Assessment of wear in extensively irradiated UHMWPE cups in simulator studies
Source abstract
Abstract
Abstract Higher levels of UHMWPE crosslinking currently are being advocated for improved wear resistance of acetabular cups. Pioneering Japanese studies, begun in 1971, have achieved good clinical results with UHMWPE irradiated to 1000 kGy for use with a cemented‐cup design. The objective of our study was to use contemporary simulator techniques to determine the in vitro wear performance of such high‐dose irradiated cups. Extruded UHMWPE cups were processed with 500, 1000, and 1500 kGy of gamma‐radiation doses under vacuum, annealed, and machined to shape. The cups were mated with 26‐mm alumina heads and run in a multidirectional simulator with bovine serum. Over a 6‐million cycle (Mc) study, the weight loss of the nonirradiated control cups averaged 52.8 mg/Mc + 1.4% (wear = 57.2 mm3/Mc). In contrast, the irradiated wear cups had a consistent weight gain. Thus cups with irradiation of 500–1500 kGy had no detectable wear in this study. The original machining marks still were partially evident in the wear zones, along with some macrofissures in the 1000‐ and 1500‐kGy cups. Areas adjacent to the fissures showed delaminating plaques of 100–300 μm in size. It also was noted that the wear cups systematically gained more weight than their corresponding soak controls. Each 200‐kGy radiation gain increased the fluid sorption ratio by 10%. The increased fluid sorption and evidence of some surface deterioration may indicate that such high‐dose irradiated cups are more susceptible to mechanical damage. This indicates that we should take care to ensure that our desire to reduce the wear debris to a zero amount does not result in a modified UHMWPE that lacks the necessary mechanical properties for contemporary metal‐backed cup designs. © 2003 Wiley Periodicals, Inc. J Biomed Mater Res 68A: 52–60, 2004
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Orthopedic Infections and Treatments · Total Knee Arthroplasty Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. CharnleyJ.Total prosthetic replacement of the hip joint using a socket of high‐density polyethylene. Centre for Hip Surgery Wrightington Hospital1966; Internal Publication No. 1.
2. The wear of plastics materials in the hip joint
3. Comparison of polyethylene wear in machined versus molded polyethylene
4. Oxidation and wear resistance of directly molded UHMWPE
5. 10.1002/(SICI)1097-4636(1999)48:3<374::AID-JBM23>3.0.CO;2-O10.1002/(SICI)1097-4636(1999)48:3<374::AID-JBM23>3.0.CO;2-O ↗
6. 10.2106/00004623-199407000-0002010.2106/00004623-199407000-00020 ↗
7. Sauer WL · 1997 · 1
8. Schmalzried TP · 1998 · 247
9. 10.1016/0883-5403(94)90059-010.1016/0883-5403(94)90059-0 ↗
10. Clarke IC · 1989 · 104
11. Mechanism and clinical significance of wear debris‐induced osteolysis10.1097/00003086-199203000-00003 ↗
12. Comparison of alumina–polyethylene and metal–polyethylene in clinical trials10.1097/00003086-199209000-00011 ↗
13. 10.1080/00016470175360664410.1080/000164701753606644 ↗
14. Time dependent oxidation and damage in retrieved and never implanted UHMWPE components
15. 10.1016/S0883-5403(96)80026-X10.1016/S0883-5403(96)80026-X ↗
16. FisherJ ReevesEA IsaacGH SaumKA SanfordWM.Comparison of the wear of aged and non‐aged ultrahigh molecular weight polyethylene sterilized by gamma irradiation and by gas plasma. Proc 5th World Biomater Cong;1996. p971.
17. BellCJ AbeysunderaM WalkerPS BlunnGW.Wear and oxidation of ultra high molecular weight polyethylene. Proc 5th World Biomater Cong;1996. p655.
18. 10.1520/JTE11485J10.1520/JTE11485J ↗
19. Improved wear of UHMWPE using a vacuum sterilization process
20. 10.1002/jor.110017020310.1002/jor.1100170203 ↗
21. The radiation improvement of polyethylene prostheses10.1302/0301-620X.60B3.681412 ↗
22. OonishiH IgakiH TakayamaY.Comparisons of wear of UHMW polyethylene sliding against metal and alumina in total hip prostheses—Wear test and clinical results. Proc 3rdWorld Biomater Cong;1988. p337.
23. Improvement of polyethylene by irradiation in artificial joints
24. Hip simulator testing of isostatically molded UHMWPE: Effect of ETO and gamma irradiation
25. Significance of the sterilization method and long‐term ageing on the in vivo wear rate of UHMWPE
26. WangA PolineniVK EssnerA SunDC StarkC DumbletonJH.Effect of radiation dosage on the wear of stabilized UHMWPE evaluated by hip and knee joint simulators. Proc 23rdAnn Mtg Soc Biomater1997; p394.
