journal article·2014-06

Czochralski growth of heavily tin-doped Si crystals

I. Yonenaga, T. Taishi, K. Inoue, R. Gotoh, K. Kutsukake, Y. Tokumoto, Y. Ohno

Publisher page

Abstract

Heavily tin (Sn)-doped Si crystals in a concentration up to 4×1019 cm−3 were grown by the Czochralski method. Variation of Sn concentration in the crystals was well expressed by the Pfann equation using a segregation coefficient of k=0.016. From the occurrence of growth interface instability and the appearance of Sn precipitates in the grown crystals, the solubility limit of Sn was considered to be around 5×1019 cm−3. Interstitially dissolved oxygen Oi was presented at a concentration of 8–9×1017 cm−3 in the grown Sn-doped crystals. The FT-IR absorption peak relating to a Si–Oi–Si quasi-molecule at 1106 cm−1 showed preferential occupation of Oi at the bond-centered position of Si–Si. The Oi peak shifted to the lower wave number side with increasing Sn concentration in Si, implying expansion of the Si–Si bond.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Diffusion and precipitation of oxygen in silicon doped with germanium10.4028/www.scientific.net/MSF.258-263.1767 ↗
2. Point defect engineering strategies to suppress A-center formation in silicon10.1063/1.3666226 ↗
3. Effect of tin doping on oxygen- and carbon-related defects in Czochralski silicon10.1063/1.3658261 ↗
4. Defect engineering of the oxygen-vacancy clusters formation in electron irradiated silicon by isovalent doping: an infrared perspective10.1063/1.4770488 ↗
5. Formation of defects as a result of electron irradiation of tin-doped p-type silicon
6. Oxygen precipitation and defects in heavily doped Czochralski silicon10.1063/1.351521 ↗
7. Specific features of the behavior of oxygen in Sn-doped silicon10.1134/1.1309402 ↗
8. Tin doping of silicon for controlling oxygen precipitation and radiation hardness10.1149/1.1417558 ↗
9. Defect-impurity interactions in irradiated tin-doped Cz-Si crystals10.1002/pssc.200306195 ↗
10. Effect of tin on point defects and oxygen precipitation in Czochralski silicon: experimental and theoretical studies10.1063/1.4794531 ↗
11. R.W. Olesinski, G.J. Abbaschian, in: T.B. Massalski (Ed.), Binary Alloy Phase Diagrams, II ed., vol. 2, 1986, p. 2050.
12. Solid solubilities of impurity elements in germanium and silicon10.1002/j.1538-7305.1960.tb03928.x ↗
13. Interstitial oxygen in GeSi alloys10.1016/S0921-4526(01)00771-2 ↗
14. Growth and fundamental properties of SiGe bulk crystals10.1016/j.jcrysgro.2004.10.071 ↗
15. Growth of heavily indium doped Si crystals by co-doping of neutral impurity carbon or germanium10.4028/www.scientific.net/KEM.508.220 ↗
16. Principles of zone-melting
17. Chromsaure-flusssaure als spezifisches system zur atzgrubenentwicklung auf silizium
18. α-Sn and β-Sn precipitates in annealed epitaxial Si0.95Sn0.0510.1103/PhysRevB.60.5770 ↗
19. Interlaboratory determination of the calibration factor for the measurement of the interstitial oxygen content of silicon by infrared absorption10.1149/1.2097135 ↗
20. Oxygen and dioxygen centers in Si and Ge: density-functional calculations10.1103/PhysRevB.62.10824 ↗
21. I. Yonenaga, R. Gotoh, K. Omote, K. Inoue, T. Taishi, Y. Tokumoto, K. Kutsukake, Y. Ohno, unpublished work.
22. A study of carbon-implanted silicon for light-emitting diode fabrication10.1016/0921-5107(89)90223-7 ↗