journal article·2025-04-01Open access

Structural evolution and nucleation dynamics of RF sputtered Ga2O3 films on Ru(0001): The impact of deposition temperature and Ru surface morphology

Aman Baunthiyal, Marco Schowalter, Martin Williams, Jon-Olaf Krisponeit, Thorsten Mehrtens, Alexander Karg, Andreas Rosenauer, Martin Eickhoff, Jens Falta

APL Materials· Volume 13· Issue 4

Abstract

The use of Ru(0001) films as substrates on α-Al2O3(0001) substrates for radio-frequency magnetron sputter deposition of gallium oxide (Ga2O3) thin films is investigated regarding its dependence on the Ru film roughness; gallium oxide deposition temperature, which ranges from room temperature (RT) to 600 °C; and post-annealing up to 900 °C. The films have been characterized using various techniques. Raman spectroscopy confirms the deposition of β-Ga2O3 at deposition temperatures above 200 °C. The surface morphology was studied by atomic force microscopy (AFM), revealing that the roughness of the Ga2O3 surface strongly depends on deposition temperature, with a maximum at intermediate temperatures and a significant decrease between 400 and 600 °C. This can be explained by enhanced surface diffusion at higher temperatures. X-ray diffraction reveals poor crystallinity of all as-deposited films. Upon post-annealing, only those RT-deposited Ga2O3 films substantially gained crystallinity, which were deposited on the rougher Ru films. The cross-sectional scanning transmission electron microscopy provides insights into the grain structure, clearly disclosing the poly-crystallinity of the post-annealed Ga2O3 films with β-Ga2O3 being the predominant crystal structure. The β-Ga2O3 grain sizes are ∼10 nm for RT-deposited films and ∼40 nm for Ga2O3 deposited at 600 °C. However, γ-Ga2O3 grains of 10–20 nm in size are also found. The initial deposition of Ga2O3 on the Ru(0001) surface was studied in detail using AFM and low-energy electron diffraction (LEED). AFM shows that Ga2O3 islands nucleate predominantly at Ru step edges. LEED analysis confirms the nucleation of compressively strained epitaxial β-Ga2O3 and reveals the appearance of a (3 × 3)-reconstruction.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Ga2O3 and related materials · ZnO doping and properties · Advanced Photocatalysis Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Solid State Physics, University of Bremen 1 , 28359 Bremen,

MAPEX Center of Material and Processes, University of Bremen 2 , 28359 Bremen,

References (54)

