journal article·2014-10

Load capacity and chloride resistance of circular concrete columns with repair mortars

Sungnam Hong, Sun-Kyu Park

Journal of Composite Materials· Volume 48· Issue 24
Publisher page

Abstract

An experimental investigation was conducted to evaluate the structural behavior and chloride penetration characteristic of reinforced concrete columns to which patch repair was applied. A total of 24 reinforced concrete columns were fabricated. Four repair materials, with different types and contents of admixtures, were selected. The contents of the three admixtures (silica fume, zeolite, and polymer dispersion) were 0%, 10%, and 15%, based on the weights of the admixture and cement. For the experimental methods, a chloride penetration test and an axial compression test were used. As a result of the experiments, compression failure occurred in the control column. For the repaired columns, however, interfacial failure was observed, as the concrete core and repair material were debonded. The repair material that showed the greatest effect was mortar, for which polymer dispersion was used as the admixture. The ultimate strength and the strain at ultimate strength of the column that was repaired with this mortar increased by 40% and 80%, respectively, compared to the control column. Furthermore, the repair mortars that were mixed with the admixture showed much lower chloride concentrations than the control column. In particular, the chloride concentration of the mortar that was mixed with 15% polymer dispersion decreased by 95%, in the section with a depth of 20–30 mm from the column surface.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Structural Behavior of Reinforced Concrete · Innovative concrete reinforcement materials · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Civil and Environmental Engineering, Sungkyunkwan University, Republic of Korea

References (39)

Show source-provided references
1. Korean Institute of Architects · 2007
2. Newsis. Corroded reinforcing steel of old Seoul city hall (Lee, D.H.) , news.naver.com/main/read.nhn?mode=LSD&mid=sec&sid1=102&oid=003&aid=0002256492 (2008, accessed 28 August 2008).
3. Neville AM · 1995
4. Morsy SM · Journal of Materials Science & Technology · 1995 · 11 · 447
5. 10.1680/macr.1991.43.156.15510.1680/macr.1991.43.156.155 ↗
6. Pedeferri P · 2004
7. Schneck U. Non-destructive diagnosis and repair of 300 concrete columns beneath a shopping mall under full operation. In: Grantham M, Mechtcherine V and Schneck U (eds) 4th international conference on concrete repair , Dresden, Germany, 26–28 September 2011, pp.113–120. London: CRC Press.10.1201/b11570-19 ↗
8. Mackechnie JR · 2001
9. Houston JT, Atimay E and Ferguson PM. Corrosion of reinforcing steel embedded in structural concrete . Report no. CFHR-3-5-68-112-1F, Center for Highway Research, University of Texas, USA, 1972.
10. 10.3846/1822-427X.2009.4.134-14210.3846/1822-427X.2009.4.134-142 ↗
11. Cho DY · Mech Compos Mater · 2006 · 47 · 531
12. 10.1007/s11029-012-9303-510.1007/s11029-012-9303-5 ↗
13. 10.1177/002199831245431810.1177/0021998312454318 ↗
14. Cambel-Allen D · 1991
15. 10.1016/0950-0618(95)00087-910.1016/0950-0618(95)00087-9 ↗
16. 10.1016/0950-0618(95)00065-810.1016/0950-0618(95)00065-8 ↗
17. 10.1016/S0958-9465(99)00044-X10.1016/S0958-9465(99)00044-X ↗
18. Cusson D · ACI Struct J · 1994 · 120 · 783
19. 10.1061/(ASCE)0733-9445(1998)124:12(1431)10.1061/(ASCE)0733-9445(1998)124:12(1431) ↗
20. ACI Committee 234 · 2006
21. 10.1016/S0008-8846(03)00171-610.1016/S0008-8846(03)00171-6 ↗
22. 10.4334/JKCI.2011.23.2.20310.4334/JKCI.2011.23.2.203 ↗
23. Kasai Y · ACI Spec Pub · 1992 · 132 · 615
24. 10.4334/JKCI.2008.20.5.63510.4334/JKCI.2008.20.5.635 ↗
25. Ohama Y · 1995
26. Pareek SN. Improvement in adhesion of polymeric repair and finish materials for reinforced concrete structures . PhD Thesis, College of Engineering, Nihon University, 1993.
27. 10.1016/0008-8846(85)90114-010.1016/0008-8846(85)90114-0 ↗
28. 10.1016/0958-9465(94)90040-X10.1016/0958-9465(94)90040-X ↗
29. 10.1016/j.cemconres.2013.01.01110.1016/j.cemconres.2013.01.011 ↗
30. 10.1016/j.conbuildmat.2012.04.03810.1016/j.conbuildmat.2012.04.038 ↗
31. 10.1016/j.conbuildmat.2005.08.00710.1016/j.conbuildmat.2005.08.007 ↗
32. 10.1016/S0958-9465(02)00092-610.1016/S0958-9465(02)00092-6 ↗
33. 10.1016/j.conbuildmat.2008.11.01110.1016/j.conbuildmat.2008.11.011 ↗
34. 10.1016/j.conbuildmat.2011.03.01110.1016/j.conbuildmat.2011.03.011 ↗
35. ACI Committee 706. Field Guide to Concrete Repair Application Procedures: Surface Repair Using Form-and-Pump Techniques , American Concrete Institute, Rap Bulletin 6, USA, 2006.
36. ASTM C39/C39M · 2005
37. ASTM C496/C496M · 2004
38. ASTM C293/C293M · 2010
39. ASTM C1152/C1152M · 2012