Abstract Potential induced degradation (PID) has been affecting the performance, durability, and reliability of crystalline Si solar cells/modules. The authors demonstrate that micro‐cracks also act as the additional recombination centers, which reduce short‐circuit current density (Jsc), open‐circuit voltage (Voc), and the effective lifetime of carriers in solar cells, in PID condition. This hypothesis was confirmed by external quantum efficiency measurements and microwave photo‐conductance decay method at the micro‐cracked areas before and after PID stress tests. In addition, the PID recovery was made significantly but non‐fully for the laminated micro‐cracked modules owing to the electrical PID recovery method. In addition, the authors showed and discussed the challenging problems in recovering the performance of the PID‐affected micro‐cracked solar modules without lamination. The achieved results from 11 cycles of PID stress/recovery tests with the same duration of PID stress and recovery processes showed that an exponentially decreasing function fits the correlation between the relative losses of Pmax, Voc, fill factor (FF), and Jsc due to the PID stress process and the number of the PID stress/recovery cycles. This provides a model for the estimation of the relative losses of Pmax, Voc, FF, and Jsc due to the PID stress process versus the number of the PID stress/recovery cycles. Finally, based on the decreasing tendency in the performance loss of the PID‐affected laminated micro‐cracked solar modules after PID stress/recovery cycles, the authors suggest that cyclic PID tests with suitable conditions might be a reasonable approach to control PID.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques · Advancements in Semiconductor Devices and Circuit Design
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Division of Materials Science Nara Institute of Science and Technology Ikoma Nara Japan
Institute of Research and Development Duy Tan University Danang 550000 Vietnam
College of Science and Engineering Aoyama Gakuin University Sagamihara Kanagawa Japan
References (28)
Show source-provided references
1. PingelS FrankO WinklerM et al.Potential induced degradation of solar cells and panels.35th IEEE Photovoltaic Specialists Conference.2010:2817–2822.10.1109/PVSC.2010.5616823 ↗
2. BergholdJ FrankO HoehneH PingelS RichardsonS WinklerM.Potential induced degradation of solar cells and panels.25th European Photovoltaic Solar Energy Conference and Exhibition/5th World Conference on Photovoltaic Energy Conversion2010:3753–3759.
3. SchützeM JunghänelM KoentoppMB et al.Laboratory study of potential induced degradation of silicon photovoltaic modules.37th IEEE Photovoltaic Specialists Conference.2011:821–826.10.1109/PVSC.2011.6186080 ↗
4. HackeP KempeM TerwilligerK et al.Characterization of multicrystalline silicon modules with system bias voltage applied in damp heat.25th European Photovoltaic Solar Energy Conference and Exhibition/5th World Conference on Photovoltaic Energy Conversion.2010:3760–3765.
5. 10.1016/j.solmat.2015.04.03710.1016/j.solmat.2015.04.037 ↗
6. 10.7567/APEX.9.11230110.7567/APEX.9.112301 ↗
7. SwansonR CudzinovicM DeceusterD et al.The surface polarization effect in high‐ efficiency silicon solar cells.15th International Photovoltaic Science & Engineering Conference2005:410–411.
8. 10.1063/1.489400710.1063/1.4894007 ↗
9. 10.1016/j.solener.2020.02.03410.1016/j.solener.2020.02.034 ↗
10. 10.1177/014233121245758310.1177/0142331212457583 ↗
11. 10.1016/j.egypro.2014.08.01110.1016/j.egypro.2014.08.011 ↗
12. 10.1016/j.solmat.2010.10.03410.1016/j.solmat.2010.10.034 ↗
13. 10.1016/j.solener.2018.08.08210.1016/j.solener.2018.08.082 ↗
14. 10.1109/JPHOTOV.2014.230023810.1109/JPHOTOV.2014.2300238 ↗
15. 10.1016/j.egypro.2014.08.01310.1016/j.egypro.2014.08.013 ↗
16. MaL XuL ZhangK et al.The measurement of series and shunt resistances of the silicon solar cell based on LabVIEW 2011 International Conference on Electrical and Control Engineering2011:2711–2714.10.1109/ICECENG.2011.6058342 ↗
17. 10.1063/1.289539610.1063/1.2895396 ↗
18. 10.7567/1347-4065/ab3f0610.7567/1347-4065/ab3f06 ↗
19. WhitfieldK SalomonA YangS SuezI.Damp heat versus field reliability for crystalline silicon.38th IEEE Photovoltaic Specialists Conference2012:1864–1870.10.1109/PVSC.2012.6317957 ↗
20. 10.1016/0927-0248(95)00150-610.1016/0927-0248(95)00150-6 ↗
21. MonG WenL RossRG Adent D. Effects of temperature and moisture on module leakage current.18th IEEE Photovoltaic Specialists Conference1985:1179–1185.
22. 10.1016/j.solmat.2006.10.00910.1016/j.solmat.2006.10.009 ↗
23. 10.1109/JPHOTOV.2015.245991910.1109/JPHOTOV.2015.2459919 ↗
24. HackeP TerwilligerK SmithR et al.System voltage potential‐induced degradation mechanisms in PV modules and methods for test.37th IEEE Photovoltaic Specialists Conference.2011:814–000820.10.1109/PVSC.2011.6186079 ↗
25. 10.1016/j.egypro.2012.07.02010.1016/j.egypro.2012.07.020 ↗
26. 10.1016/j.egypro.2013.05.04210.1016/j.egypro.2013.05.042 ↗
27. PingelS.Recovery methods for modules affected by potential induced degradation (PID) 27th European Photovoltaic Solar Energy Conference2012:3379–3383.
28. NagelH PfeifferR RaykovA WangemannK.Lifetime warranty testing of crystalline silicon modules for potential‐induced degradation.27th European Photovoltaic Solar Energy Conference and Exhibition2012:3163–3166.