Microstructural, mechanical and corrosion behaviour of Al–Si alloy reinforced with SiC metal matrix composite
Source abstract
Abstract
The aim of the present study is to investigate the effect of Si and SiC addition on the microstructure, mechanical, and corrosion properties of Al matrix-based composites. Al–Si (2 wt% fixed) alloy reinforced SiC composites were prepared by stir-casting process using SiC reinforcement contents from 0 to 20 wt% at an interval of 5%. A uniform dispersion of SiC particles in the Al matrix was observed from the scanning electron microscopic analysis. Maximum hardness is found for composites having 15 wt% reinforcement content. Pin-on-disc wear test reveals that SiC particles increase the wear resistance of composites. Corrosion test reveals that composites reinforced with 20% reinforcement content shows the minimum i corr among all the compositions, attributing to the maximum corrosion resistance. Tribological and corrosion behaviour were found to be dependent on the reinforcement content. However, they were not interdependent on each other. It is expected that the present study would be helpful in the development of lightweight composites for aerospace and shipping industries applications.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · MXene and MAX Phase Materials · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical Engineering, Amity University Uttar Pradesh, Noida, India
Department of Mechanical Engineering, Alakh Prakash Goyal Shimla University, India
Department of Ceramic Engineering, Indian Institute of Technology (Banaras Hindu University), Varanasi, India
Department of Mechanical and Industrial Engineering, Tallinn University of Technology, Estonia
Center for Advanced Materials, Qatar University, Qatar
Funding
Qatar National Research Fund
References (30)
Show source-provided references
1. Dubey A · J Appl Sci Eng · 2016 · 19 · 303
2. Gupta P · J Mater Environ Sci · 2016 · 7 · 2505
3. 10.1016/j.progpolymsci.2013.08.00310.1016/j.progpolymsci.2013.08.003 ↗
4. 10.1177/002199831983296110.1177/0021998319832961 ↗
5. 10.1016/j.compositesa.2014.10.01010.1016/j.compositesa.2014.10.010 ↗
6. 10.1016/j.jmrt.2015.05.00310.1016/j.jmrt.2015.05.003 ↗
7. 10.1177/002199831772658910.1177/0021998317726589 ↗
8. 10.1016/j.jmrt.2015.05.00410.1016/j.jmrt.2015.05.004 ↗
9. Garg P · J Mater Environ Sci · 2016 · 7 · 1461
10. 10.1016/j.ceramint.2016.12.11010.1016/j.ceramint.2016.12.110 ↗
11. 10.1016/j.acme.2017.06.01110.1016/j.acme.2017.06.011 ↗
12. 10.1016/j.matdes.2016.01.03110.1016/j.matdes.2016.01.031 ↗
13. 10.1016/j.jascer.2015.04.00110.1016/j.jascer.2015.04.001 ↗
14. 10.1016/S0924-0136(02)00234-010.1016/S0924-0136(02)00234-0 ↗
15. 10.1016/j.matchemphys.2004.02.00210.1016/j.matchemphys.2004.02.002 ↗
16. Liu X · Mater Sci Eng A · 2019
17. 10.1007/BF0281167910.1007/BF02811679 ↗
18. Guo H, Zhang J, Zhang Y, et al. Influence of hot rolling on mechanical behavior and strengthening mechanism in boron carbide reinforced aluminum matrix composites. In: TMS annual meeting & exhibition , 2018, pp. 851–860. Cham: Springer.10.1007/978-3-319-72526-0_81 ↗
19. 10.1016/j.jallcom.2018.04.22310.1016/j.jallcom.2018.04.223 ↗
20. 10.1007/s40430-017-0925-310.1007/s40430-017-0925-3 ↗
21. Gupta P, Kumar D, Quraishi MA, et al. Metal matrix nanocomposites and their application in corrosion control. In: Advances in nanomaterials , 2016, pp. 231–246. New York: Springer.10.1007/978-81-322-2668-0_6 ↗
22. Swain PK, Sahool AK, Das R, et al. Investigation, evaluation and analysis of SiCp nano particle metal matrix nanocomposite using a hybrid process. In: AIP conference proceedings , January 2018, Vol. 1930, p. 020056. New York: AIP Publishing.10.1063/1.5022950 ↗
23. Daniel SAA, Sakthivel M, Gopal PM, et al. Study on tribological behaviour of Al/SiC/MoS 2 hybrid metal matrix composites in high temperature environmental condition. In: Silicon . New York: Springer, 2018, pp. 1–11.10.1007/s12633-017-9739-2 ↗
24. 10.1016/j.jallcom.2018.01.33210.1016/j.jallcom.2018.01.332 ↗
25. 10.1016/j.jallcom.2019.01.38210.1016/j.jallcom.2019.01.382 ↗
26. Leszczyńska-Madej B · J Compos Mater · 2019
27. 10.1016/j.snb.2016.04.13410.1016/j.snb.2016.04.134 ↗
28. 10.1016/j.matchemphys.2018.08.07910.1016/j.matchemphys.2018.08.079 ↗
29. 10.1039/C4TC01037J10.1039/C4TC01037J ↗
30. Jamwal A, Vates UK, Gupta P, et al. Fabrication and characterization of Al 2 O 3 –TiC-reinforced aluminum matrix composites. In: Advances in industrial and production engineering . Singapore: Springer, 2019, pp. 349–356.10.1007/978-981-13-6412-9_33 ↗