-based alloys- A review of methods, properties, challenges, and prospects10.1016/j.heliyon.2022.e09041 ↗
12. The Additive Manufacturing (AM) of titanium alloys10.1016/j.mprp.2016.12.062 ↗
13. Physical-information machine learning for strength and ductility prediction of metastable β titanium alloys10.1080/21663831.2025.2611741 ↗
14. An Overview of Densification, Microstructure and Mechanical Property of Additively Manufactured Ti-6Al-4V — Comparison among Selective Laser Melting, Electron Beam Melting, Laser Metal Deposition and Selective Laser Sintering, and with Conventional Powder
15. High-Temperature Titanium Alloys—A Review10.1007/BF03338617 ↗
16. Design of titanium alloys by additive manufacturing: A critical review
17. Opportunities and Issues in the Application of Titanium Alloys for Aerospace Components10.3390/met10060705 ↗
18. Laser powder bed fusion (L-PBF) of Ti–6Al–4V/Ti–6Al–2Sn–4Zr–2Mo and Ti–6Al–4V/γ-TiAl bimetals: Processability, interface and mechanical properties10.1016/j.msea.2023.144907 ↗
19. Effects of direct aging on near-alpha Ti–6Al–2Sn–4Zr–2Mo (Ti-6242) titanium alloy fabricated by selective laser melting (SLM)10.1016/j.msea.2020.139533 ↗
20. Martensite decomposition during post-heat treatments and the aging response of near-α Ti-6Al-2Sn-4Zr-2Mo (Ti-6242) titanium alloy processed by selective laser melting (SLM)10.1142/S2424913020500186 ↗
21. Comparing the Cold, Warm, and Hot Deformation Flow Behavior of Selective Laser-Melted and Electron-Beam-Melted Ti–6Al–2Sn–4Zr–2Mo Alloy10.1002/adem.202301046 ↗
22. An investigation on the processing conditions of Ti-6Al-2Sn-4Zr-2Mo by electron beam powder bed fusion: Microstructure, defect distribution, mechanical properties and dimensional accuracy
23. Effects of postprocess hot isostatic pressing treatments on the mechanical performance of EBM fabricated TI-6Al-2Sn-4Zr-2Mo
24. A comparative study of machine learning algorithms in the prediction of bead geometry in wire-arc additive manufacturing
25. Selective Laser Melting of a Near-α Ti6242S Alloy for High-Performance Automotive Parts10.1002/adem.202001194 ↗
26. Optimization of the Post-Process Heat Treatment Strategy for a Near-α Titanium Base Alloy Produced by Laser Powder Bed Fusion10.3390/ma15031032 ↗
27. Electron beam powder bed fusion of Ti–6Al–2Sn–4Zr–2Mo alloy: microstructure evolution and high-temperature mechanical properties10.1007/s40964-025-00996-8 ↗
28. Comparison of two metallic additive manufacturing technologies: Selective laser melting and electron beam melting
29. Corrosion behavior of AM-Ti-6Al-4V: a comparison between EBM and SLM10.1007/s40964-022-00293-8 ↗
30. Advances in additively manufactured titanium alloys by powder bed fusion and directed energy deposition: Microstructure, defects, and mechanical behavior10.1016/j.jmst.2023.11.003 ↗
31. Modulating laser intensity profile ellipticity for microstructural control during metal additive manufacturing10.1016/j.actamat.2017.02.025 ↗
32. A Review of Metal Fabricated with Laser- and Powder-Bed Based Additive Manufacturing Techniques: Process, Nomenclature, Materials, Achievable Properties, and its Utilization in the Medical Sector10.1002/adem.201700658 ↗
33. Microstructure evolution and corresponding tensile properties of Ti–5Al–5Mo–5V–1Cr–1Fe alloy controlling by multi-heat treatments10.1016/j.pnsc.2021.08.008 ↗
34. A critical review of corrosion characteristics of additively manufactured stainless steels
35. Corrosion and high temperature oxidation behavior of additively manufactured alloys: Damage mechanisms and structure-property relationships10.1016/j.jallcom.2025.185069 ↗
36. Parent grain reconstruction from partially or fully transformed microstructures in MTEX
37. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
