Mode-I and mode-II interlaminar fracture properties of high modulus pitch-based carbon fiber reinforced polymers containing different nanostructures
Source abstract
Abstract
The mode-I and mode-II interlaminar fracture properties of high modulus pitch-based carbon fiber reinforced polymers (CFRPs) (fiber: K13C; resin: EX-1515 cyanate ester) modified with 20–30 nm β-SiC nanoparticles or multiwalled-carbon nanotubes (MWCNTs) were investigated. Different volume fractions of both the β-SiC nanoparticles (1, 2, 5, and 10 vol%) and MWCNTs (1, 3, 5, and 7 vol%) were tested. The values of the mode-I and mode-II interlaminar fracture toughness of the CFRPs containing the lowest volume fractions of these nanostructures were larger compared with the unfilled composite but decreased with increasing the volume fraction of the inclusions. No differences in mechanical properties were observed among the different nanostructure types.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Fiber-reinforced polymer composites · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Polymer Matrix Hybrid Composite Materials Group, Research Center for Structural Materials, National Institute for Materials Science (NIMS), Tsukuba, Japan
Department of Aerospace Engineering, Tohoku University, Sendai, Japan
References (21)
Show source-provided references
1. 10.1021/la062743p10.1021/la062743p ↗
2. 10.1016/0167-577X(95)00224-310.1016/0167-577X(95)00224-3 ↗
3. 10.1016/S0266-3538(02)00063-510.1016/S0266-3538(02)00063-5 ↗
4. 10.1016/j.compositesa.2006.03.00110.1016/j.compositesa.2006.03.001 ↗
5. 10.1016/j.compscitech.2007.08.01310.1016/j.compscitech.2007.08.013 ↗
6. 10.1063/1.146688010.1063/1.1466880 ↗
7. 10.1016/j.compositesa.2006.07.00510.1016/j.compositesa.2006.07.005 ↗
8. 10.1016/j.compositesa.2004.11.01710.1016/j.compositesa.2004.11.017 ↗
9. 10.1016/j.compscitech.2007.06.00710.1016/j.compscitech.2007.06.007 ↗
10. 10.1007/s10853-006-1198-x10.1007/s10853-006-1198-x ↗
11. 10.1016/j.scriptamat.2006.12.03810.1016/j.scriptamat.2006.12.038 ↗
12. 10.1016/j.compositesa.2008.08.00510.1016/j.compositesa.2008.08.005 ↗
13. 10.1016/j.compscitech.2009.05.00310.1016/j.compscitech.2009.05.003 ↗
14. 10.1177/07316844970160020310.1177/073168449701600203 ↗
15. 10.1016/0266-3538(87)90058-310.1016/0266-3538(87)90058-3 ↗
16. 10.1177/00219983920260150110.1177/002199839202601501 ↗
17. 10.1016/0266-3538(87)90033-910.1016/0266-3538(87)90033-9 ↗
18. 10.1177/00219983900240020110.1177/002199839002400201 ↗
19. 10.1243/03093247V24420710.1243/03093247V244207 ↗
20. 10.1016/j.compstruct.2019.11139210.1016/j.compstruct.2019.111392 ↗
21. JIS K 7086. Testing methods for interlaminar fracture toughness of carbon fibre reinforced plastics, 1993.