journal article·2023-02

Compressive Behavior of GFRP Tubes Filled with Self-Compacting Concrete

Pan Xie, Lik Lam, Tao Jiang

Publisher page

Abstract

Self-compacting concrete (SCC) features excellent flow ability without the need of vibration for compaction during casting. This makes it particularly suitable for application in hybrid fiber-reinforced polymer (FRP)-concrete–steel double-skin tubular columns (DSTCs), a high-performance structural form evolved from concrete-filled FRP tubes (CFFTs). In a DSTC, the space between the inner steel tube and the outer FRP tube for filling concrete may be narrow and the application of vibration may be difficult. However, because of the large shrinkage of SCC compared to traditional concrete of normal flow ability, the integrity and composite action of DSTCs with SCC become a major concern. To clarify this issue, an understanding of the behavior of CFFTs filled with SCC is an essential prerequisite. While a large number of studies have been published on CFFTs with normal concrete (NC), only limited studies have been carried out on CFFTs with SCC. This paper presents a comprehensive investigation on the effect of SCC on the behavior of large-scale CFFTs. Axial compression tests were carried out on concrete-filled glass FRP (GFRP) tubes with diameters of 150, 200, 300, and 400 mm. The compressive behavior of the CFFT specimens filled with NC, a nonexpansive SCC, and an expansive SCC (ESCC) was compared and discussed. The results showed that the specimens with nonexpansive SCC behaved differently compared to those with NC as a result of larger shrinkage, especially for large specimens for which the confinement level was lower. This situation, however, improved in specimens where ESCC was used. Finally, the test results were further analyzed using a theoretical model recently proposed by the authors’ group.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Structural Behavior of Reinforced Concrete · Concrete Corrosion and Durability · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Associate Professor, College of Water Conservancy and Civil Engineering, South China Agricultural Univ., Guangzhou 510642, China; formerly, Ph.D. Student, Dept. of Civil and Environmental Engineering, The Hong Kong Polytechnic Univ., Hong Kong, China.

Chief Research and Design Engineer, Fibrpro International Ltd., Hong Kong, China.

Associate Professor, Space Structures Research Center, Dept. of Civil Engineering, Zhejiang Univ., Hangzhou 310058, China (corresponding author). ORCID: .

References (39)