38. Investigation of the relationship between elastic modulus and hardness based on depth-sensing indentation measurements10.1016/j.actamat.2004.08.002 ↗
39. Influence of beam diameter on Laser Powder Bed Fusion (L-PBF) process
40. On the effect of small laser spot size on the mechanical behaviour of 316L stainless steel fabricated by L-PBF additive manufacturing
41. Additive manufacturing of metallic components by selective electron beam melting - A review10.1080/09506608.2016.1176289 ↗
42. Understanding melt pool characteristics in laser powder bed fusion: An overview of single- and multi-track melt pools for process optimization
43. Effect of scanning pattern and volumetric energy density on the properties of selective laser melting Ti-6Al-4V specimens10.1016/j.jmrt.2021.03.044 ↗
44. Competing roles of microstructure and defects on the mechanical properties of laser-powder bed fused Ti-6Al-2Sn-4Zr-2Mo alloy10.1007/s40964-024-00728-4 ↗
45. Microstructure control in additively manufactured Ti-6Al-4V during high-power laser powder bed fusion
46. Selection of solidification pathway in rapid solidification processes
47. Prior β grain evolution and phase transformation of selective laser melted Ti6Al4V alloy during heat treatment10.1016/j.jallcom.2022.165235 ↗
48. Effect of processing parameters on the defects, microstructure, and property evaluation of Ti-6Al-4V titanium alloy processed by laser powder bed fusion10.1063/7.0001251 ↗
49. Identification of prior β grains of additive manufactured Ti-6Al-4V alloy using electron backscatter diffraction10.1016/j.matlet.2022.132758 ↗
50. Achieving the strength-ductility balance through the control of the prior β-grain size in laser beam powder bed fusion of Ti-6Al-4V
51. Comparison of the microstructures and mechanical properties of Ti–6Al–4V fabricated by selective laser melting and electron beam melting10.1016/j.matdes.2015.12.135 ↗
52. Recent advance in laser powder bed fusion of Ti–6Al–4V alloys: microstructure, mechanical properties and machinability10.1080/17452759.2024.2446952 ↗
53. Additive manufacturing of Ti6Al4V alloy: A review10.1016/j.matdes.2018.107552 ↗
54. Recent Advancements in Microstructure Control and Performance Optimization of Titanium Alloys via Powder Bed Fusion
55. Methodology and experimental validation of analytical melt pool models for laser powder bed fusion10.1016/j.jmatprotec.2022.117547 ↗
56. Observation of keyhole-mode laser melting in laser powder-bed fusion additive manufacturing10.1016/j.jmatprotec.2014.06.005 ↗
57. Evolution of solidification texture during additive manufacturing10.1038/srep16446 ↗
58. Solidification modes during additive manufacturing of steel revealed by high-speed X-ray diffraction10.1016/j.actamat.2023.118713 ↗
59. Microstructure and Mechanical Properties of High Strength Two-Phase Titanium Alloys
60. A new approach to evaluate the elastic modulus of metallic foils10.1016/j.matdes.2020.109149 ↗
61. Elastic modulus data for additively and conventionally manufactured variants of Ti-6Al-4V, IN718 and AISI 316 L10.1038/s41597-023-02387-6 ↗
62. Nanoindentation study of mechanical properties of Ti based alloys with Fe and Ta additions10.1016/j.jallcom.2016.09.123 ↗
63. Porter · 2021
64. Small-depth nanoindentation studies of an additively manufactured titanium alloy: Anisotropic nanomechanical properties and correlation with microscopic mechanical behaviour10.1016/j.mtla.2023.101802 ↗
65. Nanoindentation and Corrosion Behavior of Additively Manufactured Ti-6Al-4V Alloy for Biomaterial Applications10.1007/s11665-023-08139-2 ↗
66. Effect of annealing temperature on microstructure and high-temperature tensile behaviour of Ti-6242S alloy produced by Laser Powder Bed Fusion10.1080/26889277.2021.1997341 ↗
67. Titanium-Based Biomaterials for Preventing Stress Shielding between Implant Devices and Bone10.1155/2011/836587 ↗