Show source-provided references
1. Appl. Phys. Rev. · 2018 · 5 · 01130110.1063/1.5006941 ↗
2. Rev. Adv. Mater. Sci. · 2016 · 44 · 63
3. IEEE Electron Device Lett. · 1989 · 10 · 45510.1109/55.43098 ↗
4. J. Cryst. Growth · 2013 · 378 · 59110.1016/j.jcrysgro.2013.02.015 ↗
5. Nanoscale Res. Lett. · 2018 · 13 · 110.1186/s11671-018-2712-1 ↗
6. Mater. Today Phys. · 2017 · 3 · 11810.1016/j.mtphys.2017.10.002 ↗
7. Appl. Phys. Lett. · 2007 · 90 · 03191210.1063/1.2432946 ↗
8. Appl. Phys. Lett. · 2023 · 123 · 21350410.1063/5.0170354 ↗
9. 2023 · 536
10. Appl. Phys. Lett. · 2010 · 97 · 19350110.1063/1.3501967 ↗
11. J. Mater. · 2019 · 5 · 54210.1016/j.jmat.2019.08.003 ↗
12. Appl. Surf. Sci. · 2001 · 175 · 72110.1016/S0169-4332(01)00080-0 ↗
13. J. Chem. Phys. · 1960 · 33 · 67610.1063/1.1731237 ↗
14. J. Phys. D: Appl. Phys. · 2021 · 54 · 45300210.1088/1361-6463/ac1af2 ↗
15. Cryst. Growth Des. · 2023 · 23 · 443510.1021/acs.cgd.3c00193 ↗
16. J. Alloys Compd. · 2020 · 819 · 15305210.1016/j.jallcom.2019.153052 ↗
17. Phys. Status Solidi A · 2008 · 205 · 194310.1002/pssa.200778856 ↗
18. Opt. Quantum Electron. · 2020 · 52 · 110.1007/s11082-020-02306-8 ↗
19. ECS J. Solid State Sci. Technol. · 2019 · 8 · Q306410.1149/2.0141907jss ↗
20. Jpn. J. Appl. Phys. · 2016 · 55 · 1202B810.7567/jjap.55.1202b8 ↗
21. Thin Solid Films · 1996 · 279 · 11510.1016/0040-6090(95)08161-5 ↗
22. J. Phys. Chem. C · 2013 · 117 · 419410.1021/jp311300e ↗
23. J. Alloys Compd. · 2018 · 753 · 18610.1016/j.jallcom.2018.04.196 ↗
24. Appl. Surf. Sci. · 1999 · 142 · 18810.1016/s0169-4332(98)00714-4 ↗
25. J. Vac. Sci. Technol. A · 2016 · 34 · 06060210.1116/1.4963376 ↗
26. ACS Appl. Electron. Mater. · 2020 · 2 · 335810.1021/acsaelm.0c00643 ↗
27. Vacuum · 2021 · 192 · 11042210.1016/j.vacuum.2021.110422 ↗
28. Nanomaterials · 2024 · 14 · 197210.3390/nano14231972 ↗
29. Sol. Energy Mater. Sol. Cells · 2001 · 66 · 36910.1016/s0927-0248(00)00196-3 ↗
30. Appl. Phys. Express · 2015 · 8 · 03110110.7567/apex.8.031101 ↗
31. Cryst. Res. Technol. · 2010 · 45 · 122910.1002/crat.201000341 ↗
32. J. Appl. Phys. · 2011 · 110 · 06372010.1063/1.3642962 ↗
33. Phys. Status Solidi RRL · 2021 · 15 · 210035710.1002/pssr.202100357 ↗
34. Chin. Phys. B · 2019 · 28 · 01710510.1088/1674-1056/28/1/017105 ↗
35. J. Adv. Dielectr. · 2019 · 9 · 195003210.1142/S2010135X19500322 ↗
36. Phys. Status Solidi A · 2009 · 206 · 24310.1002/pssa.200824436 ↗
37. Cryst. Growth Des. · 2016 · 16 · 421610.1021/acs.cgd.6b00192 ↗
38. 2014 · 173
39. 2016 · 31
40. Cullis · 2008 · 17010.1007/978-1-4020-8615-1 ↗
41. Ultramicroscopy · 2009 · 109 · 117110.1016/j.ultramic.2009.05.003 ↗
42. Phys. Rev. Lett. · 1987 · 59 · 112410.1103/PhysRevLett.59.1124 ↗
43. Surf. Sci. · 1989 · 222 · 45110.1016/0039-6028(89)90371-3 ↗
44. Sci. Rep. · 2016 · 6 · 3596410.1038/srep35964 ↗
45. Ultramicroscopy · 2013 · 128 · 6810.1016/j.ultramic.2012.12.019 ↗
46. Z. Kristallogr. · 2010 · 225 · 10310.1524/zkri.2010.1205 ↗
47. J. Appl. Phys. · 1966 · 37 · 368210.1063/1.1707904 ↗
48. J. Appl. Phys. · 1969 · 40 · 61410.1063/1.1657442 ↗
49. J. Chem. Phys. · 1966 · 44 · 103910.1063/1.1726787 ↗
50. Appl. Phys. Lett. · 1998 · 72 · 69210.1063/1.120844 ↗
51. Appl. Phys. Lett. · 1998 · 73 · 163410.1063/1.122229 ↗
52. Platinum Met. Rev. · 2013 · 57 · 12710.1595/147106713x665030 ↗
53. Thin Solid Films · 2015 · 589 · 55610.1016/j.tsf.2015.06.034 ↗
54. J. Mater. Chem. C · 2021 · 9 · 1586810.1039/d1tc02852a ↗