Enhancing interlaminar fracture characteristics of woven CFRP prepreg composites through CNT dispersion
Source abstract
Abstract
The inter-ply characteristics of polymeric prepreg composites influence their interlaminar fracture toughness and the overall performance. This article embarks on engineering the inter-ply interfaces of carbon fiber reinforced polymer (CFRP) composites. A novel and practical technique for dispersion of multi-walled carbon nanotubes (MWCNTs) onto woven CFRP prepreg is presented. The interlaminar fracture toughness of these CFRP lay-ups was evaluated experimentally and compared with the regular (without any CNTs) specimen. Double cantilever beam and end notch flexure tests were conducted for interlaminar fracture studies. It was observed that the addition of MWCNTs in between the CFRP prepreg plies helps in strengthening the interface. There existed an optimum percentage in which these nanofillers should be added. The presence of nanotubes increased fiber bridging within the ply interfaces, which in turn controlled the inter-ply crack propagation. The findings and the mechanisms are discussed using the test data, SEM pictures, schematics, and scans of the fractured surfaces.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Carbon Nanotubes in Composites · Fiber-reinforced polymer composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Mechanical and Aerospace Engineering, Nanyang Technological University, Singapore
References (47)
Show source-provided references
1. 10.1016/S0266-3538(03)00088-510.1016/S0266-3538(03)00088-5 ↗
2. Kim J-K, Mai Y-W. Engineered interfaces in fiber reinforced composites Oxford: Elsevier, 1998.
3. 10.1177/07316844990180130810.1177/073168449901801308 ↗
4. Tong L, Mouritz AP, Bannister M. 3D fibre reinforced polymer composites Oxford: Elsevier, 2002.
5. 10.1023/A:101433551151510.1023/A:1014335511515 ↗
6. 10.1163/1568551005103344910.1163/15685510051033449 ↗
7. 10.1016/j.compscitech.2008.02.00810.1016/j.compscitech.2008.02.008 ↗
8. 10.1163/15685610332239672110.1163/156856103322396721 ↗
9. 10.1163/15685550677638266410.1163/156855506776382664 ↗
10. 10.1177/07316844940130060310.1177/073168449401300603 ↗
11. 10.1520/STP14006S10.1520/STP14006S ↗
12. Jiang W, Tjong SC, Chu PK, Li RKY, Kim JK, Mai YW. Interlaminar fracture properties of carbon fibre/epoxy matrix composites interleaved with polyethylene terephthalate (PET) films. Polym Polym Compos 2001; 9(Compendex): 141–144.
13. 10.1016/j.ijfatigue.2006.02.00410.1016/j.ijfatigue.2006.02.004 ↗
14. Klein PJ, Warren GL, Sager RJ, Sue HJ, Lagoudas DC. B-staged carbon nanotube/epoxy films for the improvement of interlaminar fracture toughness Cincinnati, OH: Society for the Advancement of Material and Process Engineering, 2007.
15. 10.1016/j.compscitech.2007.06.00710.1016/j.compscitech.2007.06.007 ↗
16. Warren G Sun L Moghbelli E White K Davis D Lagoudas D et al. (2009). B-staged interleaf-toughened epoxy/SWCNT nanocomposites for VARTM applications. In: SAMPE '09 Spring Symposium Conference Proceedings 18–21 May Baltimore MD USA Society for the Advancement of Material and Process Engineering.
17. 10.1016/S1359-835X(99)00034-210.1016/S1359-835X(99)00034-2 ↗
18. 10.1016/S0263-8223(02)00108-310.1016/S0263-8223(02)00108-3 ↗
19. 10.1016/j.compositesa.2010.02.00110.1016/j.compositesa.2010.02.001 ↗
20. 10.1016/S0266-3538(01)00094-X10.1016/S0266-3538(01)00094-X ↗
21. 10.1002/pc.2005810.1002/pc.20058 ↗
22. 10.1016/j.mser.2005.04.00210.1016/j.mser.2005.04.002 ↗
23. 10.1016/j.compscitech.2005.01.01410.1016/j.compscitech.2005.01.014 ↗
24. 10.1016/j.carbon.2006.02.03810.1016/j.carbon.2006.02.038 ↗
25. 10.1117/12.83606010.1117/12.836060 ↗
26. 10.1016/j.polymer.2010.01.04410.1016/j.polymer.2010.01.044 ↗
27. 10.1039/c000041h10.1039/c000041h ↗
28. 10.1177/002199830303700404310.1177/0021998303037004043 ↗
29. 10.1016/j.matlet.2005.05.02110.1016/j.matlet.2005.05.021 ↗
30. 10.1177/002199830708618610.1177/0021998307086186 ↗
31. 10.1016/j.carbon.2008.08.01010.1016/j.carbon.2008.08.010 ↗
32. 10.1016/j.compscitech.2008.02.02010.1016/j.compscitech.2008.02.020 ↗
33. 10.1038/nmat165010.1038/nmat1650 ↗
34. 10.1016/j.compositesa.2007.11.01310.1016/j.compositesa.2007.11.013 ↗
35. 10.2514/6.2006-185710.2514/6.2006-1857 ↗
36. 10.1177/002199830809773510.1177/0021998308097735 ↗
37. 10.1016/j.compositesa.2006.07.00510.1016/j.compositesa.2006.07.005 ↗
38. 10.1016/j.compositesa.2007.07.00210.1016/j.compositesa.2007.07.002 ↗
39. 10.1016/j.carbon.2009.06.03910.1016/j.carbon.2009.06.039 ↗
40. 10.1520/STP38422S10.1520/STP38422S ↗
41. 10.1177/00219983910250050210.1177/002199839102500502 ↗
42. 10.1520/STP36312S10.1520/STP36312S ↗
43. Donald FA LA Carlsson and RB Pipes Characterization of Delamination Failure in Experimental Characterization of Advanced Composite Materials Third Edition 2003; CRC Press. p.185–194.
44. Robinson P and Hodgkinson JM Interlaminar fracture toughness in Mechanical Testing of Advanced Fibre Composites 2000; CRC Press. p.170 206..10.1533/9781855738911.170 ↗
45. 10.1016/0010-4361(95)93669-B10.1016/0010-4361(95)93669-B ↗
46. ASTM D5528 - 01(2007)e2. Standard test method for mode I interlaminar fracture toughness of unidirectional fiber-reinforced polymer matrix composites. West Conshohocken PA: ASTM.
47. JSA JIS K 7086 ERTA (R 2008). Testing methods for interlaminar fracture toughness of carbon fibre reinforced plastics. Minato-Ku Tokyo: Japanese Industrial Standard Group.