Migration of wear debris of polyethylene depends on bone microarchitecture
Source abstract
Abstract
Abstract The mechanism of hip arthroplasties loosening is related to the migration of wear debris throughout the implant environment. In vivo, polyethylene particles (PE) were shown to infiltrate the bone implant interface and the medullary spaces of the cancellous bone. Our test hypothesis was that polyethylene particle migration is correlated to bone porosity. Bone samples with a high or low trabecular volume and microarchitecture were harvested in 20 calves and 20 human cadavers. They were extensively washed to remove marrow cells. Bone cylinders were filled with a light‐curing monomer having the same viscosity as bone marrow. PE particles (7 and 33 μm) were deposited at the surface of the polymer. The bone cylinders were agitated during 7 days on an orbital shaker and the gel was left to polymerize at day light. X‐ray microtomography was performed to characterize bone volume and microarchitecture. Cylinders were sectioned and observed under polarized light. The migration distance and rate were determined. Migration of PE particles strongly depended on trabecular bone volume and microarchitecture. We found a linear relationship (r = 0.61) between speed migration and bone volume and an exponential relationship between speed migration and bone architecture. The present in vitro model confirmed our hypothesis about the key role of bone microarchitecture in the migration of large PE wear particles. This is an explanation for the development of inflammatory reaction at distance from a prosthesis although our study did not include submicron particles. © 2009 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 2009
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Total Knee Arthroplasty Outcomes · Orthopedic Infections and Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. 10.1002/jbm.82011020210.1002/jbm.820110202 ↗
2. 10.1243/PIME_PROC_1996_210_409_0210.1243/PIME_PROC_1996_210_409_02 ↗
3. 10.1097/00045391-199601000-0000610.1097/00045391-199601000-00006 ↗
4. 10.1016/S0736-0266(01)00070-510.1016/S0736-0266(01)00070-5 ↗
5. 10.3109/1745367830899659110.3109/17453678308996591 ↗
6. Agressive granulomatous lesions in cementless total hip arthroplasties10.1302/0301-620X.72B6.2246301 ↗
7. 10.2106/00004623-199274060-0000610.2106/00004623-199274060-00006 ↗
8. 10.1016/S0142-9612(98)00140-910.1016/S0142-9612(98)00140-9 ↗
9. The origin of submicron polyethylene wear debris in total hip arthroplasty
10. 10.1080/1040200070132520410.1080/10402000701325204 ↗
11. 10.1002/jbm.b.3101310.1002/jbm.b.31013 ↗
12. 10.1302/0301-620X.76B1.830068410.1302/0301-620X.76B1.8300684 ↗
13. 10.2106/00004623-199411000-0001010.2106/00004623-199411000-00010 ↗
14. 10.2106/00004623-199509000-0000210.2106/00004623-199509000-00002 ↗
15. 10.1097/00003086-199610000-0002110.1097/00003086-199610000-00021 ↗
16. Hailey JL · 1996 · 550
17. 10.1002/1097-4636(200009)53:5<490::AID-JBM7>3.0.CO;2-710.1002/1097-4636(200009)53:5<490::AID-JBM7>3.0.CO;2-7 ↗
18. Wear of historical polyethylenes in hip prostheses. Biomedical success and a biological failure10.1177/112070000301302s05 ↗
19. 10.1002/jbm.a.1045510.1002/jbm.a.10455 ↗
20. 10.2106/00004623-200004000-0000210.2106/00004623-200004000-00002 ↗
21. 10.1002/(SICI)1097-4636(199602)30:2<157::AID-JBM4>3.0.CO;2-Q10.1002/(SICI)1097-4636(199602)30:2<157::AID-JBM4>3.0.CO;2-Q ↗
22. Bone lysis in well‐fixed cemented femoral components10.1302/0301-620X.72B6.2246299 ↗
23. 10.2106/00004623-198668060-0001410.2106/00004623-198668060-00014 ↗
24. 10.2106/00004623-199072070-0001110.2106/00004623-199072070-00011 ↗
25. 10.1002/jbm.b.3000110.1002/jbm.b.30001 ↗
26. 10.1016/S0883-5403(00)91259-210.1016/S0883-5403(00)91259-2 ↗
27. The susceptibility of smooth implants surfaces to periimplant fibrosis and migration of polyethylene wear debris
28. 10.1002/jab.77006040210.1002/jab.770060402 ↗
29. 10.1002/jbm.82016061510.1002/jbm.820160615 ↗
30. Letournel E · 1987 · 318
31. Localised endosteal bone lysis in relation to the femoral components of cemented total hip arthroplasties10.1302/0301-620X.72B6.2246300 ↗
32. 10.1002/jbm.b.1007210.1002/jbm.b.10072 ↗
33. 10.1302/0301-620X.82B4.974410.1302/0301-620X.82B4.9744 ↗
34. The influence of stem size and extent of porous coating on femoral bone resorption after primary cementless hip arthroplasty
35. 10.1002/jor.110014031710.1002/jor.1100140317 ↗
36. When density fails to predict bone strength
37. 10.1016/0142-9612(93)90238-W10.1016/0142-9612(93)90238-W ↗
38. 10.1016/B978-0-12-119201-3.50015-910.1016/B978-0-12-119201-3.50015-9 ↗
39. 10.1038/nmat189010.1038/nmat1890 ↗
40. Fouassier J · 1995 · 84
41. 10.1016/0002-9343(93)90218-E10.1016/0002-9343(93)90218-E ↗
42. 10.1359/jbmr.2000.15.1.1310.1359/jbmr.2000.15.1.13 ↗
43. 10.1016/S8756-3282(00)00285-410.1016/S8756-3282(00)00285-4 ↗
44. 10.1016/S0268-0033(03)00116-510.1016/S0268-0033(03)00116-5 ↗
45. 10.2106/00004623-198870020-0001510.2106/00004623-198870020-00015 ↗
46. ParkYS YangSY WooleyPH MerrittK HsuS McNallanMJ.Bioactivity responses of different UHMWPE particles from in‐vivo and in‐vitro tests. Materials Research Society Symposium–Proceedings;2001. pLL3.8.1‐LL3.8.6.
47. Inhibition of particulate debris‐induced osteolysis by alendronate in a rat model10.3928/0147-7447-20020101-17 ↗
48. 10.1016/j.morpho.2008.10.00310.1016/j.morpho.2008.10.003 ↗