Rehabilitation of Wooden Utility Poles with Sprayed-GFRP Composites
Source abstract
Abstract
Different rehabilitation techniques have been utilized to extend the service life of wooden utility poles, which are mainly affected by degradation and decay. This paper presents an evaluation of the performance of wooden utility poles rehabilitated using sprayed glass fiber–reinforced polymer (GFRP) composites and near-surface-mounted (NSM)-GFRP bars. Seven full-size (305-mm diameter) new wooden poles and five full-size old wooden poles, taken out of service, were tested under monotonically increasing lateral load. The test parameters included the thickness (4, 6, and 8 mm) and length (1.0 and 2.0 m) of the sprayed-GFRP coating, and rehabilitation methods (sprayed-GFRP composites, NSM-GFRP bars). The results showed that the sprayed-GFRP coating can restore the load-carrying capacity and enhance the stiffness of both old and damaged poles. In addition, the load-carrying capacity of the wooden poles was not affected by the increase in GFRP thickness after the thickness reached 6 mm. It was also concluded that using the NSM-GFRP bars is not cost-effective compared to the sprayed-GFRP composites. A simple analytical procedure was introduced to estimate the load-carrying capacity of retrofitted poles and to calculate the required thickness of the sprayed-FRP layer, which yielded reasonably conservative results.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Structural Behavior of Reinforced Concrete · Geotechnical Engineering and Underground Structures · Wood Treatment and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
M.Sc. Student, Dept. of Civil Engineering, Univ. of Manitoba, 15 Gillson St., Winnipeg, MB, Canada R3T 5V6.
Lecturer, Civil Engineering Dept., Assiut Univ., Assiut 71515, Egypt. ORCID: .
Professor of Civil Engineering, Dept. of Civil Engineering, Univ. of Manitoba, 15 Gillson St., Winnipeg, MB, Canada R3T 5V6 (corresponding author). ORCID: .
References (27)
Show source-provided references
1. ACI (American Concrete Institute). 2017. Guide for the design and construction of externally bonded FRP systems for strengthening concrete structures. ACI PRC-440.2-17. Detroit, MI: ACI.
2. ASTM. 2016. Standard test method for compressive properties of polymer matrix composite materials with unsupported gage section by shear loading. ASTM D3410-16. West Conshohocken, PA: ASTM.
3. ASTM. 2017a. Standard test methods for static tests of wood poles. ASTM D1036-99. West Conshohocken, PA: ASTM.
4. ASTM. 2017b. Standard test method for tensile properties of polymer matrix composite materials. ASTM D3039-17. West Conshohocken, PA: ASTM.
5. ASTM. 2021. Standard test method for pull-off strength for FRP laminate systems bonded to concrete substrate. ASTM D7522-21. West Conshohocken, PA: ASTM.
6. 10.3390/ma1310235010.3390/ma13102350 ↗
7. Banthia, N., N. Nandakumar, and A. Boyd. 2002. “Sprayed fiber-reinforced polymers: From laboratory to a real bridge.” Concr. Int. 24 (11): 47–52.
8. Crosslink Technology Inc. 2002 “Pecker Patch Attributes.” Crosslink Technology Inc. Web Page. Accessed January 15 2022. https://www.crosslinktech.com/downloads/pecker_patch/peckerpatch_attributes.pdf.
9. CSA (Canadian Standards Association). 2019. Wood utility poles and reinforcing stubs. CSA O15-15 (R2019). Toronto, ON: CSA.
10. 10.1520/CTR10544J10.1520/CTR10544J ↗
11. 10.1520/CTR10545J10.1520/CTR10545J ↗
12. 10.1061/(ASCE)1090-0268(1999)3:2(92)10.1061/(ASCE)1090-0268(1999)3:2(92) ↗
13. 10.1061/(ASCE)1090-0268(2003)7:4(363)10.1061/(ASCE)1090-0268(2003)7:4(363) ↗
14. 10.1061/(ASCE)BE.1943-5592.000058410.1061/(ASCE)BE.1943-5592.0000584 ↗
15. Hays, W. 1986. “Extending wood pole life: Solving a $5-billion/year program.” Electr. World 41–47.
16. 10.1016/S0951-8339(03)00021-210.1016/S0951-8339(03)00021-2 ↗
17. 10.1016/j.accre.2020.10.00110.1016/j.accre.2020.10.001 ↗
18. 10.1061/(ASCE)CC.1943-5614.000097310.1061/(ASCE)CC.1943-5614.0000973 ↗
19. 10.1016/j.compstruct.2017.11.08510.1016/j.compstruct.2017.11.085 ↗
20. 10.1139/l06-10510.1139/l06-105 ↗
21. Pultrall Inc. 2019. V-ROD—Technical data sheet. Thetford Mines, QC: ADS Comp. Group.
22. Qiao P. J. F. Davalos and B. S. Trimble. 2000. “Effect of moisture on fracture toughness of composite/wood bonded interfaces.” In Vol. 31 of Fatigue and fracture mechanics ASTM STP 1389 edited by G. R. Halford and J. P. Gallagher 526–544. West Conshohochen PA: ASTM International.10.1520/STP14819S ↗
23. Rotafix Northern Ltd. 2023. “Rotafix Structural Adhesive (RSA) Data Sheet.” Accessed March 8 2022. http://rotafix.co.uk/products/timber-engineering/rotafix-structural-adhesive/.
24. 10.1061/(ASCE)CF.1943-5509.000011710.1061/(ASCE)CF.1943-5509.0000117 ↗
25. Tavassoli, A., J. Liu, and S. Sheikh. 2015. “Glass fiber-reinforced polymer-reinforced circular columns under simulated seismic loads.” ACI Struct. J. 110 (6): 941–951.
26. Thermo Fisher Scientific. 2020. “CAB-O-SIL M5 Safety Data Sheet.” Accessed March 22 2022. https://assets.thermofisher.com/DirectWebViewer/private/document.aspx?prd=ACR40373∼∼PDF∼∼MTR∼∼CLP1∼∼EN∼∼2020-12-21%2019:51:20∼∼CAB-O-SIL%c2%ae%20M5∼∼.
27. 10.1016/j.istruc.2021.04.04410.1016/j.istruc.2021.04.044 ↗