In vivo biostability of polyether polyurethanes with fluoropolymer and polyethylene oxide surface modifying endgroups; resistance to metal ion oxidation
Source abstract
Abstract
Abstract Polyether polyurethanes are subject to oxidation catalyzed by, and through direct (redox) reaction with transition metal ions (metal ion oxidation, MIO). The source of the ions is corrosion of metallic parts within an implanted device. A Shore 80A polyether polyurethane was modified with fluoropolymer (E80AF) or polyethylene oxide (E80AP) surface modifying end groups (SME). The SME migrates to the surface to form a covalently bonded monolayer, while maintaining the bulk properties of the polyurethane. In vitro tests in H2O2 solution indicated that both SME's accelerated MIO. Tubing samples containing cobalt mandrels were implanted in the subcutis of rabbits for up to 2 years. In vivo, E80AF significantly slowed the rate of visible degradation, but did not prevent MIO. E80AP had virtually identical visual performance to the unmodified control in vivo. Infrared spectroscopy and molecular weight correlated well with visual appearance. When cracks were seen, polyether soft segment oxidation was occurring. Both E80AP and the control developed severe loss of molecular weight in vivo. The changes were much less severe for E80AF. Thus, contrary to in vitro test results, the PEO SME had no effect at all on MIO resistance, while the fluoropolymer SME produced a significant improvement in biostability. © 2006 Wiley Periodicals, Inc. J Biomed Mater Res, 2007
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Nanoparticles: synthesis and applications · Polymer composites and self-healing · Marine Biology and Environmental Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Materials, microbes and man: The problem of infection associated with implantable devices
2. 10.1002/jbm.1003510.1002/jbm.10035 ↗
3. 10.1016/1054-8807(95)00023-X10.1016/1054-8807(95)00023-X ↗
4. Results with different extraction methods (success rate and complications)
5. 10.1002/(SICI)1097-4636(199902)44:2<206::AID-JBM11>3.0.CO;2-D10.1002/(SICI)1097-4636(199902)44:2<206::AID-JBM11>3.0.CO;2-D ↗
6. 10.1163/15685620376357272510.1163/156856203763572725 ↗
7. 10.1163/1568562026017838210.1163/15685620260178382 ↗
8. Inhibition of fibroblast adhesion and proliferation on polyurethanes with SMEs
9. 10.1016/1054-8807(93)90051-310.1016/1054-8807(93)90051-3 ↗
10. 10.1002/jbm.a.3039610.1002/jbm.a.30396 ↗
11. In vivo biostability of polyether polyurethanes with fluoropolymer surface modifying endgroups; resistance to biologic oxidation and stress cracking
12. 10.1002/(SICI)1097-4636(199612)32:4<493::AID-JBM1>3.0.CO;2-M10.1002/(SICI)1097-4636(199612)32:4<493::AID-JBM1>3.0.CO;2-M ↗
13. Medtronic Incorporated · 2005
14. StokesK UrbanskiP CouryA.In vivo autooxidation of polyether polyurethanes in the presence of metals: Preliminary results Transactions of 13th Annual Meeting of the Society for Biomaterials New York June 3–7 1987 10.
15. ZhaoQ AggerMP FitzpatrickM AndersonJM StokesK UrbanskiP.In vivostudies of stress‐cracking in polyetherurethanes using the cage implant system Transactions of the 15th Annual Meeting of the Society for Biomaterials Lake Buena Vista FL April 28–May 2 1989 203.
16. 10.1002/jbm.82024050810.1002/jbm.820240508 ↗
17. 10.1177/08853282860010030210.1177/088532828600100302 ↗
18. CouryAJ CahalanPT SlaikeuPC StokesKB.In vitro chemical resistance of implantable polyurethanes. Paper presented at the 11th Annual Meeting of the Society for Biomaterials. San Diego CA April 25–26 1985.
19. Bell CF · 1968