68. Revealing new depths of information with indentation mapping of microstructures10.1557/s43577-025-00919-6 ↗
69. Local substructure characterization of nanoindented additively manufactured Ti6242 alloy using STEM and EBSD10.1016/j.matchar.2025.114921 ↗
70. Recent Progress on Wear-Resistant Materials: Designs, Properties, and Applications10.1002/advs.202003739 ↗
71. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
72. Nanostructured β-phase Ti–31.0Fe–9.0Sn and sub-μm structured Ti–39.3Nb–13.3Zr–10.7Ta alloys for biomedical applications: Microstructure benefits on the mechanical and corrosion performances10.1016/j.msec.2012.07.016 ↗
73. Relationships between hardness, Young’s modulus and elastic recovery in hard nanocomposite coatings10.1016/S0257-8972(01)01714-5 ↗
74. Nanoindentation response of Cu–Ti based metallic glasses: Comparison between as-cast, relaxed and devitrified states10.1016/j.jnoncrysol.2015.05.035 ↗
75. Selective Laser Melting of Titanium Alloys and Titanium Matrix Composites for Biomedical Applications: A Review10.1002/adem.201500419 ↗
76. Towards a process-structure model for Ti-6Al-4V during additive manufacturing10.1016/j.jmapro.2020.11.033 ↗
77. Effects of post-heat treatments on the microstructure and mechanical properties of Ti–6Al–4V alloy fabricated by selective laser melting10.1016/j.jmrt.2024.09.141 ↗
78. Improved Corrosion Resistance on Selective Laser Melting Produced Ti-5Cu Alloy after Heat Treatment10.1021/acsbiomaterials.8b00319 ↗
79. Corrosion Behaviour of Selective Laser Melted Ti-TiB Biocomposite in Simulated Body Fluid10.1016/j.electacta.2017.02.112 ↗
80. The electrochemical behaviour of Ti-48Al-2Cr-2Nb produced by electron beam powder bed fusion process10.1016/j.intermet.2024.108472 ↗
81. Corrosion evaluation of multi-pass welded nickel-aluminum bronze alloy in 3.5% sodium chloride solution: A restorative application of gas tungsten arc welding process10.1016/j.matdes.2014.02.019 ↗
82. Lasia · 2014
83. Laser powder bed fusion of copper-bearing AISI 316 L: Microstructure, biofunctional and corrosion performance10.1016/j.matchar.2025.115614 ↗
84. Corrosion behavior of selective laser melted Ti-6Al-4 V alloy in NaCl solution10.1016/j.corsci.2015.10.041 ↗
85. A novel titanium alloy for load-bearing biomedical implants: Evaluating the antibacterial and biocompatibility of Ti536 produced via electron beam powder bed fusion additive manufacturing process
86. Corrosion characterization of titanium alloys by electrochemical techniques10.1016/j.electacta.2005.02.121 ↗
87. Impedance Spectroscopy: A Powerful Tool for Rapid Biomolecular Screening and Cell Culture Monitoring10.1002/elan.200503371 ↗
88. Electrochemical behavior of additively manufactured patterned titanium alloys under simulated normal, inflammatory, and severe inflammatory conditions10.1016/j.jmrt.2023.07.113 ↗
89. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗
90. Electrochemical Behavior of Electron Beam Powder Bed Fused Ti536 Alloy under Simulated Inflammatory Conditions10.1007/s40195-025-01846-w ↗
91. Optimizing the corrosion resistance of additive manufacturing TC4 titanium alloy in proton exchange membrane water electrolysis anodic environment10.1016/j.ijhydene.2024.10.440 ↗
92. Corrosion Behaviour of Electron Beam Melted Ti6Al4V: Effects of Microstructural Variation10.1149/1945-7111/abb9d1 ↗
93. Process-microstructure-corrosion of additively manufactured steels: a review10.1080/10408436.2023.2255616 ↗
94. Corrosion of Additively Manufactured Alloys
95. Effect of Grain Size on Corrosion: A Review10.5006/1.3462912 ↗
96. Surface post-treatments for metal additive manufacturing: Progress, challenges, and opportunities
97. Heat treatment effect on the microstructure and elevated temperature tensile property of the Ti6242S alloy fabricated via laser powder bed fusion10.1016/j.jallcom.2022.166656 ↗