journal article·2015-04

Designing and optimization of separation process of iron impurities from kaolin by oxalic acid in bench-scale stirred-tank reactor

M. Taran, E. Aghaie

Publisher page

Abstract

Abstract Kaolin leaching by oxalic acid in a bench-scale stirred-tank reactor using response surface methodology and face centered central composite design based on three variables: oxalic acid concentration (X1: 0.1–0.3 M), temperature (X2: 30–80 °C) and duration of the leaching test (X3: 2–4 days) was investigated. The experimental data obtained were fitted to a second-order polynomial equation using multiple regression analysis by Design-Expert 7 software and were analyzed by analysis of variance (ANOVA). According to ANOVA, all factors (X1, X2 and X3) influenced the response (dissolved iron concentration) and a positive regression coefficient of variables suggested an increase in dissolved iron concentration with an increase in oxalic acid concentration, temperature and time of leaching but there was not any interaction between them. The 3-D response surface plot and the contour plot derived from the mathematical model were applied to determine the optimal conditions. The optimum leaching conditions for maximum dissolved iron concentration were found to be oxalic acid concentration of 0.21 M, temperature of 77 °C and duration of the leaching test of 4 days. After the washing stage of kaolin, in those experiments that pH was above 4, iron oxalate precipitate was formed and the percentage of residual iron in the sample after leaching was higher than expected. In general, the minimum amount of residual iron in the kaolin was 0.75% (w/w) that was obtained in tests where the oxalic acid concentration, temperature, time of the leaching and pH of final solution were 0.3 M, 30 °C, 2 days and 3, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Clay minerals and soil interactions · Mine drainage and remediation techniques · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. The use of reactors in biomining processes10.2225/vol3-issue3-fulltext-4 ↗
2. Response Surface Methodology (RSM) Analysis of organic acid production for kaolin beneficiation by Aspergillus niger
3. Effect of organic acids on ferric iron removal from iron-stained kaolinite10.1016/S0169-1317(99)00038-1 ↗
4. Modeling and optimization I: usability of response surface methodology10.1016/j.jfoodeng.2005.11.024 ↗
5. Influence of iron on kaolin whiteness: an electron paramagnetic resonance study10.1016/j.clay.2010.04.022 ↗
6. Response surface methodology (RSM) as a tool for optimization in analytical chemistry10.1016/j.talanta.2008.05.019 ↗
7. Multifactor experimental designs for exploring response surfaces10.1214/aoms/1177707047 ↗
8. Iron leaching of a Mexican clay of industrial interest by oxalic acid
9. Iron removal from kaolin. Comparison between “in situ” and “two-stage” bioleaching processes10.1016/S0304-386X(02)00196-2 ↗
10. Bulk and surface properties of commercial kaolins10.1016/j.clay.2010.02.002 ↗
11. Iron minerals and their influence on the optical properties of two Indian kaolins10.1016/j.clay.2006.06.008 ↗
12. Bioleaching of Brazilian kaolins using organic acids and fermented medium10.1016/0892-6875(96)00087-8 ↗
13. Improvement of iron removal from silica sand using ultrasound-assisted oxalic acid10.1016/j.ultsonch.2010.07.006 ↗
14. Statistical designs and response surface techniques for the optimization of chromatographic systems10.1016/j.chroma.2007.03.051 ↗
15. Relationships between chemico-mineralogical composition and color properties in selected natural and calcined Spanish kaolins10.1016/j.clay.2004.02.004 ↗
16. Bleaching of kaolins and clays by chlorination of iron and titanium10.1016/j.clay.2006.05.001 ↗
17. Bioleaching of iron from kaolin using Fe (III)-reducing bacteria with various carbon nitrogen sources10.1016/j.clay.2010.01.010 ↗
18. Influence of organic acids, complexing agents and heavy metals on the bioleaching of iron from kaolin using Fe (III)-reducing bacteria10.1016/j.clay.2011.01.012 ↗
19. Bioleaching of iron from highly contaminated kaolin clay by Aspergillus niger10.1016/j.clay.2007.01.010 ↗
20. Study on the kinetics of iron oxide leaching by oxalic acid10.1016/j.minpro.2006.03.012 ↗
21. Dissolution of iron oxide using oxalic acid10.1016/j.hydromet.2007.02.005 ↗
22. Improvement of xylanase production by Penicillium oxalicum ZH-30 using response surface methodology10.1016/j.enzmictec.2006.10.015 ↗
23. Submerged production of oxalic acid from glucose by immobilized Aspergillus niger10.1016/j.procbio.2004.06.013 ↗
24. Leaching kinetics of iron from low grade kaolin by oxalic acid solutions10.1016/j.clay.2011.01.011 ↗
25. Montgomery · 2005
26. Bioleaching of heavy metals from a low-grade mining ore using Aspergillus niger10.1016/j.jhazmat.2004.02.040 ↗
27. Applied clay mineralogy-occurrences, processing and application of kaolins, bentonites, palygorskite–sepiolite, and common clays
28. Designing a process of kaolin bleaching in an oxalic acid enriched medium by Aspergillus niger cultivated on biodiesel-derived waste composed of glycerol and fatty acids10.1016/j.clay.2011.03.004 ↗
29. Nanda · 2008
30. Mechanism of dissolution of iron oxides in aqueous oxalic acid10.1016/0304-386X(95)00104-O ↗
31. Value addition of paper coating grade kaolins by the removal of ultrafine coloring impurities10.1016/S0301-7516(97)00040-9 ↗
32. Characterization of kaolin from the Capim River region — Brazil10.1016/j.clay.2011.11.009 ↗
33. Removal of iron from silica sand by leaching with oxalic acid10.1016/S0304-386X(97)00015-7 ↗
34. Factorial experiments for iron removal from kaolin by using single and two-step leaching with sulfuric acid10.1016/j.hydromet.2013.02.006 ↗
35. Optimization of coagulation–flocculation process for a paper-recycling wastewater treatment using response surface methodology10.1016/j.colsurfa.2007.02.023 ↗
36. Iron removal from kaolin using thiourea assisted by ultrasonic wave10.1016/j.ultsonch.2011.05.008 ↗
37. Refinement of industrial kaolin by microbial removal of iron-bearing impurities10.1016/j.clay.2013.08.041 ↗
38. Statistical optimization of culture conditions for 1,3-propanediol by Klebsiella pneumoniae AC 15 via central composite design10.1016/j.biortech.2007.02.038 ↗