Abstract Hot corrosion behavior of FGH96 powder metallurgy (P/M) superalloy in 25 % NaCl + 75 % Na 2 SO 4 molten salts at 650, 700, and 750 °C was investigated in this paper. The methods of mass loss measurement, X‐ray diffraction (XRD), scanning electron microscopy (SEM), and energy‐dispersive spectroscopy (EDS) were used here. The experimental results show that hot corrosion kinetics follows a square power law at 650 °C, while a linear one at 700 and 750 °C. The corrosion layer is detected to be composed of Cr 2 O 3 , NiO, and Ni 2 S 3 at each temperature. The cross‐sectional morphologies and corresponding elemental maps indicate that the corrosion layer is a stratified structure of oxide and sulfide. The results and analyses confirm that the hot corrosion mechanism of FGH96 P/M superalloy is a cooperate process of oxidation and sulfidation. Furthermore, the relatively higher concentrations of Cr, Co, and Ti provide better corrosion resistance to the attack of S and Cl − .
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Materials Science and Engineering University of Science and Technology Beijing 100083 Beijing China

Funding

National Basic Research Program (973 Program) of China · National Key Research and Development Program of China

References (37)

Show source-provided references
1. 10.1016/j.finel.2013.10.00710.1016/j.finel.2013.10.007 ↗
2. 10.1016/j.msea.2010.07.01810.1016/j.msea.2010.07.018 ↗
3. 10.1016/j.msea.2013.10.03410.1016/j.msea.2013.10.034 ↗
4. Hot deformation behavior of FGH96 superalloys
5. 10.3901/CJME.2009.06.92510.3901/CJME.2009.06.925 ↗
6. 10.1016/j.msea.2010.07.03910.1016/j.msea.2010.07.039 ↗
7. 10.1007/s12598‐013‐0148‐410.1007/s12598‐013‐0148‐4 ↗
8. 10.31399/asm.tb.htcma.t5208024910.31399/asm.tb.htcma.t52080249 ↗
9. 10.1016/j.matdes.2010.11.06710.1016/j.matdes.2010.11.067 ↗
10. Khanna AS · 2002 · 285
11. 10.1016/j.corsci.2004.04.01310.1016/j.corsci.2004.04.013 ↗
12. 10.1016/S1350‐6307(00)00035‐210.1016/S1350‐6307(00)00035‐2 ↗
13. 10.1016/S0010‐938X(01)00057‐910.1016/S0010‐938X(01)00057‐9 ↗
14. 10.1016/j.jallcom.2007.12.09410.1016/j.jallcom.2007.12.094 ↗
15. 10.1016/j.msea.2014.11.01610.1016/j.msea.2014.11.016 ↗
16. 10.1016/j.surfcoat.2003.12.00310.1016/j.surfcoat.2003.12.003 ↗
17. 10.1016/j.jeurceramsoc.2004.04.01310.1016/j.jeurceramsoc.2004.04.013 ↗
18. 10.1016/j.msea.2008.04.04610.1016/j.msea.2008.04.046 ↗
19. 10.1016/j.corsci.2009.01.00310.1016/j.corsci.2009.01.003 ↗
20. 10.1007/BF0066427210.1007/BF00664272 ↗
21. 10.1017/CBO978113916390310.1017/CBO9781139163903 ↗
22. 10.1016/j.apsusc.2010.05.09810.1016/j.apsusc.2010.05.098 ↗
23. 10.1016/S1006‐7191(07)60014‐310.1016/S1006‐7191(07)60014‐3 ↗
24. 10.1016/j.corsci.2013.08.00310.1016/j.corsci.2013.08.003 ↗
25. 10.1016/j.corsci.2013.11.04810.1016/j.corsci.2013.11.048 ↗
26. 10.1016/j.corsci.2014.01.02010.1016/j.corsci.2014.01.020 ↗
27. 10.1016/S1359‐0286(02)00074‐810.1016/S1359‐0286(02)00074‐8 ↗
28. 10.1007/s11085‐015‐9543‐610.1007/s11085‐015‐9543‐6 ↗
29. 10.1007/BF0061169410.1007/BF00611694 ↗
30. 10.1016/0010‐938X(84)90051‐910.1016/0010‐938X(84)90051‐9 ↗
31. 10.1016/j.corsci.2014.03.01210.1016/j.corsci.2014.03.012 ↗
32. 10.1080/02670836.1987.1178226510.1080/02670836.1987.11782265 ↗
33. 10.1016/0010‐938X(87)90072‐210.1016/0010‐938X(87)90072‐2 ↗
34. Beltran AM · 1972 · 317
35. 10.1007/s11661‐000‐0051‐010.1007/s11661‐000‐0051‐0 ↗
36. 10.1016/j.intermet.2009.08.00410.1016/j.intermet.2009.08.004 ↗
37. 10.1016/j.scriptamat.2007.01.03510.1016/j.scriptamat.2007.01.035 ↗