Show source-provided references
1. ASTM. 2014. Standard test method for static modulus of elasticity and Poisson’s ratio of concrete in compression. ASTM C469/C469M-14. West Conshohocken, PA: ASTM.
2. 10.1016/S0020-7683(99)00077-310.1016/S0020-7683(99)00077-3 ↗
3. 10.1016/S0958-9465(03)00045-310.1016/S0958-9465(03)00045-3 ↗
4. Bhirud, Y. L., and K. K. Sangle. 2017. “Comparison of shrinkage, creep and elastic shortening of VMA and powder type self-compacting concrete and normal vibrated concrete.” Open J. Civ. Eng. 7 (1): 130. https://doi.org/10.4236/ojce.2017.71008.10.4236/ojce.2017.71008 ↗
5. 10.1061/(ASCE)CC.1943-5614.000081810.1061/(ASCE)CC.1943-5614.0000818 ↗
6. Carey, S. A., and K. A. Harries. 2005. “Axial behavior and modeling of confined small-, medium-, and large-scale circular sections with carbon fiber-reinforced polymer jackets.” ACI Struct. J. 102 (4): 596–604.
7. 10.1016/j.cemconcomp.2006.07.01010.1016/j.cemconcomp.2006.07.010 ↗
8. EFNARC. 2002. Specification and guidelines for self-compacting concrete. Farnham, UK: EFNARC.
9. 10.1016/j.cemconcomp.2004.02.04510.1016/j.cemconcomp.2004.02.045 ↗
10. Fam, A. Z., and S. H. Rizkalla. 2001a. “Behavior of axially loaded concrete-filled circular FRP tubes.” ACI Struct. J. 98 (3): 280–289.
11. Fam, A. Z., and S. H. Rizkalla. 2001b. “Confinement model for axially loaded concrete confined by circular fiber-reinforced polymer tubes.” ACI Struct. J. 98 (4): 451–461.
12. Ghoddousi, P., and A. Monir Abbasi. 2008. “Influence of aggregate grading and cement paste volume on drying shrinkage of self-consolidating concrete.” In Proc., 3rd North American Conf., on the Design and Use of Self-Consolidating Concrete. Chicago, IL: Center for Advanced Cement-Based Materials (ACBM).
13. Goodier, C. I. 2003. “Development of self-compacting concrete.” Struct. Build. 156 (SB4): 405–414.10.1680/stbu.2003.156.4.405 ↗
14. 10.1016/S0008-8846(01)00463-X10.1016/S0008-8846(01)00463-X ↗
15. 10.1016/S0008-8846(02)00737-810.1016/S0008-8846(02)00737-8 ↗
16. 10.1016/j.engstruct.2007.01.01010.1016/j.engstruct.2007.01.010 ↗
17. 10.1061/(ASCE)CC.1943-5614.000122510.1061/(ASCE)CC.1943-5614.0001225 ↗
18. Jones, R. M., and D. A. R. Nelson Jr. 1975. “A new material model for the nonlinear biaxial behavior of ATJ-S graphite.” J. Compos. Mater. 9 (1): 10–27. https://doi.org/10.1177/002199837500900102.10.1177/002199837500900102 ↗
19. 10.1061/(ASCE)1090-0268(2004)8:6(539)10.1061/(ASCE)1090-0268(2004)8:6(539) ↗
20. 10.1016/j.conbuildmat.2010.11.01910.1016/j.conbuildmat.2010.11.019 ↗
21. 10.1061/(ASCE)CC.1943-5614.000065110.1061/(ASCE)CC.1943-5614.0000651 ↗
22. 10.1617/s11527-008-9367-910.1617/s11527-008-9367-9 ↗
23. 10.1016/j.conbuildmat.2019.11794810.1016/j.conbuildmat.2019.117948 ↗
24. 10.1061/(ASCE)0733-9445(1997)123:5(583)10.1061/(ASCE)0733-9445(1997)123:5(583) ↗
25. Okamura, H., K. Ozawa, and M. Ouchi. 2000. “Self-compacting concrete.” Struct. Concr. 1 (2): 3–17. https://doi.org/10.1680/stco.2000.1.1.3.10.1680/stco.2000.1.1.3 ↗
26. 10.1061/(ASCE)CC.1943-5614.000041010.1061/(ASCE)CC.1943-5614.0000410 ↗
27. Paultre, P., K. H. Khayat, D. Cusson, and S. Tremblay. 2005. “Structural performance of self-consolidating concrete used in confined concrete columns.” ACI Struct. J. 102 (4): 560–568.
28. Qasrawi, Y., P. J. Heffernan, and A. Fam. 2016. “Numerical modeling of concrete-filled FRP tubes’ dynamic behavior under blast and impact loading.” J. Struct. Eng. 142 (2): 04015106. https://doi.org/10.1061/(ASCE)ST.1943-541X.0001370.10.1061/(ASCE)ST.1943-541X.0001370 ↗
29. 10.1016/j.cemconcomp.2007.03.01010.1016/j.cemconcomp.2007.03.010 ↗
30. 10.1016/S0008-8846(99)00037-X10.1016/S0008-8846(99)00037-X ↗
31. Skarendahl, Å, and Ö Petersson. 2000. Self-compacting concrete: State-of-the art report of RILEM technical committee 174-scc. Cachan Cedex, France: RILEM Publications SARL.
32. 10.1061/(ASCE)CC.1943-5614.000112210.1061/(ASCE)CC.1943-5614.0001122 ↗
33. 10.1061/(ASCE)0733-9445(2004)130:11(1713)10.1061/(ASCE)0733-9445(2004)130:11(1713) ↗
34. 10.1061/(ASCE)1090-0268(2007)11:2(201)10.1061/(ASCE)1090-0268(2007)11:2(201) ↗
35. 10.1061/(ASCE)CC.1943-5614.000001210.1061/(ASCE)CC.1943-5614.0000012 ↗
36. 10.1061/(ASCE)CC.1943-5614.000007010.1061/(ASCE)CC.1943-5614.0000070 ↗
37. 10.1016/j.engstruct.2020.11076210.1016/j.engstruct.2020.110762 ↗
38. 10.1260/1369-4332.18.10.173710.1260/1369-4332.18.10.1737 ↗
39. Yu, T., X. L. Fang, and J. G. Teng. 2014. “FRP-confined self-compacting concrete under axial compression.” J. Mater. Civ. Eng. 26 (11).