Effects of tissue digestion solutions on surface properties of nitinol stents
Source abstract
Abstract
Abstract Analysis of explanted medical implants can provide a wealth of knowledge about device safety and performance. However, the quality of information may be compromised if the methods used to clean tissue from the device disturb the retrieved condition. Common solutions used to digest tissue may adversely affect the surface of the device and its severity can be material and processing dependent. In this study, two groups of stents made from the same material (Nitinol) were shape set in a salt pot (SP) or further processed by mechanical polishing (MP) and then immersed in one of three tissue digestion solutions (TDS): nitric acid (HNO3), sodium hydroxide (NaOH), or papain enzyme (papain). Nickel (Ni) ion concentrations were measured for each stent‐TDS combination and post‐immersion stent surface constituents, morphology and oxide depths were compared to baseline samples. Exposure to the HNO3 TDS resulted in relatively high Ni ion release and surface damage for both stent types. Papain TDS induced a greater Ni ion release than NaOH TDS, however, both were significantly lower than HNO3. The NaOH TDS increased the oxide layer thickness on MP stents. In contrast, all other stent immersions resulted in thinner oxide layers. For the Nitinol finishes used in this study, HNO3 is not recommended while papain and NaOH solutions may be appropriate depending on the post‐retrieval analysis performed. This study elucidates the importance of preliminary testing for TDS selection and how the surface finish can affect the sensitivity of a material to a TDS. 2017 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 106B: 331–339, 2018.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Orthopaedic implants and arthroplasty · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
U.S. Food and Drug Administration, Center for Devices and Radiological Health, Office of Science and Engineering Laboratories, Division of Applied Mechanics Silver Spring Maryland 20993
U.S. Food and Drug Administration, Winchester Engineering and Analytical Center Winchester Massachusetts 01890
Funding
FDA's Critical Path Initiative · Oak Ridge Institute for Science and Education (ORISE) Research Participation Program at FDA/CDRH
References (28)
Show source-provided references
1. 10.1016/j.jvs.2004.03.00810.1016/j.jvs.2004.03.008 ↗
2. 10.1177/15266028010080030310.1177/152660280100800303 ↗
3. 10.1016/S0142-9612(02)00410-610.1016/S0142-9612(02)00410-6 ↗
4. 10.1302/0301-620X.93B2.2509910.1302/0301-620X.93B2.25099 ↗
5. 10.1302/0301-620X.81B1.904710.1302/0301-620X.81B1.9047 ↗
6. ASTM F561‐13 · 2013
7. 2015
8. 10.1002/jab.77006010410.1002/jab.770060104 ↗
9. 10.1016/j.arth.2012.03.01910.1016/j.arth.2012.03.019 ↗
10. 10.1016/S0736-0266(03)00186-410.1016/S0736-0266(03)00186-4 ↗
11. Scanning electron microscopy analysis of corrosion of stainless steel and nitinol Stents from autopsy retrievals
12. In‐vivo corrosion and local release of metallic ions from vascular stents into surrounding tissue
13. Surface, corrosion and biocompatibility aspects of Nitinol as an implant material
14. Trepanier C · 1997 · 363
15. 10.1007/s40830-015-0028-x10.1007/s40830-015-0028-x ↗
16. Lasley CC · The corrosion of Nitinol by exposure to decontamination solutions. · 2004 · 375
17. Walak S. · Analysis of nitinol stent‐grafts after long term in‐vivo exposure · 2004 · 290
18. 10.1177/15266028000070020510.1177/152660280000700205 ↗
19. 10.1067/mva.2003.5810.1067/mva.2003.58 ↗
20. 10.1002/jbm.b.3169810.1002/jbm.b.31698 ↗
21. Late fiber deterioration in Dacron arterial grafts
22. 10.1002/jbm.82028041510.1002/jbm.820280415 ↗
23. 10.2106/00004623-199411000-0001010.2106/00004623-199411000-00010 ↗
24. 10.1016/j.biomaterials.2004.01.00110.1016/j.biomaterials.2004.01.001 ↗
25. 10.1016/0376-4583(82)90033-410.1016/0376-4583(82)90033-4 ↗
26. 10.1002/(SICI)1097-4636(199905)45:2<100::AID-JBM4>3.0.CO;2-010.1002/(SICI)1097-4636(199905)45:2<100::AID-JBM4>3.0.CO;2-0 ↗
27. 10.1016/j.scriptamat.2005.02.00210.1016/j.scriptamat.2005.02.002 ↗
28. 10.1007/s40830-015-0028-x10.1007/s40830-015-0028-x ↗