27. 10.1023/A:101858202734910.1023/A:1018582027349 ↗
28. Physical, chemical study and biological safety test for UHMW polyethylene cross‐linked by high‐dose γ‐irradiation
29. The effect of the peroxide content on the cross‐link density, mechanical properties, and wear behavior of UHMWPE
30. Comparative wear under three different tribological conditions of acetylene crosslinked ultra high molecular weight polyethylene
31. Extremely low wear of gamma‐crosslinked/remelted UHMW polyethylene acetabular cups
32. Clinical experience with gamma irradiation‐crosslinked polyethylene—A 14 to 20 year follow‐up report
33. 10.1302/0301-620X.81B1.882210.1302/0301-620X.81B1.8822 ↗
34. Prospective clinical and joint simulator studies of a new total hip arthroplasty using alumina ceramic heads and cross‐linked polyethylene cups10.1302/0301-620X.78B2.0780280 ↗
35. 10.1016/0142-9612(96)83281-910.1016/0142-9612(96)83281-9 ↗
36. 10.1002/(SICI)1097-4636(199802)39:2<229::AID-JBM9>3.0.CO;2-R10.1002/(SICI)1097-4636(199802)39:2<229::AID-JBM9>3.0.CO;2-R ↗
37. 10.1002/(SICI)1097-4636(199624)33:4<275::AID-JBM7>3.0.CO;2-M10.1002/(SICI)1097-4636(199624)33:4<275::AID-JBM7>3.0.CO;2-M ↗
38. OonishiH IgakiH TakayamaY.Comparisons of wear of UHMW polyethylene sliding against metal and alumina in total hip prostheses—Wear test and clinical results. Proc 3rd World Biomater Cong1988; p337.
39. LiaoYS BenyaPD LuB McKellopH.Stability of serum as a lubricant in wear simulator tests of prosthetic joints. Proc 5th World Biomater Cong;1996. p871.
40. Reply to “Wear of UHMWPE acetabular cups in a physiological hip joint simulator in the anatomical position using bovine serum as a lubricant” (1997)
41. PolineniVK WangA EssnerA StarkC DumbletonJH.Effect of lubricant protein concentration on the wear of UHMWPE acetabular cups against cobalt–chrome and alumina femoral heads. Proc 23rd Ann Mtg Soc Biomater;1997. p154.
42. The impact of lubricant protein concentration on the outcome of hip joint simulator testing
43. ClarkeIC OonishiH Ben‐NissanB SwainM WilliamsP GoodV.Confounding in‐vitro wear performances with polyethylene metal and ceramic total hips—Water versus serum lubrication in hip simulation studies. Proc Int Tribology Conf Nagasaki Japan;2000. p28.
44. 10.1016/S0043-1648(01)00656-110.1016/S0043-1648(01)00656-1 ↗
45. Forces transmitted by joints in the human body
46. CampbellP LiuTS SchmalzriedTP McKellopH GonsalvesR AmstutzHC.Characteristics of fluids around total hip and total knee replacements. Proc 23rd Ann Mtg Soc Biomater;1997. p130.
47. 10.1002/art.178014050310.1002/art.1780140503 ↗
48. ASTMD150‐85: Part 8.01. In:Annual book of ASTM standards.Philadelphia:American Society for Testing and Materials;1990. p458–463.
49. 10.1002/jab.77005010410.1002/jab.770050104 ↗
50. 10.1243/095441197153465610.1243/0954411971534656 ↗
51. Marked improvement in the wear resistance of a new form of UHMWPE in a physiologic hip simulator
52. Wear and high cycle fatigue of highly crosslinked UHMWPE
53. YamamotoK ClarkeI WilliamsP GoodV MasaokaT ImakiireA OonishiH.SEM wear mode of extensively crosslinked polyethylene cups surfaces and wear debris: In‐vitro and ex‐vivo. Proc 25thAnn Mtg Soc BioMater;1999. p503.
54. Anisotropic oxidation and radial cracks in retrieved acetabular components
55. 10.1016/0142-9612(85)90007-910.1016/0142-9612(85)90007-9 ↗
56. DengM ShalabySW.A 5.5 year post‐irradiation aging study on ultrahigh molecular weight polyethylene. Proc 26thAnn Mtg Soc Biomater;2000. p37.
57. 10.1002/app.1979.07023031310.1002/app.1979.070230313 ↗